Determination of Cobalt in Cobalt-containing Fine Organic Chemicals AITranslate
Abstract AITranslate
This paper describes the direct titration of cobalt at PH 5~6 in hexamethylenetetramine medium using xylenol orange and malachite green as indicator and EDTA as titratant. This method is simple and fast and has been satisfactorily used for the determination of cobalt in cobalt-containing fine organic chemicals,such as paint drier isooctoatal cobalt and rubber adhesion promoter cobalt borate acylate.
KeyWords AITranslate
1秦毅红,何汉兵,程玉贤,黄草明.异辛酸钴合成工艺研究[J].有色金属:冶炼部分,2005(6):39-41. 被引量:5
1周若尘,王兴隆,翁齐菲.催干剂异辛酸锌的合成工艺[J].精细与专用化学品,2013,21(3):38-40.
2万宇,单玉华,施骏,田媛,郑一天,冯洋洋,李明时,鲁墨弘.无碱条件下氧气催化氧化2-乙基己醇合成2-乙基己酸[J].精细化工,2016,33(6):654-659.
3陈巧,谢平波,许鹏.陶瓷渗透墨水用异辛酸铁的合成及墨水性能研究[J].中国陶瓷,2018,54(1):62-68. 被引量:3
4杨声海,李为轮,吴彦增,王长红,陈永明.异辛酸镍的电化学合成[J].中南大学学报:自然科学版,2019,50(7):1521-1526.
5吴孟德,李广慈,李明时,李学兵,庄庆发,陈松.镍钴助催化剂对环烷酸钼催化煤沥青悬浮床加氢反应活性的影响[J].燃料化学学报,2021,49(1):27-36. 被引量:1
1汪家铭.四种具有开发前景的精细有机化学品[J].上海化工,1999,24(17):41-41. 被引量:1
2韩莹,黄嘉梓.羰基化反应及其在有机合成上的应用[J].化工时刊,1996,10(10):3-6. 被引量:1
3具有开发价值的几种精细有机化学品[J].精细化工经济与技术信息,2000(4):6-7.
4李祖光,高云芳.氧化钴中钴快速测定[J].中国陶瓷,1999,35(1):22-23. 被引量:6
5具有开发前景的四种精细有机化学品[J].试剂与精细化学品,2000(9):15-16.
6环烷酸钴的制备[J].精细化工经济与技术信息,2002(10):15-15.
7薛连海,于龙.合成异辛酸钴工艺条件的研究[J].吉林石油化工,1991(3):8-10. 被引量:1
8张华军,张锐峰,李化全.电位滴定法测定异辛酸钴中的钴含量[J].山东化工,2000,29(2):43-44. 被引量:1
9李建兰,刘佳.醋酸储罐放空尾气处理技术研究[J].化工安全与环境,2015,0(14):17-18.
10李祖光,高昳.2-乙基己酸[J].浙江化工,1995,26(4):50-52.
Basic Information:
DOI:
Chinese Library Classification Number:TQ207.4[化学工程—有机化工]
Citation Information:
This paper describes the direct titration of cobalt at PH 5~6 in hexamethylenetetramine medium using xylenol orange and malachite green as indicator and EDTA as titratant. This method is simple and fast and has been satisfactorily used for the determination of cobalt in cobalt-containing fine organic chemicals,such as paint drier isooctoatal cobalt and rubber adhesion promoter cobalt borate acylate.
quote
| GB/T 7714-2015 | [1] LI Zu-guang, CHENG Ben-cheng. Determination of Cobalt in Cobalt-containing Fine Organic Chemicals[J]. Rare Metals and Cemented Carbides, 1996(2): 43-45. |
| MLA | [1] LI Zu-guang, and CHENG Ben-cheng. "Determination of Cobalt in Cobalt-containing Fine Organic Chemicals." Rare Metals and Cemented Carbides, no. 2, 1996, pp. 43-45. |
| APA | [1] LI Zu-guang, & CHENG Ben-cheng. (1996). Determination of Cobalt in Cobalt-containing Fine Organic Chemicals. Rare Metals and Cemented Carbides(2), 43-45. |
| IEEE | [1] LI Zu-guang and CHENG Ben-cheng, "Determination of Cobalt in Cobalt-containing Fine Organic Chemicals," Rare Metals and Cemented Carbides, no. 2, pp. 43-45, 1996. keywords: {cobalt,EDTA titration,fine organic chemicals} |