Research on Enhancement of CVD DiamondNucleation by Carbon Nanotubes AITranslate
Abstract AITranslate
The paper has reviewed the latest development and mechanism of carbon nanotubes enhancement of CVD diamond nucleation.
KeyWords AITranslate
1Iijima S.Helical microtubes of graphitic carbon[J].Nature,1991,354:56.
2Wong E W,et al .Nanobeam mecharics:Elasticity,strength,and toughness of nanorods and nanotubes[J],Science,1997,277:1971..
3Che G L,et al .Carbon nanotube membranes for electrochemical energy storage storage and production[J].Nature,1998,393:346.
4Wei B Q,et al .Reliability and current carrying capacity of car-bon nanotubes[J].Appl Phys Lett,2001,79(8):1172.
5Da Jing Yang ,et al .Thermal conductivity of multiwalled car-bon nanotubes[J].Phys Rew B,2002,66:165440-1.
6Arif A Mamedov,et al.Molecular design of carbon nanotube/pllyelectrolyte multilayer composites[J].Nature,2002,(1):1940.
7王茂章,杨全红,成会明.碳的结构及其同素异性体[J].炭素技术,2001,20(1):23-28. 被引量:6
8Meilunas R J,et al .Kiamond nucleation on surface using caubon clusters[J].J Mater Res ,1994,9(1):61.
9Hisako Hirai,et al. Amorphous diamond from C60 fullerene[J]Appl Phys Lett,1994,64(14):1979.
10刘波,王豪,阮昊,干福熹.C_(60)膜上金刚石的成核与生长形貌研究[J].人工晶体学报,2002,31(2):153-157. 被引量:1
1代明江,匡同春,刘正义,成晓玲,白晓军.金刚石膜剥落后硬质合金基体的表面形态[J].金属学报,2000,36(7):780-784.
2张云鹤,李庚,苗孟河,李云苍.粉末冶金法碳纳米管增强镁基复合材料的微观组织及力学性能[J].复合材料学报,2013,30(S1):102-106. 被引量:12
3崔照雯,蒋立坤,刘建金,贾成厂.Al_2O_3含量对碳纳米管增强Cu基复合材料性能的影响[J].粉末冶金工业,2015,25(2):31-34. 被引量:6
4聂俊辉,张亚丰,史娜,贾成厂.镀钨碳纳米管增强铜基复合材料的制备及性能[J].北京科技大学学报,2012,34(7):823-829. 被引量:8
5F.Deuerler,王祖娟,吴建国.硬质合金工具的耐磨金刚石涂层[J].国外难熔金属与硬质材料,2003,19(1):23-28.
6曾谊晖,刘忠,罗飞霞,柏春旺.高钴硬质合金基底上化学气相沉积金刚石膜的研究[J].金刚石与磨料磨具工程,2004,24(1):31-33. 被引量:3
7贾璐,刘意春,谢明,易健宏.碳纳米管/银氧化锡复合材料的制备及其性能研究[J].现代化工,2017,37(1):104-107. 被引量:1
8钟磊,卢文壮,左敦稳,林欢庆.EACVD金刚石膜沉积设备衬底温度的测量[J].机械制造与自动化,2008,37(5):30-32.
9袁安富,王珉.真空弧沉积类金刚石膜探讨[J].中国表面工程,2001,14(1):31-35. 被引量:1
10苗晋琦,张鬲君,王成彪,吕建国,唐伟忠,吕反修.酸浸+等离子体刻蚀YG6微米-纳米金刚石复合涂层工具研究[J].金刚石与磨料磨具工程,2005,25(5):18-23. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
The paper has reviewed the latest development and mechanism of carbon nanotubes enhancement of CVD diamond nucleation.
quote
| GB/T 7714-2015 | [1] SUN Xin-yuan, ZHANG Gang. Research on Enhancement of CVD DiamondNucleation by Carbon Nanotubes[J]. Rare Metals and Cemented Carbides, 2004(2): 42-46. |
| MLA | [1] SUN Xin-yuan, and ZHANG Gang. "Research on Enhancement of CVD DiamondNucleation by Carbon Nanotubes." Rare Metals and Cemented Carbides, no. 2, 2004, pp. 42-46. |
| APA | [1] SUN Xin-yuan, & ZHANG Gang. (2004). Research on Enhancement of CVD DiamondNucleation by Carbon Nanotubes. Rare Metals and Cemented Carbides(2), 42-46. |
| IEEE | [1] SUN Xin-yuan and ZHANG Gang, "Research on Enhancement of CVD DiamondNucleation by Carbon Nanotubes," Rare Metals and Cemented Carbides, no. 2, pp. 42-46, 2004. keywords: {chemical vapor deposition;diamond films;carbon nanotubes} |