daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Comprehensive Recycling Technology of Waste Lithium Batteries AITranslate

China International Engineering Design and Research Institute Co.,Ltd.;China International Engineering Design and Research Institute Co.,Ltd.;China International Engineering Design and Research Institute Co.,Ltd.;China International Engineering Design and Research Institute Co.,Ltd.;China International Engineering Design and Research Institute Co.,Ltd.;China International Engineering Design and Research Institute Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To address the environmental pollution caused by waste lithium iron phosphate batteries and the shortage of lithium resources,an innovative bipolar membrane method was proposed using recycled waste lithium iron phosphate batteries as the raw materials.LiOH was prepared from acid leached Li2SO4 by bi-polar membrane electrodialysis,then refined Li2CO3 was obtained,and battery grade LiFePO4 cathode ma-terial was ultimately prepared.The main processes include crushing and sorting of lithium iron phosphate battery,black powder leaching,impurity removal of material liquid,and synthesis of iron phosphate and lithium iron phosphate,thereby obtaining the main products of Li2CO3 and FePO4 and by-products such as aluminum particles and copper particles.Through synthesis regeneration technology,LiFePO4 cathode ma-terials that meet the gradeⅠstandard in GB/T 30835-2014 are obtained.The prepared LiFePO4 products have a first coulombic efficiency of over 96%and a rate performance of over 94.5%.This process achieves the goal of saving production costs of LiFePO4 and realizing the recycling of renewable resources.

KeyWords AITranslate

lithium iron phosphate battery recycling crushing and sorting hydrometallurgy bipolar mem-brane Li2CO3
No data

Basic Information:

DOI:

Chinese Library Classification Number:X705[环境科学与工程—环境工程]

Citation Information:

To address the environmental pollution caused by waste lithium iron phosphate batteries and the shortage of lithium resources,an innovative bipolar membrane method was proposed using recycled waste lithium iron phosphate batteries as the raw materials.LiOH was prepared from acid leached Li2SO4 by bi-polar membrane electrodialysis,then refined Li2CO3 was obtained,and battery grade LiFePO4 cathode ma-terial was ultimately prepared.The main processes include crushing and sorting of lithium iron phosphate battery,black powder leaching,impurity removal of material liquid,and synthesis of iron phosphate and lithium iron phosphate,thereby obtaining the main products of Li2CO3 and FePO4 and by-products such as aluminum particles and copper particles.Through synthesis regeneration technology,LiFePO4 cathode ma-terials that meet the gradeⅠstandard in GB/T 30835-2014 are obtained.The prepared LiFePO4 products have a first coulombic efficiency of over 96%and a rate performance of over 94.5%.This process achieves the goal of saving production costs of LiFePO4 and realizing the recycling of renewable resources.

quote

GB/T 7714-2015 [1] CHEN Yu-yang, LIU Yong, ZHOU Cheng-qian, et al. Research on Comprehensive Recycling Technology of Waste Lithium Batteries[J]. Rare Metals and Cemented Carbides, 2024(5): 103-108.
MLA [1] CHEN Yu-yang, et al., "Research on Comprehensive Recycling Technology of Waste Lithium Batteries." Rare Metals and Cemented Carbides, no. 5, 2024, pp. 103-108.
APA [1] CHEN Yu-yang, LIU Yong, ZHOU Cheng-qian, ZHOU Yong, ZHOU Yang, & LUO Jia. (2024). Research on Comprehensive Recycling Technology of Waste Lithium Batteries. Rare Metals and Cemented Carbides(5), 103-108.
IEEE [1] CHEN Yu-yang, LIU Yong, ZHOU Cheng-qian, ZHOU Yong, ZHOU Yang, and LUO Jia, "Research on Comprehensive Recycling Technology of Waste Lithium Batteries," Rare Metals and Cemented Carbides, no. 5, pp. 103-108, 2024. keywords: {lithium iron phosphate battery;recycling;crushing and sorting;hydrometallurgy;bipolar mem-brane;LiCO}