Study of Technical Conditions for the Prereduction of Niobium Concentrate-carbon Pellets AITranslate

Northeastern University;Northeastern University;Northeastern University;Northeastern University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The influence of technical conditions on dephosphorization & deferrization during prereduction in the 'Two step' metallurgy of Nb and Fe has been studied. Optimized technical conditions for Nb/Fe>1. 0 Nb/P>10 Nb-rich slags are obtained. Analysis is made on the Nb-rich slags nad semi-steel structures of by-products.

KeyWords AITranslate

pellets with carbon prereduction Nb-Fe alloy deferrization dephosphorization

1陈义胜,宿洪亮,闫永旺,陈红妃,赵凯.含铌铁矿粉氢气选择性还原过程中磷行为[J].钢铁,2016,51(3):22-26. 被引量:4

1陈义胜,武锦,闫永旺,石强,冯运来,李佳琦.含铌铁矿粉选择性还原富集铌的正交实验研究[J].真空科学与技术学报,2019,39(6):524-528. 被引量:2

2李佳琦,陈义胜,闫永旺,石强,武锦.铝热还原法制备铌铁合金的实验研究[J].金属材料与冶金工程,2019,0(5):53-58.

3陈义胜,石强,闫永旺,武锦,冯运来,李佳琦.含铌铁矿粉氢气选择性还原过程中硫行为的研究[J].矿冶工程,2019,39(5):100-102. 被引量:2

4冯运来,陈义胜,闫永旺,武锦,石强.碳直接还原富铌渣制取铌铁合金温度的影响[J].矿产综合利用,2021(2):141-145.

1马伟,钟祥,贺泽全.包头铌精矿内配碳球团还原行为研究[J].矿冶工程,1996,16(2):51-54. 被引量:4

2张俊卿,冯德荣.N_(235)萃取铌的研究[J].包头钢铁学院学报,1999,18(2):156-158. 被引量:1

3陈宏,韩其勇,胡志高,吴雪平,朱腾.酸洗铌精矿富铌除磷的研究[J].稀有金属,1995,19(2):86-88.

4陈既明.浅谈钽铌湿法冶炼中稀有金属的回收[J].稀有金属与硬质合金,1997,25(4):56-58. 被引量:2

5李建强.火焰原子吸收法测定铌精矿及炉渣中氧化钙[J].北京科技大学学报,1997,19(2):218-222. 被引量:1

6罗会秋.从钽铌冶炼废水中回收钛的工艺研究[J].稀有金属与硬质合金,1997,25(4):19-22. 被引量:2

7张耀华,陈既明.不同浓度的仲辛醇对钽铌的萃取与反萃取性能的影响[J].稀有金属与硬质合金,1996,24(2):6-9. 被引量:3

8陈宏.直接还原法在铌提取上的应用[J].宝钢技术,1998(5):26-29. 被引量:12

9包安文.浅论硅铬合金降碳[J].铁合金,1996,27(3):17-21.

10石应江.高纯铌的制备[J].稀有金属与硬质合金,1995,23(1):41-47. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF841.603[冶金工程—有色金属冶金]

Citation Information:

The influence of technical conditions on dephosphorization & deferrization during prereduction in the 'Two step' metallurgy of Nb and Fe has been studied. Optimized technical conditions for Nb/Fe>1. 0 Nb/P>10 Nb-rich slags are obtained. Analysis is made on the Nb-rich slags nad semi-steel structures of by-products.

quote

GB/T 7714-2015 [1] MA Wei, ZHONG Xiang, HE Ze-quan, et al. Study of Technical Conditions for the Prereduction of Niobium Concentrate-carbon Pellets[J]. Rare Metals and Cemented Carbides, 1995(4): 12-17.
MLA [1] MA Wei, et al., "Study of Technical Conditions for the Prereduction of Niobium Concentrate-carbon Pellets." Rare Metals and Cemented Carbides, no. 4, 1995, pp. 12-17.
APA [1] MA Wei, ZHONG Xiang, HE Ze-quan, & YANG Ying-liang. (1995). Study of Technical Conditions for the Prereduction of Niobium Concentrate-carbon Pellets. Rare Metals and Cemented Carbides(4), 12-17.
IEEE [1] MA Wei, ZHONG Xiang, HE Ze-quan, and YANG Ying-liang, "Study of Technical Conditions for the Prereduction of Niobium Concentrate-carbon Pellets," Rare Metals and Cemented Carbides, no. 4, pp. 12-17, 1995. keywords: {pellets with carbon, prereduction, Nb-Fe alloy,deferrization, dephosphorization}