daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Segmented Highly Reversible Thermochromic Layered Perovskite [(CH2)2(NH3)2]CuCl4 Crystal Coupled with an Inverse Magnetocaloric Effect AITranslate

National Taiwan University; National Taiwan University; National Taiwan University; National Cheng Kung University; National Taiwan University;Institute of Physics; National Taiwan University; National Taiwan University;Institute of Physics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The layered, lead-free hybrid perovskites are superior in organic electronics compared to their three-dimensional (3D) counterparts due to their facile synthesis and promising stability to various environmental conditions. To learn more about the multifunctional side of such materials, a layered perovskite (EDA)CuCl4 [EDA is (CH2)2(NH3)2] crystal was grown in solution and crystallographically characterized by single-crystal X-ray diffraction. The crystal is thermally very stable and exhibits a high reversible thermochromic working temperature (∼503 K), intense conductivity changes with temperature, and strong exotic magnetic properties. The structural changes of the crystal with temperature are monitored and explained by powder X-ray diffraction and UV–vis absorption. The absorption band of the crystal shows little variation after repeated heating/cooling cycles, indicating admirable stability. Moreover, the Cu hybrid consists of a strong ferromagnetic interaction in antiferromagnetically coupled layers with a Néel temperature of about 34 K. The magnetocaloric effect of the crystal was investigated and found to be inverse due to the magnetic entropy change associated with the antiferromagnetic transition and the strong ferromagnetic interaction, indicating the suitability of the perovskite hybrid as a candidate for an environmentally friendly low-temperature magnetic cooling technology. The overall results promise a potential multipurpose two-dimensional (2D) perovskite for future electronic applications in a wide temperature range.

KeyWords AITranslate

2D perovskite single crystal thermochromism magnetocaloric effect antiferromagnetism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01108

Chinese Library Classification Number:

Citation Information:

The layered, lead-free hybrid perovskites are superior in organic electronics compared to their three-dimensional (3D) counterparts due to their facile synthesis and promising stability to various environmental conditions. To learn more about the multifunctional side of such materials, a layered perovskite (EDA)CuCl4 [EDA is (CH2)2(NH3)2] crystal was grown in solution and crystallographically characterized by single-crystal X-ray diffraction. The crystal is thermally very stable and exhibits a high reversible thermochromic working temperature (∼503 K), intense conductivity changes with temperature, and strong exotic magnetic properties. The structural changes of the crystal with temperature are monitored and explained by powder X-ray diffraction and UV–vis absorption. The absorption band of the crystal shows little variation after repeated heating/cooling cycles, indicating admirable stability. Moreover, the Cu hybrid consists of a strong ferromagnetic interaction in antiferromagnetically coupled layers with a Néel temperature of about 34 K. The magnetocaloric effect of the crystal was investigated and found to be inverse due to the magnetic entropy change associated with the antiferromagnetic transition and the strong ferromagnetic interaction, indicating the suitability of the perovskite hybrid as a candidate for an environmentally friendly low-temperature magnetic cooling technology. The overall results promise a potential multipurpose two-dimensional (2D) perovskite for future electronic applications in a wide temperature range.

quote

GB/T 7714-2015 [1] Somrita Dutta, Deepak Vishnu S. K, Sudipta Som, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01108.
MLA [1] Somrita Dutta, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01108.
APA [1] Somrita Dutta, Deepak Vishnu S. K, Sudipta Som, Rajneesh Chaurasiya, Dinesh Kumar Patel, Kalimuthu Moovendaran, ChengChieh Lin, ChunWei Chen, & Raman Sankar. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01108
IEEE [1] Somrita Dutta, Deepak Vishnu S. K, Sudipta Som, Rajneesh Chaurasiya, Dinesh Kumar Patel, Kalimuthu Moovendaran, ChengChieh Lin, ChunWei Chen, and Raman Sankar, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01108. keywords: {2D perovskite single crystal thermochromism magnetocaloric effect antiferromagnetism}