Determination of the W and Mo Content in Nb-W-Mo Alloy with X-ray Fluorescence Spectrometry AITranslate
Abstract AITranslate
The contents of W and Mo in Nb-W-Mo alloy were determined by X-ray fluorescence spectrometer with the optimal measurement condition combination. Based on the corresponding relation between absolute fluorescence intensity and elementary mass fraction, the correction equations were chosen to fit the actual working curves of W and Mo in Nb-W-Mo alloy. The results show that both the precision and accuracy of X-ray fluorescence spectrometry are high enough to compare with national standard chemical test or ICP test.
KeyWords AITranslate
1卢钟录,符宁,宋纯智.实用冶金分析方法与基础[M].沈阳:辽宁科学技术出版社.1990.651-675.
2Berting E P.X射线光谱分析的原理和应用[M].李瑞城,译.北京:国防工业出版社,1983.255.
3盐川二郎.仪器分析导论[M].陈美智,译.北京:化学工业出版社,1988.72.
4彭国靖.X荧光分析和计算机处理在一级标准物质研制中应用[A].岛津公司.第四届岛津XRF用户论文集[C].日本岛津:岛津公司,1992.98-115.
1许宁辉,唐武,于红艳.X荧光光谱法测定铌钨合金中钨、钼、锆元素[J].当代化工,2020,0(1):200-203. 被引量:4
1朱晓晗,张愚若,姜红,陈城洋,陈敏璠.多元分析在鞋套碎片RAMAN检验中的应用[J].化学工程与装备,2020(9):228-230.
2于红燕,唐武,许宁辉,刘昊辰.X射线荧光光谱法测定钽铌矿石中锑[J].化学分析计量,2020,29(6):109-112. 被引量:1
3周海渊,郭世明,宋青锋,赵龙,李凤毅.中子活化煤质分析仪在沙曲选煤厂的应用[J].山西焦煤科技,2021,45(6):8-10. 被引量:2
4赵亚男,王小强,余文丽,杜天军,杨惠玲.X射线荧光光谱法测定铁矿石中主次量组分[J].当代化工,2021,50(10):2517-2520. 被引量:5
1马雅静,吴文琪,许涛.钆镁合金X荧光光谱点滴滤纸片薄样测定法的研究[J].稀土,2012,33(4):73-76. 被引量:1
2朴英华.X射线荧光光谱法测定中低合金钢中的各元素[J].化学分析计量,2007,16(5):35-38. 被引量:7
3马宏彦,杜建民,王兆利,刘颖晓.X射线荧光光谱法测定铁矿石中TFe不确定度评定[J].广东化工,2010,37(8):174-174. 被引量:1
4陈锁志,杨俊睿.X射线荧光光谱测定润滑油中铜[J].光谱实验室,1992,9(3):25-26.
5张春启.X射线荧光光谱法测定润滑油中铁的含量[J].光谱实验室,1992,9(3):38-39. 被引量:2
6郑建明.微波消解ICP-AES法测定润滑油中的铁,镍,铜,锌,硼,磷[J].广州化工,2010,38(2):141-142. 被引量:6
7张奇,郑昱.微波消解ICP-MS法测定土壤中的8种金属元素[J].广东化工,2016,43(9):241-242. 被引量:3
8周宏.电感耦合等离子体发射光谱法(ICP-AES)测定蒙药云香十五味丸中多种元素[J].化学工程与装备,2013(12):157-158. 被引量:1
9杨金辉,张小毅.电感耦合等离子体质谱法测定煤中11种元素[J].冶金分析,2013,33(9):8-13. 被引量:9
10陈秋生,刘烨潼,张强,殷萍,孟兆芳,张玺.电感耦合等离子体质谱法同时测定葡萄中40种痕量元素[J].理化检验:化学分册,2013,49(6):686-690. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:O657.34[理学—分析化学]
Citation Information:
The contents of W and Mo in Nb-W-Mo alloy were determined by X-ray fluorescence spectrometer with the optimal measurement condition combination. Based on the corresponding relation between absolute fluorescence intensity and elementary mass fraction, the correction equations were chosen to fit the actual working curves of W and Mo in Nb-W-Mo alloy. The results show that both the precision and accuracy of X-ray fluorescence spectrometry are high enough to compare with national standard chemical test or ICP test.
quote
| GB/T 7714-2015 | [1] LIU Bai-li, SHI Ai-xia, YU Hong-yan. Determination of the W and Mo Content in Nb-W-Mo Alloy with X-ray Fluorescence Spectrometry[J]. Rare Metals and Cemented Carbides, 2009(2): 31-33. |
| MLA | [1] LIU Bai-li, et al., "Determination of the W and Mo Content in Nb-W-Mo Alloy with X-ray Fluorescence Spectrometry." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 31-33. |
| APA | [1] LIU Bai-li, SHI Ai-xia, & YU Hong-yan. (2009). Determination of the W and Mo Content in Nb-W-Mo Alloy with X-ray Fluorescence Spectrometry. Rare Metals and Cemented Carbides(2), 31-33. |
| IEEE | [1] LIU Bai-li, SHI Ai-xia, and YU Hong-yan, "Determination of the W and Mo Content in Nb-W-Mo Alloy with X-ray Fluorescence Spectrometry," Rare Metals and Cemented Carbides, no. 2, pp. 31-33, 2009. keywords: {X-ray fluorescence spectrometry;Nb-W-Mo alloy;W and Mo content;precision;accuracy} |