Superior Water-Resistant Poly(2-hydroxyethyl methacrylate phosphate) Flame Retardant and a Transparent, Flame-Retardant, and Biodegradable Poly(lactide) Blend Film AITranslate

Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An environmentally friendly and superefficient flame retardant poly(2-hydroxyethyl methacrylate phosphate) (PHEMAP) was synthesized through precipitated polymerization of 2-hydroxyethyl methacrylate phosphate (HEMAP). The cross-linked PHEMAP microscale particles exhibited superior water resistance and high thermal stability, which could effectively prevent the release of phosphorus-containing compounds into the environment. Poly(lactide) (PLA) with only 0.5 wt % PHEMAP achieved UL-94 V-0 rating, and its limited oxygen index (LOI) value was 28%. Remarkably, the PLA/PHEMAP films maintained good transparency, owing to their similar refractive indices and uniform dispersion of PHEMAP microparticles in the PLA matrix. This study explored a kind of sustainable, transparent, and superefficient flame-retardant PLA blend film to expand its potential application in mobile phones, automotive interiors, and three-dimensional (3D) printing fields.

KeyWords AITranslate

phosphoruscontaining flame retardant flame retardancy PLA water resistance transparency
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01140

Chinese Library Classification Number:

Citation Information:

An environmentally friendly and superefficient flame retardant poly(2-hydroxyethyl methacrylate phosphate) (PHEMAP) was synthesized through precipitated polymerization of 2-hydroxyethyl methacrylate phosphate (HEMAP). The cross-linked PHEMAP microscale particles exhibited superior water resistance and high thermal stability, which could effectively prevent the release of phosphorus-containing compounds into the environment. Poly(lactide) (PLA) with only 0.5 wt % PHEMAP achieved UL-94 V-0 rating, and its limited oxygen index (LOI) value was 28%. Remarkably, the PLA/PHEMAP films maintained good transparency, owing to their similar refractive indices and uniform dispersion of PHEMAP microparticles in the PLA matrix. This study explored a kind of sustainable, transparent, and superefficient flame-retardant PLA blend film to expand its potential application in mobile phones, automotive interiors, and three-dimensional (3D) printing fields.

quote

GB/T 7714-2015 [1] Xiaobing Ma, Han Yun, Ningjing Wu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01140.
MLA [1] Xiaobing Ma, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01140.
APA [1] Xiaobing Ma, Han Yun, Ningjing Wu, Fukun Niu, & Jihang Yu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01140
IEEE [1] Xiaobing Ma, Han Yun, Ningjing Wu, Fukun Niu, and Jihang Yu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01140. keywords: {phosphoruscontaining flame retardant;flame retardancy;PLA;water resistance;transparency}