Research Progress on Recycling Technology of Cathode Materials of Waste Lithium Iron Phosphate Batteries AITranslate
Abstract AITranslate
The ingredients,performance indicators and recycling value of cathode materials of waste lithium iron phosphate batteries are analyzed.The latest research progress on the current recycling technology of cathode materials of waste lithium iron phosphate batteries,including physical methods(magnetic separa-tion,flotation,and gravity separation)and chemical methods(dry methods and wet methods),is reviewed in detail.Finally,the development direction and challenges of the recycling technology of cathode materials of waste lithium iron phosphate batteries are pointed out,aiming at promoting the recycling and sustainable utilization of cathode materials of waste lithium iron phosphate batteries.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:X705[环境科学与工程—环境工程]
Citation Information:
The ingredients,performance indicators and recycling value of cathode materials of waste lithium iron phosphate batteries are analyzed.The latest research progress on the current recycling technology of cathode materials of waste lithium iron phosphate batteries,including physical methods(magnetic separa-tion,flotation,and gravity separation)and chemical methods(dry methods and wet methods),is reviewed in detail.Finally,the development direction and challenges of the recycling technology of cathode materials of waste lithium iron phosphate batteries are pointed out,aiming at promoting the recycling and sustainable utilization of cathode materials of waste lithium iron phosphate batteries.
quote
| GB/T 7714-2015 | [1] ZHOU Yong, TAN Xin, CHEN Yu-yang, et al. Research Progress on Recycling Technology of Cathode Materials of Waste Lithium Iron Phosphate Batteries[J]. Rare Metals and Cemented Carbides, 2024(5): 109-114. |
| MLA | [1] ZHOU Yong, et al., "Research Progress on Recycling Technology of Cathode Materials of Waste Lithium Iron Phosphate Batteries." Rare Metals and Cemented Carbides, no. 5, 2024, pp. 109-114. |
| APA | [1] ZHOU Yong, TAN Xin, CHEN Yu-yang, HUANG Zong-peng, & SHI Run-feng. (2024). Research Progress on Recycling Technology of Cathode Materials of Waste Lithium Iron Phosphate Batteries. Rare Metals and Cemented Carbides(5), 109-114. |
| IEEE | [1] ZHOU Yong, TAN Xin, CHEN Yu-yang, HUANG Zong-peng, and SHI Run-feng, "Research Progress on Recycling Technology of Cathode Materials of Waste Lithium Iron Phosphate Batteries," Rare Metals and Cemented Carbides, no. 5, pp. 109-114, 2024. keywords: {waste lithium iron phosphate battery;cathode material;recycling technology;research progress;development direction} |