First-principles study of structural stabilities, electronic and elastic properties of BaF2 under high pressure AITranslate

Baicheng Normal College; Hebei Normal University of Science and Technology; Hebei Normal University of Science and Technology; Hebei Normal University of Science and Technology; Hebei Normal University of Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A theoretical investigation on the structural stabilities, electronic and elastic properties of BaF2 under high pressure is conducted using first-principles calculations based on density functional theory (DFT) with the plane wave basis set as implemented in the CASTEP code. Our results demonstrate that the sequence of the pressure-induced structure transition of BaF2 is from the fluorite (β) structure to the PbCl2-type (α) structure, to the Ni2In-type (γ) structure. The transition pressures are 2.83 and 12.7 GPa, respectively. The energy gap increases with pressure in β and α structures, then begin to decreases in γ structure above 60 GPa. The band gap overlap metallization, however, does not occur up to 210 GPa. The pressure effect on the elastic properties of β-BaF2 is investigated.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.05.045

Chinese Library Classification Number:

Citation Information:

A theoretical investigation on the structural stabilities, electronic and elastic properties of BaF2 under high pressure is conducted using first-principles calculations based on density functional theory (DFT) with the plane wave basis set as implemented in the CASTEP code. Our results demonstrate that the sequence of the pressure-induced structure transition of BaF2 is from the fluorite (β) structure to the PbCl2-type (α) structure, to the Ni2In-type (γ) structure. The transition pressures are 2.83 and 12.7 GPa, respectively. The energy gap increases with pressure in β and α structures, then begin to decreases in γ structure above 60 GPa. The band gap overlap metallization, however, does not occur up to 210 GPa. The pressure effect on the elastic properties of β-BaF2 is investigated.

quote

GB/T 7714-2015 [1] Xiaocui Yang, Aimin Hao, Xiaoming Wang, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.045.
MLA [1] Xiaocui Yang, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.045.
APA [1] Xiaocui Yang, Aimin Hao, Xiaoming Wang, Xin Liu, & Yan Zhu. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.045
IEEE [1] Xiaocui Yang, Aimin Hao, Xiaoming Wang, Xin Liu, and Yan Zhu, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.045.