Spectrophotometric Determination of the Ba Content in Si-Ca-Ba Alloy by Using Chlorophosphonazo as the Spectral Chromogenic Reagent AITranslate
Abstract AITranslate
The eolour reaction of chlorophosphonazo with barium( Ⅱ ) was studied. And the effects of the coexistent ions on the colour reaction were also investigated. The results show that the chromogenic reagent (chlorophosphonazo) reacts with barium to form a stable green complex in NH3 · H2O-NH4Cl buffer solution of pH10.0. The complex exhibits an absorption maximum at 670 nm with an apparent molar absorptivity of 6.49 × 10^4 L/(mol · cm). The spectrophotometric determination is of high sensitivity obeying Beer's law,when 25 mL sample solution contains 0450 μg barium. The disturbance of Ba determination from Al and Fe can be sheltered by adding triethanolamine and 1,10-phenanthroline monohydrate, and Ca disturbance by adding EGTA-Pb. The Ba content in Si-Ca-Ba alloy can be determined by spectrophotometry with chlorophosphonazo,where the determined result is in good agreement with the certified value and the relative standard deviation (RSD) is less than 2 %.
KeyWords AITranslate
1沙艳梅,赵学沛,王明军,何雪梅.硅钙钡镁合金中钡钙镁的测定[J].岩矿测试,2004,23(4):308-310. 被引量:10
2罗道成,易平贵,陈安国,李佳秋.EDTA络合滴定法测定硅钙钡合金中钙和钡[J].冶金分析,2002,22(2):47-48. 被引量:11
3刘道平,陈先聪,周斌,汪绍红.硅钙钡及硅钡铁合金中钙、钡的测定[J].冶金分析,1996,16(1):54-55. 被引量:13
4孟平,陆军,龙如成.ICP-AES内标法测定硅钙钡合金中的元素[J].金属制品,2005,31(1):45-46. 被引量:9
5陈玉珍,刘迎新.β-环糊精─偶氮氯膦Ⅲ分光光度法测定微量钡[J].湘潭大学自然科学学报,1994,16(1):73-76. 被引量:3
6刘道平.钡-偶氮氯膦Ⅲ-铜(Ⅱ)-邻菲啰啉多元体系的显色反应及其应用[J].化学试剂,1992,14(1):13-14. 被引量:8
7沈令熙,凌蓉.钡—偶氮氯膦Ⅲ—锌—邻啡罗啉混合多核配合物显色反应的研究[J].痕量分析,1989,5(3):16-21. 被引量:5
8王雪莹,薄凤英,魏崇敏,迟少婷.偶氮氯膦Ⅲ吸光光度法测定钢铁中微量钡[J].理化检验:化学分册,2001,37(8):374-375. 被引量:2
1李蓉,任轶,王劲榕,李啸寅,郭春阳.含铅重晶石中硫酸钡的测定[J].云南冶金,2014,43(4):62-65. 被引量:3
2史静,钱庆长,周颖,谢鹏,钱瑞娟.电感耦合等离子体原子发射光谱法测定铜阳极泥中钡[J].冶金分析,2020,40(6):81-85. 被引量:2
3於利慧.两步法熔融制样-X射线荧光光谱法测定硅钙钡合金中9种主次量元素[J].理化检验:化学分册,2021,57(9):840-844. 被引量:2
1王劲榕.2014年云南冶金分析年评[J].云南冶金,2015,44(2):101-109. 被引量:1
2毛香菊,倪文山,肖芳,高小飞,张宏丽.电感耦合等离子体原子发射光谱法测定重晶石选矿流程样品中硫酸钡[J].冶金分析,2016,36(9):47-51. 被引量:4
3孙杨,李冬梅,刘茜,苏丹,刘岩,沈启慧.X射线荧光光谱法辅助测定重晶石中的硫酸钡[J].吉林化工学院学报,2018,35(5):27-29. 被引量:1
4刘文倩,岳元媛,王依平,王茹.硫酸钡比浊法测定食盐中钡含量的优化[J].食品安全质量检测学报,2020,11(19):6910-6914.
5宁骏斌,赵书运,郭海珍.重量法测定铜阳极泥中硫酸钡[J].中国有色冶金,2022,51(2):89-92. 被引量:1
6张秀艳,刘丹娜,张红,包香春.电感耦合等离子体质谱法测定稀土熔盐电解回收料中铝铬镍锌[J].冶金分析,2022,42(9):68-74.
7万芒,刘伟,曾小平.熔融制样-X射线荧光光谱法测定稀土硅铁中11种主次元素[J].冶金分析,2023,43(1):54-61.
1吴丽娟.丁二酮肟分光光度法测定硅钙钡合金中的镍含量[J].冶金标准化与质量,2012(1):33-34.
2钟国秀,杨浩义,黄清华,卢钒.三溴偶氮胂光度法测定硅钙钡合金中钡含量[J].稀有金属与硬质合金,2010,38(1):44-46. 被引量:2
3罗来辉,张莉.对硅钙钡合金中Ca、Ba的连续测定方法的探讨[J].黄山学院学报,2004,6(3):53-53. 被引量:1
4郑会清,王翠翠,张有毅.ICP-OES法测定硅钙钡合金中主量和微量元素[J].广州化工,2013,41(21):98-99. 被引量:3
5张杰,崔红,刘宝林.2,2′-氧联二苯甲酸合钡一维配位聚合物的合成与晶体结构[J].化学研究,2011,22(6):17-20.
6俞长兴,张敏芳,高英立.锌柱还原分光光度法测定微量砷[J].分析化学,1997,25(5):531-533. 被引量:6
7傅君丹,叶莉青,张春艳,温一航.二维钡配位聚合物[Ba(μ_5-1,8-nap)]_n的水热合成、晶体结构和荧光性质(英文)[J].无机化学学报,2011,27(1):179-183. 被引量:1
8赵长容,李卓,连国军,曹建明.蛋白质的偶氮胂Ⅲ-钡(Ⅱ)配合物光谱探针测定[J].分析测试学报,2007,26(6):904-906. 被引量:2
9韩敏敏,陈晓,张依萍,冯云龙.以3,5-二(吡啶-4-甲氧基)苯甲酸为配体构筑的两个钡(Ⅱ)、铅(Ⅱ)配位聚合物(英文)[J].无机化学学报,2014,30(7):1653-1659. 被引量:2
10杜尧国,王君.银(Ⅰ)、铊(Ⅰ)、汞(Ⅰ)、锶(Ⅱ)和钡(Ⅱ)盐的合成与表征──8-羟基喹啉合十钒酸盐的研究(Ⅴ)[J].吉林大学自然科学学报,1994(4):113-114.
Basic Information:
DOI:
Chinese Library Classification Number:O657.32[理学—分析化学]
Citation Information:
The eolour reaction of chlorophosphonazo with barium( Ⅱ ) was studied. And the effects of the coexistent ions on the colour reaction were also investigated. The results show that the chromogenic reagent (chlorophosphonazo) reacts with barium to form a stable green complex in NH3 · H2O-NH4Cl buffer solution of pH10.0. The complex exhibits an absorption maximum at 670 nm with an apparent molar absorptivity of 6.49 × 10^4 L/(mol · cm). The spectrophotometric determination is of high sensitivity obeying Beer's law,when 25 mL sample solution contains 0450 μg barium. The disturbance of Ba determination from Al and Fe can be sheltered by adding triethanolamine and 1,10-phenanthroline monohydrate, and Ca disturbance by adding EGTA-Pb. The Ba content in Si-Ca-Ba alloy can be determined by spectrophotometry with chlorophosphonazo,where the determined result is in good agreement with the certified value and the relative standard deviation (RSD) is less than 2 %.
quote
| GB/T 7714-2015 | [1] ZHONG Guo-xiu, YANG Hao-yi, HUANG Qing-hua. Spectrophotometric Determination of the Ba Content in Si-Ca-Ba Alloy by Using Chlorophosphonazo as the Spectral Chromogenic Reagent[J]. Rare Metals and Cemented Carbides, 2009(2): 34-36. |
| MLA | [1] ZHONG Guo-xiu, et al., "Spectrophotometric Determination of the Ba Content in Si-Ca-Ba Alloy by Using Chlorophosphonazo as the Spectral Chromogenic Reagent." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 34-36. |
| APA | [1] ZHONG Guo-xiu, YANG Hao-yi, & HUANG Qing-hua. (2009). Spectrophotometric Determination of the Ba Content in Si-Ca-Ba Alloy by Using Chlorophosphonazo as the Spectral Chromogenic Reagent. Rare Metals and Cemented Carbides(2), 34-36. |
| IEEE | [1] ZHONG Guo-xiu, YANG Hao-yi, and HUANG Qing-hua, "Spectrophotometric Determination of the Ba Content in Si-Ca-Ba Alloy by Using Chlorophosphonazo as the Spectral Chromogenic Reagent," Rare Metals and Cemented Carbides, no. 2, pp. 34-36, 2009. keywords: {chlorophosphonazo;spectrophotometry;Ba content;Si-Ca-Ba alloy} |