Technical Study on Impurity Aluminum Removal from High-concentration Pr-NdCl3 Feed Solution(Ⅱ) AITranslate

State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth;State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth;State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth;State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth;State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth;State Key Laboratory of Bayan Obo Rare Earth Resource Researches and Comprehensive Utilization,Baotou Research Institute of Rare Earth
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-concentration Pr-NdCl3 feed solution separated from Bayan Obo rare earth concentrate by smelting contains 0.10~0.34 g/L aluminum,and the aluminum content directly affects the quality of downstream products,so it is necessary to separate aluminum from rare earth.Based on the principle of preferential extraction of aluminum in naphthenic acid-isooctanol-sulfonated kerosene system,the non rare earth impurity aluminum can be removed from high-concentration Pr-NdCl3 feed solution by cascade extraction separation process.The pilot scale test was carried out based on the analysis and demonstration of the whole technological process and the cascade extraction and cascade washing process.The results show that after 30-stage cascade extraction separation process,the concentration of REO is more than 220 g/L,the content of aluminum impurity is greatly reduced,the mass ratio of Al2O3 to REO is less than 7.8×10-5,and the product quality meets the standard.The application of cascade extraction separation process not only optimizes and improves the existing single-stage extraction process,but also improves and stabilizes the product quality,having promotion value.

KeyWords AITranslate

Pr-NdCl3 feed solution aluminum naphthenic acid cascade extraction washing stripping process optimization

1J.M.D.Coey.Perspective and Prospects for Rare Earth Permanent Magnets[J].工程(英文),2020,6(2):119-131. 被引量:25

2墨柯.锂离子电池产业链发展研究[J].新材料产业,2019,0(2):32-39. 被引量:3

3王健力.浅谈电动车辆动力电池的性能特点及其发展[J].科技风,2019(3):150-150. 被引量:3

4杨玉梅.稀土永磁材料的研究与应用[J].中国粉体工业,2020,0(2):27-30. 被引量:6

5柳云龙,聂仲文,罗启顺,陈云.镨钕氧化物的物理性质对其电解生产的影响及改善措施[J].稀有金属与硬质合金,2016,44(2):50-53. 被引量:5

6郑国栋,王琨,陈其慎,张艳飞,邢佳韵,龙涛,董延涛,倪晋鹏.世界稀土产业格局变化与中国稀土产业面临的问题[J].地球学报,2021,42(2):265-272. 被引量:27

7吉力强,陈明昕,顾虎,赵京辉,杨烜.轻稀土资源现状及在新能源汽车领域的应用[J].中国稀土学报,2020,38(2):129-138. 被引量:19

8马升峰,孟志军,李裕,许延辉,高天佐,关卫华,王荣,王永利.高浓度镨钕料液去除杂质铝的工艺研究(Ⅰ)[J].稀有金属与硬质合金,2021,49(2):9-14. 被引量:1

9周洁英,杨新华,洪侃,赖兰萍,陈冬英.从稀土分解液中连续去除铁、铝[J].湿法冶金,2016,35(6):513-516. 被引量:8

10王彩英,王士智,李平.稀土萃取分离工艺的改进与废水循环利用研究[J].稀有金属与硬质合金,2017,45(5):7-10. 被引量:5

1高习贵,林平,孙明华,李瑞宏,程文琳.氟化镨钕绿色制备生产工艺研究[J].科技创新与应用,2020(27):113-114. 被引量:1

2孙汉林.纳米纯铜与铜铝合金中Σ13(320)晶界的剪切耦合行为研究[J].工程与建设,2020,34(6):1188-1190.

3徐海阳.我国工业企业节水技术应用探讨[J].西南给排水,2021,43(4):62-66.

4麻少莹,杨昌鹏,韦璐,黄杰,孙钦菊.利用超临界流体萃取法提取天然香蕉香精[J].食品工业,2021,42(6):179-183. 被引量:6

5张立萍,吕灵灵,孔慧,张新功,张晓佳.废炼油催化剂酸浸液中钒与铁的共萃取与梯度分离[J].化工环保,2021,41(4):446-451.

6王印松,孙天舒.基于二分类NMF网络的执行器故障状态评估[J].系统仿真学报,2021,33(8):1882-1891. 被引量:1

7梁业新,程海梅,孟庆国,苑明哲.响应曲面法对离心萃取高浓度含酚废水工艺的优化[J].广东化工,2021,48(12):121-124.

8李乐斌,齐恩伍,吕卫星,胡石林.低温泵控制系统设计与实现[J].低温工程,2021(4):19-22. 被引量:1

9张立萍,吕灵灵,孔慧,叶红,祝汉国.控制萃取平衡时间选择性分离回收FCC废催化剂酸浸液中的钒[J].石油炼制与化工,2021,52(8):96-101. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

High-concentration Pr-NdCl3 feed solution separated from Bayan Obo rare earth concentrate by smelting contains 0.10~0.34 g/L aluminum,and the aluminum content directly affects the quality of downstream products,so it is necessary to separate aluminum from rare earth.Based on the principle of preferential extraction of aluminum in naphthenic acid-isooctanol-sulfonated kerosene system,the non rare earth impurity aluminum can be removed from high-concentration Pr-NdCl3 feed solution by cascade extraction separation process.The pilot scale test was carried out based on the analysis and demonstration of the whole technological process and the cascade extraction and cascade washing process.The results show that after 30-stage cascade extraction separation process,the concentration of REO is more than 220 g/L,the content of aluminum impurity is greatly reduced,the mass ratio of Al2O3 to REO is less than 7.8×10-5,and the product quality meets the standard.The application of cascade extraction separation process not only optimizes and improves the existing single-stage extraction process,but also improves and stabilizes the product quality,having promotion value.

quote

GB/T 7714-2015 [1] MENG Zhi-jun, XU Yan-hui, GAO Tian-zuo, et al. Technical Study on Impurity Aluminum Removal from High-concentration Pr-NdCl3 Feed Solution(Ⅱ)[J]. Rare Metals and Cemented Carbides, 2021(4): 6-10.
MLA [1] MENG Zhi-jun, et al., "Technical Study on Impurity Aluminum Removal from High-concentration Pr-NdCl3 Feed Solution(Ⅱ)." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 6-10.
APA [1] MENG Zhi-jun, XU Yan-hui, GAO Tian-zuo, GUAN Wei-hua, LI Yu, & MA Sheng-feng. (2021). Technical Study on Impurity Aluminum Removal from High-concentration Pr-NdCl3 Feed Solution(Ⅱ). Rare Metals and Cemented Carbides(4), 6-10.
IEEE [1] MENG Zhi-jun, XU Yan-hui, GAO Tian-zuo, GUAN Wei-hua, LI Yu, and MA Sheng-feng, "Technical Study on Impurity Aluminum Removal from High-concentration Pr-NdCl3 Feed Solution(Ⅱ)," Rare Metals and Cemented Carbides, no. 4, pp. 6-10, 2021. keywords: {Pr-NdCl3 feed solution;aluminum;naphthenic acid;cascade extraction;washing;stripping;process optimization}