Effective Approach for Improvement of Tungsten Metallurgical Recovery AITranslate

Ganzhou Huaxing Tungsten Products Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Analysis is made of reason for metal tungsten loss during APT preparation by ion exchange.Meanwhile,based on the theory and practice,effective measures are presented for reduction of metal tungsten loss and improvement of overall metallurgical metal tungsten recovery up to 95%.

KeyWords AITranslate

tungsten metallurgy ion exchange metal tungsten loss metal recovery

1陈树茂,郭永忠.离子交换法处理仲钨酸铵结晶母液试验与实践[J].中国钨业,2001,16(3):22-24. 被引量:14

2中南工业大学.从钨酸盐溶液中除钼、砷、锑、锡的方法[P].WO Pat:ZL97108113.1,1997-06-19.

1伏彩萍,杨利群,姜文伟.浅谈钨冶炼萃取工艺流程的钨回收率[J].中国钨业,2005,20(3):37-38. 被引量:6

2刘飞飞,刘辉辉,李俊荣.基于RBF神经网络的WO_3浸出率软测量建模[J].有色金属科学与工程,2013,4(5):117-121. 被引量:4

1肖军辉,文书明.海南钨钼多金属矿选矿试验研究[J].稀有金属,2010,34(4):578-584. 被引量:4

2杨利群.钨湿法冶炼新工艺技术的应用[J].稀有金属与硬质合金,2006,34(2):52-54. 被引量:3

3梁卫东.二次压煮工艺提高钨冶炼金属回收率的应用[J].稀有金属与硬质合金,2006,34(4):45-47. 被引量:6

4张建平,梁松林.矿业类科技论文摘要平行语料库建设的可行性研究[J].中国钨业,2008,23(6):47-50. 被引量:5

5赵中伟,肖露萍,郭持皓,陈星宇,陈爱良,霍广生,李洪桂.Influence of earth gravity on reaction engineering of tubular reactor for high concentration tungsten ion-exchange[J].中国有色金属学报:英文版,2010,20(12):2379-2386. 被引量:3

6许亮,陈冬英,杨新华,常德民,周洁英,欧阳红.钨钽铌粗精矿碱分解液萃取试验研究[J].中国钨业,2014,29(1):48-51.

7刘飞飞,祝恩宇,李俊荣.钨碱煮工艺温度的自适应广义预测控制研究[J].中国钨业,2015,30(3):63-66.

8刘飞飞,祝恩宇,徐鹏,龚亚忠,罗贤平,张宇舟.碱煮工艺过程的智能集成建模研究[J].有色金属:冶炼部分,2015(6):63-66. 被引量:2

9刘飞飞,罗贤平,古帅奇,辛鹏武.碱煮过程浸出率预测与优化研究[J].有色金属:冶炼部分,2016(5):29-32. 被引量:1

10李明周,朱伟伟,黄金堤,童长仁,张文海,汪金良.基于两温两密度法的FeO-Fe_2O_3-SiO_2三元渣系成分软测量模型[J].有色金属科学与工程,2016,7(5):37-41. 被引量:1

1牛士珍,牛四通.海绵铁在电炉炼钢中使用效果的分析[J].特殊钢,1997,18(4):37-39. 被引量:5

2梁卫东.二次压煮工艺提高钨冶炼金属回收率的应用[J].稀有金属与硬质合金,2006,34(4):45-47. 被引量:6

3张国才.降低熔化黄铜废料时的金属损失[J].稀有金属快报,1993(3):17-18.

4廖运友.锰铁高炉提高锰回收率的措施[J].铁合金,2002,33(6):13-15.

5李晶,孙铭良,黄克雄,杜恒清,陈新民.铜熔炼渣中隔膜层形成与金属损失[J].有色金属:冶炼部分,1990(5):20-22. 被引量:3

6成荣明,程广斌,陈奕卫,杨宝林.离子交换法提纯钯的优化工艺条件[J].应用化学,1999,16(5):113-114. 被引量:1

7李涛,Zhang Jielei.高铋、锑和银的铅阳极泥火法处理工艺设计[J].世界有色金属,2015,40(5):42-44. 被引量:2

8王明.钨冶炼离子交换工艺技术的研究进展[J].稀有金属与硬质合金,2013,41(6):13-16. 被引量:8

9倪起峰.离子交换法在稀土分离中的地位[J].稀有金属与硬质合金,1990(1):32-34. 被引量:4

10张文昭,杨志刚.用离子交换法制备超纯硫酸锌[J].有色冶炼,1994,23(2):49-50.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

Analysis is made of reason for metal tungsten loss during APT preparation by ion exchange.Meanwhile,based on the theory and practice,effective measures are presented for reduction of metal tungsten loss and improvement of overall metallurgical metal tungsten recovery up to 95%.

quote

GB/T 7714-2015 [1] CHEN Shu-mao. Effective Approach for Improvement of Tungsten Metallurgical Recovery[J]. Rare Metals and Cemented Carbides, 2004(2): 39-41.
MLA [1] CHEN Shu-mao. "Effective Approach for Improvement of Tungsten Metallurgical Recovery." Rare Metals and Cemented Carbides, no. 2, 2004, pp. 39-41.
APA [1] CHEN Shu-mao. (2004). Effective Approach for Improvement of Tungsten Metallurgical Recovery. Rare Metals and Cemented Carbides(2), 39-41.
IEEE [1] CHEN Shu-mao, "Effective Approach for Improvement of Tungsten Metallurgical Recovery," Rare Metals and Cemented Carbides, no. 2, pp. 39-41, 2004. keywords: {tungsten metallurgy;ion exchange;metal tungsten loss;metal recovery}