Formulation of Chitosan/Gelatin/Pequi Oil Emulsions: Rheological, Thermal, and Antimicrobial Properties AITranslate

National Nanotechnology Laboratory for Agribusiness; University of São Paulo; University of São Paulo; University of São Paulo; University of São Paulo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The search for bioactive compounds to replace synthetic food preservatives has been drawing attention in recent times, as it aims to solve the problem of food loss using a sustainable proposal better accepted by consumers. In this study, natural emulsions of chitosan/gelatin containing pequi oil (CGPO) were obtained. Thermogravimetric analysis allowed inferring the effects of the addition of pequi oil on the thermal stability of the polymeric network of chitosan and gelatin. Rheological deformation tests indicated that all emulsions were more elastic than viscous (G′ > G″), and that the increase in the pequi oil concentration enhanced their elastic behavior. Higher oil concentrations also led to lower gelation temperatures and increased the emulsion viscosity. In addition, emulsions stabilized by CG had long-term storage stability. CGPO emulsions showed a better antimicrobial activity against Staphylococcus aureus when compared to CG, suggesting a synergism between the oil and chitosan in the desired antimicrobial protection. These results offer a strategy for the development and application of emulsions containing natural compounds, disclosing their potential as food additives.

KeyWords AITranslate

emulsions antimicrobial activity chitosan pequi oil food preservatives
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01036

Chinese Library Classification Number:

Citation Information:

The search for bioactive compounds to replace synthetic food preservatives has been drawing attention in recent times, as it aims to solve the problem of food loss using a sustainable proposal better accepted by consumers. In this study, natural emulsions of chitosan/gelatin containing pequi oil (CGPO) were obtained. Thermogravimetric analysis allowed inferring the effects of the addition of pequi oil on the thermal stability of the polymeric network of chitosan and gelatin. Rheological deformation tests indicated that all emulsions were more elastic than viscous (G′ > G″), and that the increase in the pequi oil concentration enhanced their elastic behavior. Higher oil concentrations also led to lower gelation temperatures and increased the emulsion viscosity. In addition, emulsions stabilized by CG had long-term storage stability. CGPO emulsions showed a better antimicrobial activity against Staphylococcus aureus when compared to CG, suggesting a synergism between the oil and chitosan in the desired antimicrobial protection. These results offer a strategy for the development and application of emulsions containing natural compounds, disclosing their potential as food additives.

quote

GB/T 7714-2015 [1] Crisiane A. Marangon, Mirella Romanelli V. Bertolo, Virginia da C Amaro Martins, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01036.
MLA [1] Crisiane A. Marangon, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01036.
APA [1] Crisiane A. Marangon, Mirella Romanelli V. Bertolo, Virginia da C Amaro Martins, Marcia Nitschke, & Ana Maria de Guzzi Plepis. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01036
IEEE [1] Crisiane A. Marangon, Mirella Romanelli V. Bertolo, Virginia da C Amaro Martins, Marcia Nitschke, and Ana Maria de Guzzi Plepis, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01036. keywords: {emulsions;antimicrobial activity;chitosan;pequi oil;food preservatives}