Magnetic Field Sensor Based on a OLED/Organic Photodetector Stack Magnetic Field Sensor Based on a OLED/Organic Photodetector Stack AITranslate

National Institute of Standards and Technology; National Institute of Standards and Technology; National Institute of Standards and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, an all-organic magnetic field sensor based on an organic light-emitting diode (OLED) and organic photodetector (OPD) layer stack is presented. This sensor opens possibilities to create printable, flexible magnetic field sensors using commercially viable components, allowing magnetic field sensors to be simply integrated into the existing OLED technology. The sensor function is driven by the large magneto-electroluminescence (MEL) of a thermally activated delayed fluorescence (TADF)-emitter-based OLED, which in reference devices have shown an MEL of about 60% for magnetic fields on the order of 10 mT. Maximum sensitivity of about 0.15 nA/mT (150 μV/mT or 15 mV/kG with amplification) is achieved at a magnetic field of 3–4 mT. While the detectivity is limited to ∼10–3 T·Hz–1/2, we show this can be improved upon as the magnetic field detection sensitivity of OLEDs measured by an external Si-detector is about an order of magnitude higher. Sensitivity of 2 nA/mT and detectivities better than 10–5 T·Hz –1/2 are demonstrated, and the intrinsic detectivity limit is estimated to be on the order of 10–9 T·Hz –1/2.

KeyWords AITranslate

magnetometer organic lightemitting diodes thermally assisted delayed fluorescence magnetic field response organicShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00745

Chinese Library Classification Number:

Citation Information:

In this study, an all-organic magnetic field sensor based on an organic light-emitting diode (OLED) and organic photodetector (OPD) layer stack is presented. This sensor opens possibilities to create printable, flexible magnetic field sensors using commercially viable components, allowing magnetic field sensors to be simply integrated into the existing OLED technology. The sensor function is driven by the large magneto-electroluminescence (MEL) of a thermally activated delayed fluorescence (TADF)-emitter-based OLED, which in reference devices have shown an MEL of about 60% for magnetic fields on the order of 10 mT. Maximum sensitivity of about 0.15 nA/mT (150 μV/mT or 15 mV/kG with amplification) is achieved at a magnetic field of 3–4 mT. While the detectivity is limited to ∼10–3 T·Hz–1/2, we show this can be improved upon as the magnetic field detection sensitivity of OLEDs measured by an external Si-detector is about an order of magnitude higher. Sensitivity of 2 nA/mT and detectivities better than 10–5 T·Hz –1/2 are demonstrated, and the intrinsic detectivity limit is estimated to be on the order of 10–9 T·Hz –1/2.

quote

GB/T 7714-2015 [1] Sebastian Engmann, Emily G. Bittle, David J. Gundlach. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00745.
MLA [1] Sebastian Engmann, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00745.
APA [1] Sebastian Engmann, Emily G. Bittle, & David J. Gundlach. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00745
IEEE [1] Sebastian Engmann, Emily G. Bittle, and David J. Gundlach, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00745. keywords: {magnetometer organic lightemitting diodes thermally assisted delayed fluorescence magnetic field response organicShow More}