daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Promoting Energy Storage Performance of Sr0.7Ba0.3Nb2O6 Tetragonal Tungsten Bronze Ceramic by a Two-Step Sintering Technique AITranslate

Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; China Jiliang University; Hangzhou Dianzi University; Hangzhou Dianzi University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Dielectric ceramic capacitors have attracted immense interest because of their remarkable power density and excellent charging–discharging performance. Tetragonal tungsten bronze (TTB)-based ferroelectrics are the second large category of ferroelectric materials. However, they have not received enough appreciation in the dielectric capacitor field because of their poor energy storage properties. In this study, a two-step sintering technique was employed to prepare TTB relaxor ferroelectric ceramic Sr0.7Ba0.3Nb2O6 (SBN70), aiming to promote its energy storage performance. Remarkable recoverable energy storage density (Wrec ∼ 3.2 J/cm3) and excellent efficiency (η ∼ 90%) were realized simultaneously, which profited from the reduction of the average grain size and the enhancement of the breakdown strength. Moreover, the ceramic also exhibited an ultrashort discharge time (<65 ns), great discharge current density (789.8 A/cm2), and large power density (79 MW/cm3). The obtained results indicate the immense potential of TTB structure relaxor ferroelectric ceramics for energy storage applications.

KeyWords AITranslate

tetragonal tungsten bronze ceramic relaxor ferroelectric twostep sintering energy storage
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01091

Chinese Library Classification Number:

Citation Information:

Dielectric ceramic capacitors have attracted immense interest because of their remarkable power density and excellent charging–discharging performance. Tetragonal tungsten bronze (TTB)-based ferroelectrics are the second large category of ferroelectric materials. However, they have not received enough appreciation in the dielectric capacitor field because of their poor energy storage properties. In this study, a two-step sintering technique was employed to prepare TTB relaxor ferroelectric ceramic Sr0.7Ba0.3Nb2O6 (SBN70), aiming to promote its energy storage performance. Remarkable recoverable energy storage density (Wrec ∼ 3.2 J/cm3) and excellent efficiency (η ∼ 90%) were realized simultaneously, which profited from the reduction of the average grain size and the enhancement of the breakdown strength. Moreover, the ceramic also exhibited an ultrashort discharge time (<65 ns), great discharge current density (789.8 A/cm2), and large power density (79 MW/cm3). The obtained results indicate the immense potential of TTB structure relaxor ferroelectric ceramics for energy storage applications.

quote

GB/T 7714-2015 [1] Chong Luo, Chenghao Zhu, Yuhao Liang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01091.
MLA [1] Chong Luo, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01091.
APA [1] Chong Luo, Chenghao Zhu, Yuhao Liang, Peng Zheng, Wangfeng Bai, Lili Li, Fei Wen, Jingji Zhang, Liang Zheng, & Yang Zhang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01091
IEEE [1] Chong Luo, Chenghao Zhu, Yuhao Liang, Peng Zheng, Wangfeng Bai, Lili Li, Fei Wen, Jingji Zhang, Liang Zheng, and Yang Zhang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01091. keywords: {tetragonal tungsten bronze ceramic relaxor ferroelectric twostep sintering energy storage}