Embedding Quaternary V1–x–ySrxWyO2 into Multilayer Systems to Enhance Its Thermochromic Properties for Smart Glass Applications AITranslate

Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen; Justus Liebig University Giessen
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Smart window glazing technology possesses a great potential for reducing the overall energy demand in the building sector. Thin films based on thermochromic vanadium dioxide (VO2) are ideally suited as functional layers of thermochromic smart windows. VO2 itself exhibits a significant change in optical transparency and reflectivity in the infrared spectrum. However, the optimization of VO2-based thin films for application as intelligent window glazing is still ongoing. The improvement is rather tedious because the key parameters set by the application such as transmittance modulation ΔT2500, luminous transmittance Tlum, solar transmittance modulation ΔTsol, and transition temperature ϑc affect each other. Codoping of VO2 with strontium (Sr) and tungsten (W) drives the parameters close to the desired range. However, the requirements set for the use as smart window coating cannot be fully met. Here, we show by a systematic comparison of simulations and experiments that embedding a layer of thermochromic V1–x–ySrxWyO2 between an optimized TiO2 buffer and a TiO2 antireflection layer already adds additional degrees of freedom to simultaneously fulfill all smart window requirements for the optical parameters ΔT2500, Tsol, Tlum, and ΔTsol. In particular, the luminous transmittance Tlum is improved by not less than ≈10% in such a trilayer structure.

KeyWords AITranslate

thermochromism vanadium dioxide codoping smart windows buffer layer antireflection layer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01115

Chinese Library Classification Number:

Citation Information:

Smart window glazing technology possesses a great potential for reducing the overall energy demand in the building sector. Thin films based on thermochromic vanadium dioxide (VO2) are ideally suited as functional layers of thermochromic smart windows. VO2 itself exhibits a significant change in optical transparency and reflectivity in the infrared spectrum. However, the optimization of VO2-based thin films for application as intelligent window glazing is still ongoing. The improvement is rather tedious because the key parameters set by the application such as transmittance modulation ΔT2500, luminous transmittance Tlum, solar transmittance modulation ΔTsol, and transition temperature ϑc affect each other. Codoping of VO2 with strontium (Sr) and tungsten (W) drives the parameters close to the desired range. However, the requirements set for the use as smart window coating cannot be fully met. Here, we show by a systematic comparison of simulations and experiments that embedding a layer of thermochromic V1–x–ySrxWyO2 between an optimized TiO2 buffer and a TiO2 antireflection layer already adds additional degrees of freedom to simultaneously fulfill all smart window requirements for the optical parameters ΔT2500, Tsol, Tlum, and ΔTsol. In particular, the luminous transmittance Tlum is improved by not less than ≈10% in such a trilayer structure.

quote

GB/T 7714-2015 [1] Florian Kuhl, Martin Becker, Sebastian L. Benz, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01115.
MLA [1] Florian Kuhl, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01115.
APA [1] Florian Kuhl, Martin Becker, Sebastian L. Benz, Jonas Hauptmann, Jill Kessler, Sangam Chatterjee, Angelika Polity, & Peter J. Klar. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01115
IEEE [1] Florian Kuhl, Martin Becker, Sebastian L. Benz, Jonas Hauptmann, Jill Kessler, Sangam Chatterjee, Angelika Polity, and Peter J. Klar, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01115. keywords: {thermochromism vanadium dioxide codoping smart windows buffer layer antireflection layer}