Process Optimization of Recycling Lithium from Waste Ternary Power Battery AITranslate

CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of the long recovery process and low lithium recovery rate of waste ternary power batte-ry,and the situation that most enterprises only produce crude lithium carbonate and lithium phosphate,and the added value of products is low,the lithium extraction process of flotation-reduction roasting carbonization is used to produce battery grade lithius carbonate.The results show that under the optimized process index and device sign parameters,the recovery rate of lithium is more than 90%.The removal of most ne-gative graphite by flotation can effectively reduce the specifications of leaching equipment and pressure filtration equipment,shorten the subsequent recovery process of nickel,cobalt and manganese,and reduce the acid and alkali consumption in the extraction process.The impurity content of the solution after lithium extraction by carbonization is low,and the battery grade lithium carbonate can be produced after purification,which can improve the economic benefit of the enterprise.

KeyWords AITranslate

waste ternary power battery lithium recovery lithium carbonate flotation reduction roasting carbonization

1王沿森,吕灵灵,臧刚刚,刘敏福.废旧锂离子电池回收技术进展[J].世界有色金属,2018,43(5):26-28. 被引量:4

2杨长远.废旧锂离子动力电池三元正极材料短流程回收再生研究[J].江西化工,2020,36(6):72-74. 被引量:1

3张燕,赵振中,马朝辉,赵彦才,陈治毓,马正强.碳化法制备电池级碳酸锂工艺优化研究[J].无机盐工业,2020,52(3):68-71. 被引量:3

4陈玲,章小明,朱志全,刘超,许鑫,廖萃.从废旧锂离子电池回收粗制磷酸锂中提取锂制备电池级碳酸锂工艺探究[J].江西化工,2018,34(6):94-96. 被引量:7

5刘帆,周有池,王林生,周健,文小强.从废旧锂离子电池提钴后液中回收锂[J].无机盐工业,2017,49(2):50-53. 被引量:8

6严康,熊正阳,刘志楼,徐志峰,王瑞祥,聂华平.废旧三元锂离子电池正极还原焙烧回收Li的研究[J].中南大学学报:自然科学版,2020,51(12):3367-3378. 被引量:8

7李浩强,范茂松,何鹏琛,汪浩,刘晶冰.退役三元动力电池回收利用进展[J].化学通报,2020,83(3):226-231. 被引量:7

8王晶,梁精龙,李慧,王冬斌.废旧锂电池中有价金属的处理方法现状及展望[J].热加工工艺,2018,47(22):12-15. 被引量:3

1于志勇.考虑区块链技术投入的新能源汽车电池回收策略[J].物流技术,2022,41(11):37-43.

1薛磊.质量管理体系在机械设计与开发中的运用[J].现代企业,2021(8):31-32.

2王莉莉,韦飞,吴吉华,段亚甫,和逸飞,张哲哲.溶出条件对印尼铝土矿各指标影响研究[J].云南冶金,2021,50(3):24-28.

3王海,张杰,吴继崇,李超,王泽强.废三元锂电材料还原焙烧提锂试验研究[J].广东化工,2021,48(13):16-17. 被引量:2

4林伟.电解法生产电池级锂及高纯级锂工艺浅析[J].工业加热,2021,50(8):12-13.

5刘娇洋,陈文江.基于Fluent的中心筒结构转化器数值模拟[J].有色冶金设计与研究,2021,42(4):7-11.

6郑欢,冯晓兰,赵博,杨岗,杨鹏程,刘宇春,张锦飞.高铝粉煤灰碱石灰低钙烧结熟料的浸出[J].洁净煤技术,2021,27(3):275-280.

7聂光旭,陈钢,罗永春,袁海滨,陆涛.高杂铜电解液净化生产实践[J].云南冶金,2021,50(4):72-76. 被引量:1

8陈光强,陆冠诚.气相色谱法测定大米中7种有机磷农药分析[J].种子科技,2021,39(16):31-32. 被引量:2

9郭明钢,卞冰,米盼盼,杨晓航,韩加奇.油田脱烃采出气回收减排工艺研究[J].山东化工,2021,50(14):161-164. 被引量:1

10谢堂锋,陈若葵,巩勤学,蔡罗蓉.氟硅酸钾滴定法测定粗制氟化钠中二氧化硅[J].无机盐工业,2021,53(9):92-96.

Basic Information:

DOI:

Chinese Library Classification Number:TF19[冶金工程—冶金物理化学]

Citation Information:

In view of the long recovery process and low lithium recovery rate of waste ternary power batte-ry,and the situation that most enterprises only produce crude lithium carbonate and lithium phosphate,and the added value of products is low,the lithium extraction process of flotation-reduction roasting carbonization is used to produce battery grade lithius carbonate.The results show that under the optimized process index and device sign parameters,the recovery rate of lithium is more than 90%.The removal of most ne-gative graphite by flotation can effectively reduce the specifications of leaching equipment and pressure filtration equipment,shorten the subsequent recovery process of nickel,cobalt and manganese,and reduce the acid and alkali consumption in the extraction process.The impurity content of the solution after lithium extraction by carbonization is low,and the battery grade lithium carbonate can be produced after purification,which can improve the economic benefit of the enterprise.

quote

GB/T 7714-2015 [1] DONG Xiao-wei, ZHAO Jian-bo. Process Optimization of Recycling Lithium from Waste Ternary Power Battery[J]. Rare Metals and Cemented Carbides, 2021(4): 11-14.
MLA [1] DONG Xiao-wei, and ZHAO Jian-bo. "Process Optimization of Recycling Lithium from Waste Ternary Power Battery." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 11-14.
APA [1] DONG Xiao-wei, & ZHAO Jian-bo. (2021). Process Optimization of Recycling Lithium from Waste Ternary Power Battery. Rare Metals and Cemented Carbides(4), 11-14.
IEEE [1] DONG Xiao-wei and ZHAO Jian-bo, "Process Optimization of Recycling Lithium from Waste Ternary Power Battery," Rare Metals and Cemented Carbides, no. 4, pp. 11-14, 2021. keywords: {waste ternary power battery;lithium recovery;lithium carbonate;flotation;reduction roasting carbonization}