daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Advanced Design of Acrylate Polymers for Solid-State Electrolytes in Sodium-Ion Batteries:Current Advances and Future Perspectives AITranslate

State Key Laboratory of Explosion Science and Safety Protection,School of Mechatronical Engineering,Beijing Institute of Technology,Beijing 100081,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the continuous development of technology,the demand for energy in human society is increasing day by day. Fossil fuels,as the main source of energy at present,bring about huge carbon dioxide emissions,which exacerbate the greenhouse effect and cause rapid global temperature rise and seriously affecting the global climate. Reducing the use of fossil fuels and developing renewable and sustainable green energy has become a consensus among all the humanity. However,green energy sources such as solar energy,wind energy,hydropower and geothermal energy suffer from temporal and spatial imbalances and instability,making it difficult to meet the sustainable and stable requirements of human society for energy. Therefore,there is an urgent need to increase research on energy storage devices with high energy density and long cycle life to help make up the shortcomings of the green energy that we are suing now. At present,lithium batteries play an important part of large-scale commercial energy storage devices for their good comprehensive performance. They marvelously meet the above requirements while adapt to the needs of the rising industries such as new energy vehicles and smartphones. However,lithium-ion batteries have high costs and the supply of raw materials is difficult to meet the rapidly increasing demand. Reliable substitutes for lithium batteries are needed. Sodium and lithium are located in the same main group in the periodic table with similar chemical properties. Besides,sodium is widely distributed on Earth,thus it is easy to obtain and cost-effective. Sodium ion batteries work in a similar way to lithium-ion batteries. The smaller Stokes radius of sodium ions in solvents helps them achieve higher ion migration rates and numbers,making sodium ion batteries a potential alternative to lithium-ion batteries. Electrolytes,as the medium for ion transport,play an important part of batteries,greatly affecting their overall performance and safety. The electrolyte systems that use organic solvents are widely studied in sodium ion batteries. However,liquid electrolytes are difficult to control the growth of dendrites,resulting in a decrease in the cycling stability and Coulombic efficiency of the battery. Besides,the dendrites piercing through the separator can cause a short circuit in the battery,and may cause serious safety accidents such as leakage of flammable organic electrolytes and explosions. Developing solid electrolytes instead of liquid electrolytes can greatly reduce safety hazards and improve battery performance. Solid electrolytes can be mainly divided into inorganic solid electrolytes,organic solid electrolytes,and composite solid electrolytes according to their composition. The organic polymer solid electrolyte can be divided into gel electrolyte and pure solid electrolyte according to its morphology. Acrylate polymer solid electrolytes have the characteristics of easy availability,wide application,mature process,and good compatibility with electrode materials,making them popular candidate materials for developing new generation secondary batteries with high energy density and safety. Based on this,according to the role of acrylate in electrolyte,this article reviewed the research progress of acrylic polymer electrolytes in sodium ion batteries by dividing them into three categories:acrylate cross-linked copolymer electrolytes,poly-acrylate gel electrolytes,and poly-acrylate composite electrolytes. Acrylate mainly acted as the crosslinking agents in cross-linked electrolytes. While in the poly-acrylate gel electrolytes,the acrylate played the leading role,determining the electrochemical performance of the electrolyte. As for the poly-acrylate composite electrolytes,the acrylate was regarded as the matrix of electrolyte and play an important part of their electrochemical performance. Then their advantages and disadvantages were discussed. The acrylate cross-linked copolymer electrolytes could achieve multiple functions according to different needs,making them adaptable to complex scenarios. However,the electrochemical performance of acrylate crosslinking agents had not been fully utilized. The research on poly-acrylate gel electrolyte mainly focused on polymethyl methacrylate. Their electrochemical performance could satisfy the basic needs of batteries,while poor mechanical performance limited its application. As for the poly-acrylate composite electrolytes,they were the most widely studied acrylate electrolytes for their good comprehensive performance. They combined the advantages of organic and inorganic components,thus possessing excellent electrochemical,mechanical,and processing properties. They could be divided into three categories:composite with other polymers,composite with active inorganic fillers,and composite with inert inorganic fillers. Compositing with other polymers mainly improved their mechanical strength and stability,while compositing with inorganic fillers mainly enhance their ion conductivity. Compositing with inorganic fillers could provide more ion transport pathways,resulting in higher ion conductivity than inert inorganic fillers. However,the proportion of acrylate in composite electrolytes was often less than half,which failed to fully utilize the excellent electrochemical performance of the acrylate matrix. Besides,the influence of acrylate content on electrochemical properties of composite electrolytes was often ignored. More inorganic fillers increased the cost of batteries. Finally,based on the properties of different categories of acrylate electrolyte,this article proposed corresponding optimization strategies and looked forward to their trends of future development.

KeyWords AITranslate

sodium ion battery gel polymer electrolyte acrylate compounds solid state electrolyte

[1]Johnsson F,Kjärstad J,Rootzén J. The threat to climate change mitigation posed by the abundance of fossil fuels [J]. Climate Policy,2019,19(2):258.

[2](孙如梦,周礼菊,司大强,黄瑶,王雷刚. 基于DEFORM-3D的新能源电池壳底部台阶镦挤成形工艺改进与优化 [J]. 锻压技术,2023,48(9):1.)

R M Sun,L J Zhou,D Q Si,Y Huang,L G Wang. Improvement and optimization on upset-extrusion forming process for bottom step of new energy battery shell based on DEFORM-3D [J]. Forging & Stamping Technology,2023,48(9):1.

[3]Li G,Li M,Taylor R,Hao Y,Besagni G,Markides C N. Solar energy utilisation:current status and roll-out potential [J]. Applied Thermal Engineering,2022,209:118285.

[4]Kumar Y,Ringenberg J,Depuru S S,Devabhaktuni V K,Lee J W,Nikolaidis W,Andersen B,Afjeh A. Wind energy:trends and enabling technologies [J]. Renewable and Sustainable Energy Reviews,2016,53:209.

[5]Nayak P K,Yang L,Brehm W,Adelhelm P. From lithium‐ion to sodium‐ion batteries:advantages,challenges,and surprises [J]. Angewandte Chemie International Edition,2018,57(1):102.

[6](张可翔,王泽,唐淑璟,彭洪亮,闫二虎,孙立贤. LiNixCoyMn1-x-yO2三元氧化物正极材料碳包覆策略 [J]. 稀有金属,2025,49(4):565.)

K X Zhang,Z Wang,S J Tang,H L Peng,E H Yan,L X Sun. Carbon coating strategies of LiNixCoyMn1-x-yO2 ternary oxide cathode materials [J]. Chinese Journal of Rare Metals,2025,49(4):565.

[7](梁媛,赵景腾,韩志杰,尉海军. 锂稀有金属在二次电池中的应用 [J]. 稀有金属,2019,43(11):1187.)

Y Liang,J T Zhao,Z J Han,H J Yu. Application of lithium rare metal in rechargeable batteries [J]. Chinese Journal of Rare Metals,2019,43(11):1187.

[8](张德沛,叶向阳,庞越鹏. Na-B-H体系固体电解质的研究现状 [J].稀有金属,2025,49(4):553.)

D P Zhang,X Y Ye,Y P Pang. Research progress on Na-B-H based solid electrolytes [J]. Chinese Journal of Rare Metals,2025,49(4):553.

[9]Chayambuka K,Mulder G,Danilov D L,Notten P H L. From Li‐ion batteries toward Na‐ion chemistries:challenges and opportunities [J]. Advanced Energy Materials,2020,10(38):2001310.

[10]Zhao C L,Liu L L,Qi X G,Lu Y X,Wu F X,Zhao J M,Yu Y,Hu Y S,Chen L Q. Solid‐state sodium batteries [J]. Advanced Energy Materials,2018,8(17):1703012.

[11]Che H Y,Chen S L,Xie Y Y,Wang H,Amine K,Liao X Z,Ma Z F. Electrolyte design strategies and research progress for room-temperature sodium-ion batteries [J]. Energy & Environmental Science,2017,10(5):1075.

[12]Zhang Z Z,Shao Y J,Lotsch B,Hu Y S,Li H,Janek J,Nazar L F,Nan C W,Maier J,Armand M,Chen L Q. New horizons for inorganic solid state ion conductors [J]. Energy & Environmental Science,2018,11(8):1945.

[13]Yin H,Han C J,Liu Q R,Wu F Y,Zhang F,Tang Y B. Recent advances and perspectives on the polymer electrolytes for sodium/potassium‐ion batteries [J]. Small,2021,17(31):2006627.

[14]Tiwari R,Verma D K,Kumar D,Yadav S,Kumar K,Krishnamoorthi S. Ionic conductivity and dielectric properties of bulk SPP-PEG hydrogels as Na+ ion-based SPE materials for energy storage applications [J]. Materials Chemistry Frontiers,2021,5(15):5857.

[15]Zhang Z Z,Xu K Q,Rong X H,Hu Y S,Li H,Huang X J,Chen L Q. Na3.4Zr1.8Mg0.2Si2PO12 filled poly (ethylene oxide)/Na(CF3SO2)2N as flexible composite polymer electrolyte for solid-state sodium batteries [J]. Journal of Power Sources,2017,372:270.

[16]Vignarooban K,Badami P,Dissanayake M,Ravirajan P,Kannan A M. Poly-acrylonitrile-based gel-polymer electrolytes for sodium-ion batteries [J]. Ionics,2017,23:2817.

[17]Manuel J,Zhao X H,Cho K K,Kim J K,Ahn J H. Ultralong life organic sodium ion batteries using a polyimide/multiwalled carbon nanotubes nanocomposite and gel polymer electrolyte [J]. ACS Sustainable Chemistry & Engineering,2018,6(7):8159.

[18]Kumar N,Sahu D K,Mahipal Y K. Effect of TiO2 on ion transport properties and dielectric relaxation of sodium ion-conducting novel PEO/PAN-blended solid polymer electrolyte [J]. Journal of Materials Research,2023,38(9):2506.

[19]Arya A,Sharma A L. Optimization of salt concentration and explanation of two peak percolation in blend solid polymer nanocomposite films [J]. Journal of Solid State Electrochemistry,2018,22:2725.

[20]Duraikkan V,Sultan A B,Nallaperumal N,Shunmuganarayanan A. Structural,thermal and electrical properties of polyvinyl alcohol/poly (vinyl pyrrolidone)-sodium nitrate solid polymer blend electrolyte [J]. Ionics,2018,24:139.

[21]Rao M C,Koutavarapu R,Kumar K V. Structural and electrochemical properties of ZrO2 doped PVP-Na+ based nanocomposite polymer films [J]. Materials Science in Semiconductor Processing,2019,89:41.

[22]Liu Z Z,Li G J,Qin Q,Mi L W,Li G R,Zheng G Q,Liu C T,Li Q,Liu X H. Electrospun PVDF/PAN membrane for pressure sensor and sodium-ion battery separator [J]. Advanced Composites and Hybrid Materials,2021,4:1215.

[23]Janakiraman S,Surendran A,Ghosh S,Anandhan S,Venimadhav A. Electroactive poly (vinylidene fluoride) fluoride separator for sodium ion battery with high coulombic efficiency [J]. Solid State Ionics,2016,292:130.

[24]Ma J L,Yin Y B,Liu T,Zhang X B,Yan J M,Jiang Q. Suppressing sodium dendrites by multifunctional polyvinylidene fluoride (PVDF) interlayers with nonthrough pores and high flux/affinity of sodium ions toward long cycle life sodium oxygen‐batteries [J]. Advanced Functional Materials,2018,28(13):1703931.

[25]Xie D H,Zhang M,Wu Y,Xiang L,Tang Y B. A flexible dual‐ion battery based on sodium‐ion quasi‐solid‐state electrolyte with long cycling life [J]. Advanced Functional Materials,2020,30(5):1906770.

[26]Hashmi S A,Bhat M Y,Singh M K,Sundaram N T K,Raghupathy B P C,Tanaka H. Ionic liquid-based sodium ion-conducting composite gel polymer electrolytes:effect of active and passive fillers [J]. Journal of Solid State Electrochemistry,2016,20:2817.

[27]Suharto Y,Lee Y,Yu J S,Choi W C,Kim K J. Microporous ceramic coated separators with superior wettability for enhancing the electrochemical performance of sodium-ion batteries [J]. Journal of Power Sources,2018,376:184.

[28]Sångeland C,Younesi R,Mindemark J,Brandell D. Towards room temperature operation of all-solid-state Na-ion batteries through polyester-polycarbonate-based polymer electrolytes [J]. Energy Storage Materials,2019,19:31.

[29]Ojanguren A,Mittal N,Lizundia E,Niederberger M. Stable Na electrodeposition enabled by agarose-based water-soluble sodium ion battery separators [J]. ACS Applied Materials & Interfaces,2021,13(18):21250.

[30]Yang J F,Zhang H R,Zhou Q,Qu H T,Dong T T,Zhang M,Tang B,Zhang J J,Cui G L. Safety-enhanced polymer electrolytes for sodium batteries:recent progress and perspectives [J]. ACS Applied Materials & Interfaces,2019,11(19):17109.

[31]Li J Y,Zhu H J,Wang X E,Armand M,MacFaelane D R,Forsyth M. Synthesis of sodium poly [4-styrenesulfonyl (trifluoromethylsulfonyl) imide]-co-ethylacrylate] solid polymer electrolytes [J]. Electrochimica Acta,2015,175:232.

[32]Kim J I,Choi Y G,Ahn Y,Kim D,Park J H. Optimized ion-conductive pathway in UV-cured solid polymer electrolytes for all-solid lithium/sodium ion batteries [J]. Journal of Membrane Science,2021,619:118771.

[33]Zheng J Y,Liu X L,Dian Y L,Chen L J,Zhang X C,Feng X M,Chen W H,Zhao Y F. Stable cross-linked gel terpolymer electrolyte containing methyl phosphonate for sodium ion batteries [J]. Journal of Membrane Science,2019,583:163.

[34]Zheng J Y,Yang Y W,Li W J,Feng X M,Chen W H,Zhao Y F. Novel flame retardant rigid spirocyclic biphosphate based copolymer gel electrolytes for sodium ion batteries with excellent high-temperature performance [J]. Journal of Materials Chemistry A,2020,8(43):22962.

[35]Iijima T,Toyoguchi Y,Eda N. Quasi-solid organic electrolytes gelatinized with polymethyl-methacrylate and their applications for lithium batteries [J]. Denki Kagaku,1985,53(8):619.

[36]Bohnke O,Rousselot C,Gillet P A,Truche C. Gel electrolyte for solid‐state electrochromic cell [J]. Journal of the Electrochemical Society,1992,139(7):1862.

[37]Xue Y,Li X,Quesnel D J. Electrochemical and mechanical properties of sodium-ion conducting cross-linked polymer gel electrolyte [J]. International Journal of Electrochemical Science,2017,12(11):10674.

[38]Verma H,Mishra K,Rai D K. Microporous PVDF-PMMA blend-based gel polymer electrolyte for electrochemical applications:effect of PMMA on electrochemical and structural properties [J]. Journal of Electronic Materials,2022,51:635.

[39]Gabryelczyk A,Smogór H,Swiderska-Mocek A. Highly conductive gel polymer electrolytes for sodium-ion batteries with hard carbon anodes [J]. Electrochimica Acta,2023,439:141645.

[40]Xue Y,Quesnel D J. Synthesis and electrochemical study of sodium ion transport polymer gel electrolytes [J]. RSC Advances,2016,6(9):7504.

[41]Zhao S Z,Che H Y,Chen S L,Tao H X,Liao J P,Liao X Z,Ma Z F. Research progress on the solid electrolyte of solid-state sodium-ion batteries [J]. Electrochemical Energy Reviews,2024,7(1):3.

[42]Zhou C,Bag S,Thangadurai V. Engineering materials for progressive all-solid-state Na batteries [J]. ACS Energy Letters,2018,3(9):2181.

[43]Zhao X F,Zhu M Q,Tang C G,Quan K C,Tong Q S,Cao H W,Jiang J C,Yang H T,Zhang J D. ZIF-8@MXene-reinforced flame-retardant and highly conductive polymer composite electrolyte for dendrite-free lithium metal batteries [J]. Journal of Colloid and Interface Science,2022,620:478.

[44]Mishra K,Arif T,Kumar R,Kumar D. Effect of Al2O3 nanoparticles on ionic conductivity of PVDF-HFP/PMMA blend-based Na+-ion conducting nanocomposite gel polymer electrolyte [J]. Journal of Solid State Electrochemistry,2019,23:2401.

[45]Liu Z H,Wang X X,Chen J J,Tang Y H,Mao Z Y,Wang D J. Gel polymer electrolyte membranes boosted with sodium-conductive β-alumina nanoparticles:application for Na-ion batteries [J]. ACS Applied Energy Materials,2021,4(1):623.

[46]Yao Y W,Wang X X,Dong C L,Chen J J,Wang D J,Mao Z Y. Constructing effective interface for room-temperature beta-Al2O3 based sodium metal batteries [J]. Journal of Power Sources,2022,523:231034.

[47]Shi J,Xiong H G,Yang Y F,Shao H X. Nano-sized oxide filled composite PEO/PMMA/P (VDF-HFP) gel polymer electrolyte for rechargeable lithium and sodium batteries [J]. Solid State Ionics,2018,326:136.

[48]Ling W,Fu N,Yue J P,Zeng X X,Ma Q,Deng Q,Xiao Y,Wan L J,Guo Y G,Wu X W. A flexible solid electrolyte with multilayer structure for sodium metal batteries [J]. Advanced Energy Materials,2020,10(9):1903966.

[49]Yi Q,Zhang W Q,Li S Q,Li X Y,Sun C W. Durable sodium battery with a flexible Na3Zr2Si2PO12-PVDF-HFP composite electrolyte and sodium/carbon cloth anode [J]. ACS Applied Materials & Interfaces,2018,10(41):35039.

[50]Wang X X,Liu Z H,Wang Y Q,Chen J J,Mao Z Y,Wang D J. Conductive Na2Zn2TeO6 filler modified gel polymer electrolyte membranes for application in sodium‐ions batteries [J]. ChemElectroChem,2020,7(24):5021.

[51]Wang X T,Wang X X,Chen J J,Zhao Y,Mao Z Y,Wang D J. Durable sodium battery composed of conductive Ti3C2Tx MXene modified gel polymer electrolyte [J]. Solid State Ionics,2021,365:115655.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24030022

Chinese Library Classification Number:TQ152

Citation Information:

With the continuous development of technology,the demand for energy in human society is increasing day by day. Fossil fuels,as the main source of energy at present,bring about huge carbon dioxide emissions,which exacerbate the greenhouse effect and cause rapid global temperature rise and seriously affecting the global climate. Reducing the use of fossil fuels and developing renewable and sustainable green energy has become a consensus among all the humanity. However,green energy sources such as solar energy,wind energy,hydropower and geothermal energy suffer from temporal and spatial imbalances and instability,making it difficult to meet the sustainable and stable requirements of human society for energy. Therefore,there is an urgent need to increase research on energy storage devices with high energy density and long cycle life to help make up the shortcomings of the green energy that we are suing now. At present,lithium batteries play an important part of large-scale commercial energy storage devices for their good comprehensive performance. They marvelously meet the above requirements while adapt to the needs of the rising industries such as new energy vehicles and smartphones. However,lithium-ion batteries have high costs and the supply of raw materials is difficult to meet the rapidly increasing demand. Reliable substitutes for lithium batteries are needed. Sodium and lithium are located in the same main group in the periodic table with similar chemical properties. Besides,sodium is widely distributed on Earth,thus it is easy to obtain and cost-effective. Sodium ion batteries work in a similar way to lithium-ion batteries. The smaller Stokes radius of sodium ions in solvents helps them achieve higher ion migration rates and numbers,making sodium ion batteries a potential alternative to lithium-ion batteries. Electrolytes,as the medium for ion transport,play an important part of batteries,greatly affecting their overall performance and safety. The electrolyte systems that use organic solvents are widely studied in sodium ion batteries. However,liquid electrolytes are difficult to control the growth of dendrites,resulting in a decrease in the cycling stability and Coulombic efficiency of the battery. Besides,the dendrites piercing through the separator can cause a short circuit in the battery,and may cause serious safety accidents such as leakage of flammable organic electrolytes and explosions. Developing solid electrolytes instead of liquid electrolytes can greatly reduce safety hazards and improve battery performance. Solid electrolytes can be mainly divided into inorganic solid electrolytes,organic solid electrolytes,and composite solid electrolytes according to their composition. The organic polymer solid electrolyte can be divided into gel electrolyte and pure solid electrolyte according to its morphology. Acrylate polymer solid electrolytes have the characteristics of easy availability,wide application,mature process,and good compatibility with electrode materials,making them popular candidate materials for developing new generation secondary batteries with high energy density and safety. Based on this,according to the role of acrylate in electrolyte,this article reviewed the research progress of acrylic polymer electrolytes in sodium ion batteries by dividing them into three categories:acrylate cross-linked copolymer electrolytes,poly-acrylate gel electrolytes,and poly-acrylate composite electrolytes. Acrylate mainly acted as the crosslinking agents in cross-linked electrolytes. While in the poly-acrylate gel electrolytes,the acrylate played the leading role,determining the electrochemical performance of the electrolyte. As for the poly-acrylate composite electrolytes,the acrylate was regarded as the matrix of electrolyte and play an important part of their electrochemical performance. Then their advantages and disadvantages were discussed. The acrylate cross-linked copolymer electrolytes could achieve multiple functions according to different needs,making them adaptable to complex scenarios. However,the electrochemical performance of acrylate crosslinking agents had not been fully utilized. The research on poly-acrylate gel electrolyte mainly focused on polymethyl methacrylate. Their electrochemical performance could satisfy the basic needs of batteries,while poor mechanical performance limited its application. As for the poly-acrylate composite electrolytes,they were the most widely studied acrylate electrolytes for their good comprehensive performance. They combined the advantages of organic and inorganic components,thus possessing excellent electrochemical,mechanical,and processing properties. They could be divided into three categories:composite with other polymers,composite with active inorganic fillers,and composite with inert inorganic fillers. Compositing with other polymers mainly improved their mechanical strength and stability,while compositing with inorganic fillers mainly enhance their ion conductivity. Compositing with inorganic fillers could provide more ion transport pathways,resulting in higher ion conductivity than inert inorganic fillers. However,the proportion of acrylate in composite electrolytes was often less than half,which failed to fully utilize the excellent electrochemical performance of the acrylate matrix. Besides,the influence of acrylate content on electrochemical properties of composite electrolytes was often ignored. More inorganic fillers increased the cost of batteries. Finally,based on the properties of different categories of acrylate electrolyte,this article proposed corresponding optimization strategies and looked forward to their trends of future development.

quote

GB/T 7714-2015 [1] Qingyi Song, Zongyou Li, Jianguo Zhang, et al. Advanced Design of Acrylate Polymers for Solid-State Electrolytes in Sodium-Ion Batteries:Current Advances and Future Perspectives[J]. Chinese Journal of Rare Metals, 2026, 50(3): 439-451. DOI:10.13373/j.cnki.cjrm.XY24030022.
MLA [1] Qingyi Song, et al., "Advanced Design of Acrylate Polymers for Solid-State Electrolytes in Sodium-Ion Batteries:Current Advances and Future Perspectives." Chinese Journal of Rare Metals, vol. 50, no. 3, 2026, pp. 439-451, https://doi.org/10.13373/j.cnki.cjrm.XY24030022.
APA [1] Qingyi Song, Zongyou Li, Jianguo Zhang, & Qiyao Yu. (2026). Advanced Design of Acrylate Polymers for Solid-State Electrolytes in Sodium-Ion Batteries:Current Advances and Future Perspectives. Chinese Journal of Rare Metals, 50(3), 439-451. https://doi.org/10.13373/j.cnki.cjrm.XY24030022
IEEE [1] Qingyi Song, Zongyou Li, Jianguo Zhang, and Qiyao Yu, "Advanced Design of Acrylate Polymers for Solid-State Electrolytes in Sodium-Ion Batteries:Current Advances and Future Perspectives," Chinese Journal of Rare Metals, vol. 50, no. 3, pp. 439-451, 2026, doi: 10.13373/j.cnki.cjrm.XY24030022. keywords: {sodium ion battery;gel polymer electrolyte;acrylate compounds;solid state electrolyte}