daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Reversible Thermally-Responsive Copolymer Valve for Manipulating Water Wicking AITranslate

Northwestern University; China|University of Chinese Academy of Sciences; Northwestern University;Institute of Chemistry;Institute of Chemistry;Institute of Chemistry;Institute of Chemistry;Institute of Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wicking action produced equipment is widely noted for its ease of miniaturization, simplicity of equipment, and lack of external energy supply requirement. However, current materials used for controlled wicking are very scarce and not reversible, severely limiting the application of the wicking phenomenon. In this work, a reversible thermally responsive valve is developed from thermally responsive copolymer [poly(N-acryloyl glycinamide-co-styrene), PNAGA/PSt], which shows suitable temperature-dependent wicking performance. The wicking capacity of the valve can be increased by 5.75 times from 20 to 80 °C and can be cycled at least five times. The excellent wicking performance is ascribed to the hydrogen bonding variation of PNAGA/PSt. The wicking is controlled by temperature only. Furthermore, based on the thermally responsive valve, a microflow platform is developed to promote or prevent large drop (45 μL) accumulation. This work opens a new avenue to design and prepare materials with controlled wicking capability, providing a platform for water collection, miniature biochemical reactions, and microliquid control.

KeyWords AITranslate

thermally responsive copolymers UCSTtype polymer controllable wicking wicking valve microfluidic manipulation microfluidic platforms
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01579

Chinese Library Classification Number:

Citation Information:

Wicking action produced equipment is widely noted for its ease of miniaturization, simplicity of equipment, and lack of external energy supply requirement. However, current materials used for controlled wicking are very scarce and not reversible, severely limiting the application of the wicking phenomenon. In this work, a reversible thermally responsive valve is developed from thermally responsive copolymer [poly(N-acryloyl glycinamide-co-styrene), PNAGA/PSt], which shows suitable temperature-dependent wicking performance. The wicking capacity of the valve can be increased by 5.75 times from 20 to 80 °C and can be cycled at least five times. The excellent wicking performance is ascribed to the hydrogen bonding variation of PNAGA/PSt. The wicking is controlled by temperature only. Furthermore, based on the thermally responsive valve, a microflow platform is developed to promote or prevent large drop (45 μL) accumulation. This work opens a new avenue to design and prepare materials with controlled wicking capability, providing a platform for water collection, miniature biochemical reactions, and microliquid control.

quote

GB/T 7714-2015 [1] Xin Zhou, Yifan He, Saipeng Huang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01579.
MLA [1] Xin Zhou, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01579.
APA [1] Xin Zhou, Yifan He, Saipeng Huang, Kun Zheng, Xinyu Cao, Jingnan Zhang, Gang Ye, & Yongmei Ma. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01579
IEEE [1] Xin Zhou, Yifan He, Saipeng Huang, Kun Zheng, Xinyu Cao, Jingnan Zhang, Gang Ye, and Yongmei Ma, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01579. keywords: {thermally responsive copolymers UCSTtype polymer controllable wicking wicking valve microfluidic manipulation microfluidic platforms}