daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Changing the Structural and Mechanical Anisotropy of Foam-Formed Cellulose Materials by Affecting Bubble–Fiber Interaction with Surfactant AITranslate

VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä; Imperial College London;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä; United Kingdom|Institute for Molecular Science and Engineering;VTT Technical Research Centre of Finland Ltd, FI-40101 Jyväskylä
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cellulose fiber materials suitable for filtering, insulation, protective, and hygiene applications can be formed using aqueous foam as a carrier phase. The subtle fiber–bubble interaction provides a tool which can be utilized to alter both structural and mechanical material properties. Earlier model surface studies have only indicated clear surface-bubble adhesion when both the surface hydrophobicity and surface tension of the solution are high enough. In this work, we first show that for silica model surfaces these basic mechanisms are similar for both nonionic polyethylene glycol sorbitan monolaurate (Tween 20) and anionic sodium dodecyl sulfate (SDS) surfactants. In the second step, thick nonwoven materials were foam formed from hydrophilic or hydrophobic viscose fibers using small amounts of cellulose microfibers (CMFs) to form a bonding agent. There was a clear variation in structure and strength properties between the samples made using different fibers and surfactants. The partial alignment and layering of fibers in the wet foam led to anisotropy in the mechanical properties of the formed samples. Using SDS, the fiber alignment was very strong for hydrophilic fibers but was reduced for hydrophobic fibers because of stronger coupling to bubbles during structure forming, impacting the microscale fiber network. For nonionic Tween 20, in addition to surfactant adsorption on the fibers, the ethoxylated surfactant headgroups are suggested to form bridges between CMFs and other fibers, restricting fiber movements during formation. For hydrophilic fibers, this showed up as a lower in-plane compression modulus but higher transverse strength for Tween 20 compared with SDS surfactant. For hydrophobic fibers, the sensitivity of the mechanical properties on surfactant type was even stronger.

KeyWords AITranslate

foam surfactant cellulose fiber hydrophobicity structure anisotropy mechanical properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01248

Chinese Library Classification Number:

Citation Information:

Cellulose fiber materials suitable for filtering, insulation, protective, and hygiene applications can be formed using aqueous foam as a carrier phase. The subtle fiber–bubble interaction provides a tool which can be utilized to alter both structural and mechanical material properties. Earlier model surface studies have only indicated clear surface-bubble adhesion when both the surface hydrophobicity and surface tension of the solution are high enough. In this work, we first show that for silica model surfaces these basic mechanisms are similar for both nonionic polyethylene glycol sorbitan monolaurate (Tween 20) and anionic sodium dodecyl sulfate (SDS) surfactants. In the second step, thick nonwoven materials were foam formed from hydrophilic or hydrophobic viscose fibers using small amounts of cellulose microfibers (CMFs) to form a bonding agent. There was a clear variation in structure and strength properties between the samples made using different fibers and surfactants. The partial alignment and layering of fibers in the wet foam led to anisotropy in the mechanical properties of the formed samples. Using SDS, the fiber alignment was very strong for hydrophilic fibers but was reduced for hydrophobic fibers because of stronger coupling to bubbles during structure forming, impacting the microscale fiber network. For nonionic Tween 20, in addition to surfactant adsorption on the fibers, the ethoxylated surfactant headgroups are suggested to form bridges between CMFs and other fibers, restricting fiber movements during formation. For hydrophilic fibers, this showed up as a lower in-plane compression modulus but higher transverse strength for Tween 20 compared with SDS surfactant. For hydrophobic fibers, the sensitivity of the mechanical properties on surfactant type was even stronger.

quote

GB/T 7714-2015 [1] Annika E. Ketola, Wenzhe Song, Timo Lappalainen, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01248.
MLA [1] Annika E. Ketola, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01248.
APA [1] Annika E. Ketola, Wenzhe Song, Timo Lappalainen, Kristian Salminen, Janika Viitala, Tuomas Turpeinen, Arttu Miettinen, KoonYang Lee, & Jukka A. Ketoja. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01248
IEEE [1] Annika E. Ketola, Wenzhe Song, Timo Lappalainen, Kristian Salminen, Janika Viitala, Tuomas Turpeinen, Arttu Miettinen, KoonYang Lee, and Jukka A. Ketoja, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01248. keywords: {foam;surfactant;cellulose fiber;hydrophobicity;structure;anisotropy;mechanical properties}