Study on Microstructure and Tensile Properties of New γ-TiAl Alloy Sheet AITranslate

Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The microstructure of newγ-TiAl alloy sheet before and after rolling was investigated as well as its tensile properties after rolling.The results show that the forged microstructure before rolling mainly containsγphase,α2 phase and a certain amount of B2/βphase.After rolling,the coarse lamellar microstructure decreases and recrystallized isometricγgrains increase.The lamellar clusters are elongated along the rolling direction,and their broken degree is related to rolling deformation.The number of B2/βphase is significantly reduced due to high temperature rolling.After three cycles of heat treatment in the(γ+α2)phase zone,the alloy lamellar microstructure increases,lamellar space decreases,and the microstructure is significantly refined.The high-temperature tensile plasticity of the sheet is relatively high,and its high-temperature tensile fracture mainly has the mixed features of translamellar facture,interlamellar facture and transgrain facture.

KeyWords AITranslate

γ-TiAl alloy sheet hot-pack rolling microstructure tensile property tensile fracture

1陈玉勇,苏勇君,孔凡涛.TiAl金属间化合物制备技术的研究进展[J].稀有金属材料与工程,2014,43(3):757-762. 被引量:40

2林均品,陈国良.TiAl基金属间化合物的发展[J].中国材料进展,2009,28(1):31-37. 被引量:71

3张俊红,黄伯云,贺跃辉,周科朝,唐建成.TiAl基合金板材制备技术的发展现状[J].材料导报,2002,16(2):16-18. 被引量:12

4陈玉勇,孔凡涛,崔宁.TiAl合金板材的制备与组织分析[J].中国材料进展,2015,34(5):379-382. 被引量:7

5王刚,徐磊,崔玉友,杨锐.Ti-47Al-2Cr-2Nb-0.2W-0.15B合金板材的制备及其拉伸性能[J].中国有色金属学报,2010,20(B10):274-279. 被引量:3

1王微,陈武,彭德林.热处理对Ti-48Al-2Cr合金组织与力学性能的影响[J].材料热处理学报,2019,0(6):75-80.

1宋庆功,赵俊普,顾威风,甄丹丹,郭艳蕊,李泽朋.影响Nb替位掺杂γ-TiAl基合金延性的电子性质因素[J].稀有金属,2018,42(7):705-712. 被引量:4

2李路娜,胡旭.弱化织构提高汽车镁合金板材冲压成形性能研究[J].热加工工艺,2017,46(21):106-108. 被引量:1

3陈永光.做硬质材料领域的领导者[J].现代制造,2018,0(21):20-20.

4陈纪强,戴青松,桑高锋,赵明伟.工艺参数对5754铝合金组织和性能的影响[J].材料科学,2018,8(3):137-143. 被引量:1

5莫林波,唐政山,乔小银,杨寅柯.茶多酚对氧化偶氮甲烷/葡聚糖硫酸钠诱导高脂饮食小鼠结直肠癌的影响[J].科学技术与工程,2017,17(26):189-195. 被引量:4

6丁春辉,刘长军.AA7075超硬铝合金双脉冲MIG焊-机械振动联合工艺优化[J].热加工工艺,2018,47(9):216-218. 被引量:5

7胥福顺,张劲,邓运来,张新明.蛇形轧制对Al-Cu-Mg合金板材强韧性能及微观组织的影响[J].中国有色金属学报,2017,27(10):2005-2011. 被引量:6

8李文渊,刘建荣,陈志勇,赵子博,王清江.Ti60合金板材的室温强度与其显微组织和织构的关系[J].材料研究学报,2018,32(6):455-463. 被引量:8

9胡晓青,房洪杰,王艳娟,孙杰,尹登峰,吕正风.Ti和Ce对2524铝合金组织和力学性能的影响[J].金属热处理,2018,43(6):41-45. 被引量:3

10王玉航,汪进凯,傅泽航,王昊,何燕霖,鲁晓刚.γ-TiAl金属间化合物4种剪切变形方式的第一性原理计算[J].上海金属,2018,40(3):6-10. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

The microstructure of newγ-TiAl alloy sheet before and after rolling was investigated as well as its tensile properties after rolling.The results show that the forged microstructure before rolling mainly containsγphase,α2 phase and a certain amount of B2/βphase.After rolling,the coarse lamellar microstructure decreases and recrystallized isometricγgrains increase.The lamellar clusters are elongated along the rolling direction,and their broken degree is related to rolling deformation.The number of B2/βphase is significantly reduced due to high temperature rolling.After three cycles of heat treatment in the(γ+α2)phase zone,the alloy lamellar microstructure increases,lamellar space decreases,and the microstructure is significantly refined.The high-temperature tensile plasticity of the sheet is relatively high,and its high-temperature tensile fracture mainly has the mixed features of translamellar facture,interlamellar facture and transgrain facture.

quote

GB/T 7714-2015 [1] LUO Yuan-yuan, YANG Fan, ZHAO Bin, et al. Study on Microstructure and Tensile Properties of New γ-TiAl Alloy Sheet[J]. Rare Metals and Cemented Carbides, 2018(4): 64-68.
MLA [1] LUO Yuan-yuan, et al., "Study on Microstructure and Tensile Properties of New γ-TiAl Alloy Sheet." Rare Metals and Cemented Carbides, no. 4, 2018, pp. 64-68.
APA [1] LUO Yuan-yuan, YANG Fan, ZHAO Bin, SU Hang-biao, GUO Di-zi, & WU Jin-ping. (2018). Study on Microstructure and Tensile Properties of New γ-TiAl Alloy Sheet. Rare Metals and Cemented Carbides(4), 64-68.
IEEE [1] LUO Yuan-yuan, YANG Fan, ZHAO Bin, SU Hang-biao, GUO Di-zi, and WU Jin-ping, "Study on Microstructure and Tensile Properties of New γ-TiAl Alloy Sheet," Rare Metals and Cemented Carbides, no. 4, pp. 64-68, 2018. keywords: {γ-TiAl alloy sheet;hot-pack rolling;microstructure;tensile property;tensile fracture}