daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Aqueous-Based Polyimine Functionalization of Cellulose Nanofibrils for Effective Drying and Polymer Composite Reinforcement AITranslate

Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; University of Maine; University of Maine; Oak Ridge National Laboratory; University of Maine; Oak Ridge National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A simple strategy was developed to synthesize polyimine-coated cellulose nanofibrils (CNF) for effective CNF drying and composite reinforcement. The polyimine was synthesized in an aqueous medium using a selective hydrophilic and hydrophobic component that forces the polyimine to precipitate, which prevents the reverse imine reaction. The polyimine coating allowed the CNF to be easily oven-dried while maintaining a fibrillar morphology to provide mechanical reinforcement in poly(ethylene terephthalate glycol) (PETG) composites. In comparison, poor mechanical performance and a heterogeneous fracture surface were observed when the coated CNF were incorporated into poly(l-lactide) (PLA) composites. It is hypothesized that intermolecular aromatic–aromatic interactions are formed at the interface between fibers and the polymer matrix in the PETG system, while no such phenomena occur in the PLA system. Overall, this facile strategy to produce modified, easily dried CNF can be adapted to produce polyimine-coated CNF with unique functionalities that are useful in a range of applications.

KeyWords AITranslate

cellulose nanofibrils (CNF) composites polyimine PETG surface treatment
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01286

Chinese Library Classification Number:

Citation Information:

A simple strategy was developed to synthesize polyimine-coated cellulose nanofibrils (CNF) for effective CNF drying and composite reinforcement. The polyimine was synthesized in an aqueous medium using a selective hydrophilic and hydrophobic component that forces the polyimine to precipitate, which prevents the reverse imine reaction. The polyimine coating allowed the CNF to be easily oven-dried while maintaining a fibrillar morphology to provide mechanical reinforcement in poly(ethylene terephthalate glycol) (PETG) composites. In comparison, poor mechanical performance and a heterogeneous fracture surface were observed when the coated CNF were incorporated into poly(l-lactide) (PLA) composites. It is hypothesized that intermolecular aromatic–aromatic interactions are formed at the interface between fibers and the polymer matrix in the PETG system, while no such phenomena occur in the PLA system. Overall, this facile strategy to produce modified, easily dried CNF can be adapted to produce polyimine-coated CNF with unique functionalities that are useful in a range of applications.

quote

GB/T 7714-2015 [1] Meghan E. Lamm, Kai Li, Katie Copenhaver, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01286.
MLA [1] Meghan E. Lamm, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01286.
APA [1] Meghan E. Lamm, Kai Li, Katie Copenhaver, Peter V. Kelly, Hathaithep Senkum, Halil Tekinalp, William M. Gramlich, & Soydan Ozcan. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01286
IEEE [1] Meghan E. Lamm, Kai Li, Katie Copenhaver, Peter V. Kelly, Hathaithep Senkum, Halil Tekinalp, William M. Gramlich, and Soydan Ozcan, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01286. keywords: {cellulose nanofibrils (CNF);composites;polyimine;PETG;surface treatment}