daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Three-Dimensional Liquid-Based Exchangeable Gradient Osmosis Chip for a Permeability Controllable Microfluidic Device AITranslate

Hanyang University; Korea Institute of Industrial Technology; Pusan National University; Purdue University; Pusan National University; Sogang University; Hanyang University; Korea Institute of Industrial Technology; Korea Institute of Industrial Technology; Korea Institute of Industrial Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

3D printing technology has significant potential for use in the field of microfluidics. Microfluidic chips are biochips that have been applied in biomedical areas such as disease diagnosis and drug delivery in vivo. However, traditional 2D manufacturing techniques limit the scope of their fabrication and usage. In addition, membrane-embedded microfluidic chips need intricately designed structures and well-defined nanofiber membranes for delivering specific drugs and filtering out impurities from blood, and it is difficult to respond quickly to the design and production of these complex three-dimensional shapes. Herein, we introduce a liquid-based exchangeable gradient osmosis (LEGO) chip comprising a 3D structured channel printed via a digital light processing system within 10 min and an electrospun nanofiber membrane. The attachment conditions of the nanofiber membranes to the 3D channel were optimized, while the permeability of specific materials was controlled by adjusting the concentration of nanofibers and the flow speed through the 3D channel. We anticipate that the LEGO chip will be used to produce bio-applicable devices for mass transfer in vivo.

KeyWords AITranslate

3D microfluidic chip digital light processing (DLP) nanofiber membrane electrospinning permeability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01072

Chinese Library Classification Number:

Citation Information:

3D printing technology has significant potential for use in the field of microfluidics. Microfluidic chips are biochips that have been applied in biomedical areas such as disease diagnosis and drug delivery in vivo. However, traditional 2D manufacturing techniques limit the scope of their fabrication and usage. In addition, membrane-embedded microfluidic chips need intricately designed structures and well-defined nanofiber membranes for delivering specific drugs and filtering out impurities from blood, and it is difficult to respond quickly to the design and production of these complex three-dimensional shapes. Herein, we introduce a liquid-based exchangeable gradient osmosis (LEGO) chip comprising a 3D structured channel printed via a digital light processing system within 10 min and an electrospun nanofiber membrane. The attachment conditions of the nanofiber membranes to the 3D channel were optimized, while the permeability of specific materials was controlled by adjusting the concentration of nanofibers and the flow speed through the 3D channel. We anticipate that the LEGO chip will be used to produce bio-applicable devices for mass transfer in vivo.

quote

GB/T 7714-2015 [1] Jae Won Choi, Jisun Lee, Jeongho Yang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01072.
MLA [1] Jae Won Choi, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01072.
APA [1] Jae Won Choi, Jisun Lee, Jeongho Yang, Young Won Kim, Suk Hee Park, Seokbeom Kim, Sukjoon Hong, Yong Son, Jisu Han, & Cheol Woo Ha. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01072
IEEE [1] Jae Won Choi, Jisun Lee, Jeongho Yang, Young Won Kim, Suk Hee Park, Seokbeom Kim, Sukjoon Hong, Yong Son, Jisu Han, and Cheol Woo Ha, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01072. keywords: {3D microfluidic chip;digital light processing (DLP);nanofiber membrane;electrospinning;permeability}