Stability of the In-Plane Room Temperature van der Waals Ferromagnet Chromium Ditelluride and Its Conversion to Chromium-Interleaved CrTe2 Compounds Stability of the In-Plane Room Temperature van der Waals Ferromagnet Chromium Ditelluride and Its Conversion to Chromium-Interleaved CrTe2 Compounds AITranslate
Abstract AITranslate
Van der Waals magnetic materials are building blocks for novel kinds of spintronic devices and playgrounds for exploring collective magnetic phenomena down to the two-dimensional limit. Chromium–tellurium compounds are relevant in this perspective. In particular, the 1T phase of CrTe2 has been argued to have a Curie temperature above 300 K, a rare and desirable property in the class of lamellar materials, making it a candidate for practical applications. However, recent literature reveals a strong variability in the reported properties, including magnetic ones. Using electron microscopy, diffraction, and spectroscopy techniques, together with local and macroscopic magnetometry approaches, our work sheds new light on the structural, chemical, and magnetic properties of bulk 1T-CrTe2 exfoliated in the form of flakes having a thickness ranging from few to several tens of nanometers. We unambiguously establish that 1T-CrTe2 flakes are ferromagnetic above room temperature, have an in-plane easy axis of magnetization, and low coercivity, and we confirm that their Raman spectroscopy signatures are two modes: E2g (103.5 cm–1) and A1g (136.5 cm–1). We also prove that thermal annealing causes a phase transformation to monoclinic Cr5Te8 and, to a lesser extent, to trigonal Cr5Te8. In sharp contrast with 1T-CrTe2, none of these compounds have a Curie temperature above room temperature, and they both have perpendicular magnetic anisotropy. Our findings reconcile the apparently conflicting reports in the literature and open opportunities for phase-engineered magnetic properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01256
Chinese Library Classification Number:
Citation Information:
Van der Waals magnetic materials are building blocks for novel kinds of spintronic devices and playgrounds for exploring collective magnetic phenomena down to the two-dimensional limit. Chromium–tellurium compounds are relevant in this perspective. In particular, the 1T phase of CrTe2 has been argued to have a Curie temperature above 300 K, a rare and desirable property in the class of lamellar materials, making it a candidate for practical applications. However, recent literature reveals a strong variability in the reported properties, including magnetic ones. Using electron microscopy, diffraction, and spectroscopy techniques, together with local and macroscopic magnetometry approaches, our work sheds new light on the structural, chemical, and magnetic properties of bulk 1T-CrTe2 exfoliated in the form of flakes having a thickness ranging from few to several tens of nanometers. We unambiguously establish that 1T-CrTe2 flakes are ferromagnetic above room temperature, have an in-plane easy axis of magnetization, and low coercivity, and we confirm that their Raman spectroscopy signatures are two modes: E2g (103.5 cm–1) and A1g (136.5 cm–1). We also prove that thermal annealing causes a phase transformation to monoclinic Cr5Te8 and, to a lesser extent, to trigonal Cr5Te8. In sharp contrast with 1T-CrTe2, none of these compounds have a Curie temperature above room temperature, and they both have perpendicular magnetic anisotropy. Our findings reconcile the apparently conflicting reports in the literature and open opportunities for phase-engineered magnetic properties.
quote
| GB/T 7714-2015 | [1] Anike Purbawati, Suman Sarkar, Sébastien Pairis, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01256. |
| MLA | [1] Anike Purbawati, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01256. |
| APA | [1] Anike Purbawati, Suman Sarkar, Sébastien Pairis, Marek Kostka, Abdellali HadjAzzem, Didier Dufeu, Priyank Singh, Daniel Bourgault, Manuel NuñezRegueiro, Jan Vogel, Julien Renard, Laëtitia Marty, Florentin Fabre, Aurore Finco, Vincent Jacques, Lei Ren, Vivekanand Tiwari, Cedric Robert, Xavier Marie, . . . Johann Coraux. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01256 |
| IEEE | [1] Anike Purbawati, Suman Sarkar, Sébastien Pairis, Marek Kostka, Abdellali HadjAzzem, Didier Dufeu, Priyank Singh, Daniel Bourgault, Manuel NuñezRegueiro, Jan Vogel, Julien Renard, Laëtitia Marty, Florentin Fabre, Aurore Finco, Vincent Jacques, Lei Ren, Vivekanand Tiwari, Cedric Robert, Xavier Marie, Nedjma Bendiab, Nicolas Rougemaille, and Johann Coraux, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01256. keywords: {van der Waals ferromagnets twodimensional materials stability room temperature ferromagnetism CrTe2 Cr5Te8} |