Development and Commercial Practice of Digesting-solvent Extraction-crystallization Technique for Processing Wolframite in China AITranslate
Abstract AITranslate
This paper presents the development of wolframite digesting-solvent extraction-crystallization technique in China and its commercial practice for fourteen years at Zhuzhou Cemented Carbide Factory, Hunan.This advanced technique, offers the advantages of simple flowsheet, high metal recoveries and excellent product quality.Owing to its successful application, China has caught up with the world advanced levels in metallulgy of wolframite.
KeyWords AITranslate
1林伯颖.关于我国硬质合金工业科技进步的研讨[J].硬质合金,1994,11(4):246-251. 被引量:2
1万林生,徐国钻,严永海,聂华平,赵立夫,肖学有.中国钨冶炼工艺发展历程及技术进步[J].中国钨业,2009,24(5):63-66. 被引量:20
2彭伟,黄健,王振杰,刘安荣.钨冶炼渣中有价金属回收利用研究现状[J].化工进展,2022,41(12):6656-6663.
1万林生,赵立夫,李红超.崇义章源钨业APT绿色冶炼的技术进步和发展[J].中国钨业,2012,27(1):47-49. 被引量:13
2傅清青,李荫璐,杨金德,卢燕琼.某钨业公司白钨矿生产仲钨酸铵建设项目职业病危害控制效果评价[J].中国卫生工程学,2012,11(2):117-120.
3万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18
4王明.钨冶炼离子交换工艺技术的研究进展[J].稀有金属与硬质合金,2013,41(6):13-16. 被引量:8
5万林生,舒柳飞,赵立夫,谌勇明,李红超.黑钨矿与碳酸钙人工合成白钨的反应过程和机理[J].稀有金属与硬质合金,2014,42(2):1-4. 被引量:3
6李琼芳.钨提取技术的中国专利现状[J].有色金属科学与工程,2014,5(3):65-69. 被引量:1
7万林生,黄小晶,杨亮,邓登飞,李红超,谌勇明.钨酸钠溶液氢氧化钙苛化-沉淀白钨的研究[J].有色金属科学与工程,2014,5(4):23-27. 被引量:3
8刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4
9万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.
10于亮,吴绍祖,程红光.季铵盐GW05和N263对Na_2WO_4溶液的萃钨性能对比研究[J].稀有金属,2015,39(3):193-200. 被引量:2
1邓舜勤.离子交换法提取钨的新工艺[J].湿法冶金,1996,15(1):34-38. 被引量:7
2霍广生,孙培梅,贾根贵.关于钨钼分离的可能方法[J].稀有金属与硬质合金,1997,25(1):52-56. 被引量:12
3Barry J.Welch,郑宏.铝电解技术进入第二个世纪[J].轻金属,1989(11):34-40.
4高清举.布袋除尘和球式热风炉技术进入新阶段[J].南方钢铁,1991(3):16-18.
5尹树普,赵静.离子交换工艺解吸钨过程中Cl、P、Sn等杂质行为的研究[J].中国钨业,2000,15(2):27-28. 被引量:1
6孙君泉.塔兰托烧结厂生产发展与改造经验[J].国外钢铁,1993,18(12):5-7.
7石明柱.仲钨酸铵的粒度与形貌对掺杂钨丝性能的影响[J].稀有金属材料与工程,1994,23(6):36-40. 被引量:3
8纳洪良,杨汝全.钨精矿中钨的氧化还原滴定法[J].冶金分析,1997,17(3):41-43. 被引量:2
9李汉广,彭志辉.氟化物CVD法直接制取特纯高致密异型钨制品[J].稀有金属材料与工程,1994,23(6):74-77. 被引量:13
10林振坚.DCS在压力反应釜自控系统中的应用[J].中国钨业,2001,16(5):108-109.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.104[冶金工程—有色金属冶金]
Citation Information:
This paper presents the development of wolframite digesting-solvent extraction-crystallization technique in China and its commercial practice for fourteen years at Zhuzhou Cemented Carbide Factory, Hunan.This advanced technique, offers the advantages of simple flowsheet, high metal recoveries and excellent product quality.Owing to its successful application, China has caught up with the world advanced levels in metallulgy of wolframite.
quote
| GB/T 7714-2015 | [1] LIU Mo-xi. Development and Commercial Practice of Digesting-solvent Extraction-crystallization Technique for Processing Wolframite in China[J]. Rare Metals and Cemented Carbides, 1996(2): 48-50. |
| MLA | [1] LIU Mo-xi. "Development and Commercial Practice of Digesting-solvent Extraction-crystallization Technique for Processing Wolframite in China." Rare Metals and Cemented Carbides, no. 2, 1996, pp. 48-50. |
| APA | [1] LIU Mo-xi. (1996). Development and Commercial Practice of Digesting-solvent Extraction-crystallization Technique for Processing Wolframite in China. Rare Metals and Cemented Carbides(2), 48-50. |
| IEEE | [1] LIU Mo-xi, "Development and Commercial Practice of Digesting-solvent Extraction-crystallization Technique for Processing Wolframite in China," Rare Metals and Cemented Carbides, no. 2, pp. 48-50, 1996. keywords: {wolframite metallurgy, digesting, solvent extraction,technical development, commercial practice} |