daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of Organic Matter Removal from Industrial H_2TaF_7 Solution by Active Carbon AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of removal of organic matter from industrial H_2TaF_7 solution by active carbon in order to reduce carbon content in K_2TaF_7 crystal.The test results showed that active carbon can reduce COD value in H_2TaF_7 solution,consequently reduce carbon content in K_2TaF_7 crystal from 0.002 5%~0.003 0% to 0.001.0 %~0.001 5%, and the percloration & absorption factor reached 70In addition,there is linear relationship between COD value in H_2TaF_7 solution and carbon content in K_2TaF_7 crystal,the carbon content in K_2TaF_7 crystal decreases with the decreasing of COD value in H_2TaF_7 solution.When COD value is lower than 8 mg/L,carbon content in K_2TaF_7 crystal would be reduced down to less than 0.001 5%.

KeyWords AITranslate

absorption Ta solution active carbon organic matter removal

1何季麟,刘红东,卢振达,马春红.高比容钽粉关键技术及应用开发研究[J].材料导报,2000,14(5):8-9. 被引量:4

2唐晓风.钽粉杂质含量对钽电容器性能的影响[J].电子元件与材料,1998,17(1):38-39. 被引量:4

3刘传雪,赖永玲.氟钽酸钾中碳存在形式的探讨[J].分析试验室,1994,13(2):23-24. 被引量:5

4车荣睿.吸附树脂在有机物分离,提取和回收中的应用(上)[J].天津化工,1990(2):29-31. 被引量:2

5Yeh Ruth Yu-Li,et al.Textile wastewater treatment with activated sludge and powdered activated carbon[J].International Journal of Environmental Studies,2002,59(5): 607.

6马峥,张振良,于惠芳.活性炭对水中有机物去除的研究[J].环境保护,1999,27(5):41-44. 被引量:33

7Gander M A,et al.Membrane bioreactors for use in small wastewater treatment plants:membrane materials and effluent quality[J].Water Science and Technology,2000,41(1): 205.

8Croli B T. Membrane technology.The way forward[J].Journal of the Institution of Water and Environment Management,1992,6(2):121.

9唐建军,周康根.减压膜蒸馏及其应用于易挥发性有机物分离的研究现状[J].水处理技术,2002,28(2):67-70. 被引量:11

10唐建军,周康根,张启修,李青刚,马荣骏.实验条件对减压膜蒸馏法脱除水溶液中MIBK的影响[J].水处理技术,2002,28(1):22-24. 被引量:5

1王璞,闵小波,柴立元,王云燕,方艳,常皓,袁林.颗粒活性炭对乳酸钠的吸附及其特性[J].中国有色金属学报,2007,17(6):1008-1013. 被引量:2

2邱衍嵩.氟钽酸钾结晶工艺研究[J].广东化工,2014,41(13):76-77. 被引量:1

3洪根德.树脂除油法在制取低碳氟钽酸钾中的实验研究[J].中国金属通报,2020(12):183-184.

1尤翔宇,杨杰,王云燕,苏艳蓉,柴立元,舒余德.苯酚在活性炭上的吸附模型[J].中国有色金属学报,2012,22(10):2924-2929. 被引量:14

2宋忠来,徐东彦,张宇松,程飞.煤质活性炭对苯酚吸附动力学研究[J].山东化工,2015,44(3):4-5. 被引量:4

3洪根德.树脂除油法在制取低碳氟钽酸钾中的实验研究[J].中国金属通报,2020(12):183-184.

1洪志成.海鑫6号高炉溜槽穿漏判断及处理措施[J].炼铁技术通讯,2005,0(4):7-8.

2刘兰田.无钟炉顶溜槽穿漏和脱落事故[J].炼铁,1989,8(6):5-7.

3余新明,吴学军,吕先昌.布袋收尘穿漏监测及定位技术现状与展望[J].工业安全与环保,2005,31(5):13-14. 被引量:4

4王欢,邰盛彪,贺小塘,韩守礼,吴喜龙,李勇,刘文,马明涛,谭明亮.双氧水行业含钯废催化剂回收工艺的研究[J].贵金属,2013,34(S01):4-7. 被引量:4

5袁艺,陈义.铝酸钠溶液中有机物排除试验研究[J].广州化工,2014,42(5):59-60. 被引量:3

6陈文汨,陈学刚.焙烧氧化法在去除拜耳法有机物中的应用(下)[J].轻金属,2008(9):13-16. 被引量:4

7陈文汨,陈学刚.焙烧氧化法在去除拜耳法有机物中的应用(上)[J].轻金属,2008(8):10-12. 被引量:11

8包福毅,杨明德,方军,张志庚,何培炯,朱大和.采用离心萃取器萃取净化氯化浸出镍溶液[J].矿冶工程,1995,15(1):42-47. 被引量:4

9鄢艳.澳矿生产氧化铝采用一二段分解技术的联合对比分析[J].中国高新技术企业,2015(11):156-157. 被引量:2

10陆富汉,胡明轩,梁志华.40吨钢包包衬新工艺的开发与应用[J].柳钢科技,2003(1):18-19.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

Study is made of removal of organic matter from industrial H_2TaF_7 solution by active carbon in order to reduce carbon content in K_2TaF_7 crystal.The test results showed that active carbon can reduce COD value in H_2TaF_7 solution,consequently reduce carbon content in K_2TaF_7 crystal from 0.002 5%~0.003 0% to 0.001.0 %~0.001 5%, and the percloration & absorption factor reached 70In addition,there is linear relationship between COD value in H_2TaF_7 solution and carbon content in K_2TaF_7 crystal,the carbon content in K_2TaF_7 crystal decreases with the decreasing of COD value in H_2TaF_7 solution.When COD value is lower than 8 mg/L,carbon content in K_2TaF_7 crystal would be reduced down to less than 0.001 5%.

quote

GB/T 7714-2015 [1] LI Qing-gang, ZHANG Qi-xiu, ZHOU Kang-gen. Study of Organic Matter Removal from Industrial H_2TaF_7 Solution by Active Carbon[J]. Rare Metals and Cemented Carbides, 2004(4): 1-3.
MLA [1] LI Qing-gang, et al., "Study of Organic Matter Removal from Industrial H_2TaF_7 Solution by Active Carbon." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 1-3.
APA [1] LI Qing-gang, ZHANG Qi-xiu, & ZHOU Kang-gen. (2004). Study of Organic Matter Removal from Industrial H_2TaF_7 Solution by Active Carbon. Rare Metals and Cemented Carbides(4), 1-3.
IEEE [1] LI Qing-gang, ZHANG Qi-xiu, and ZHOU Kang-gen, "Study of Organic Matter Removal from Industrial H_2TaF_7 Solution by Active Carbon," Rare Metals and Cemented Carbides, no. 4, pp. 1-3, 2004. keywords: {absorption;Ta solution;active carbon;organic matter removal}