daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Photoexcitation Dynamics of Thiophene–Fluorene Fluorophore in Matrix Encapsulation for Deep-Blue Amplified Spontaneous Emission AITranslate

Nanjing Tech University (NanjingTech);Madrid Institute for Advanced Studies (IMDEA Nanociencia); Nanjing Tech University (NanjingTech); Nanjing Tech University (NanjingTech); Nanjing University of Posts & Telecommunications; Nanjing University of Posts & Telecommunications; Nanjing Tech University (NanjingTech); Northwestern Polytechnical University (NPU); Nanjing Tech University (NanjingTech); Nanjing Tech University (NanjingTech); Northwestern Polytechnical University (NPU)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Precise control of the photophysical process is crucial to obtain efficient organic laser materials with high optical gain and low optical losses for the realization of organic lasers. Herein, we systematically demonstrated the photophysical process of steric thiophene–fluorene (MC6Cz-Th) fluorophore in an encapsulated polystyrene (PS) matrix for efficient deep-blue amplified spontaneous emission (ASE). MC6Cz-Th presents poor film morphology and low luminous intensity under solid conditions on account of strong intermolecular aggregation and photo-oxidation. Therefore, no ASE can be observed. Upon incorporation of this deep-blue fluorophore into an inert PS matrix, an intermolecular coupling of excited states was efficiently suppressed. To get further insights into the exciton behavior of MC6Cz-Th, a comparison of excited dynamics in a dilute solution, blend film, and neat film was performed using ultrafast transient absorption (TA) spectroscopy. The stimulate emission (SE) and photoinduced absorption (PA) decay curves of MC6Cz-Th in a dilute solution and blend film exhibit quite slow and perfect mirror shape located along the two sides beside the x-axis, indicating that the excitons originate from the same singlet that is dominated by the intrachain interaction. Moreover, the ASE threshold realized in the blend film was 44.3 μJ/cm2, highlighting its potential application in lasing materials.

KeyWords AITranslate

photophysical process thiophene−fluorene encapsulated excited dynamics amplified spontaneous emission
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01092

Chinese Library Classification Number:

Citation Information:

Precise control of the photophysical process is crucial to obtain efficient organic laser materials with high optical gain and low optical losses for the realization of organic lasers. Herein, we systematically demonstrated the photophysical process of steric thiophene–fluorene (MC6Cz-Th) fluorophore in an encapsulated polystyrene (PS) matrix for efficient deep-blue amplified spontaneous emission (ASE). MC6Cz-Th presents poor film morphology and low luminous intensity under solid conditions on account of strong intermolecular aggregation and photo-oxidation. Therefore, no ASE can be observed. Upon incorporation of this deep-blue fluorophore into an inert PS matrix, an intermolecular coupling of excited states was efficiently suppressed. To get further insights into the exciton behavior of MC6Cz-Th, a comparison of excited dynamics in a dilute solution, blend film, and neat film was performed using ultrafast transient absorption (TA) spectroscopy. The stimulate emission (SE) and photoinduced absorption (PA) decay curves of MC6Cz-Th in a dilute solution and blend film exhibit quite slow and perfect mirror shape located along the two sides beside the x-axis, indicating that the excitons originate from the same singlet that is dominated by the intrachain interaction. Moreover, the ASE threshold realized in the blend film was 44.3 μJ/cm2, highlighting its potential application in lasing materials.

quote

GB/T 7714-2015 [1] YaMin Han, Chen Sun, LuBing Bai, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01092.
MLA [1] YaMin Han, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01092.
APA [1] YaMin Han, Chen Sun, LuBing Bai, JinYi Lin, Man Xu, YuYu Liu, XueHua Ding, LingHai Xie, Kang Shen, TianShi Qin, & Wei Huang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01092
IEEE [1] YaMin Han, Chen Sun, LuBing Bai, JinYi Lin, Man Xu, YuYu Liu, XueHua Ding, LingHai Xie, Kang Shen, TianShi Qin, and Wei Huang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01092. keywords: {photophysical process;thiophene−fluorene;encapsulated;excited dynamics;amplified spontaneous emission}