Effect of Beryllium Bead Raw Material and Smelting Process on Yield of Beryllium Ingots AITranslate
Abstract AITranslate
Vacuum induction smelting experiments were carried out using beryllium beads with different magnesium contents and different particle size ratios,and the effect of the chemical composition and particle size of the beryllium beads on the yield of beryllium ingots was investigated.Based on the long-term accumulated production experience,the influences of design and manufacture of beryllium oxide crucible,control of smelting power,smelting vacuum,casting temperature and speed on the yield of beryllium ingots are discussed.The experimental results show that the beryllium ingot yield is increased by 5%~8% on ave-rage,by strictly controlling the magnesium content(<0.8%)of the raw beryllium beads,scientifically matching the particle size of beryllium beads and reasonably arranging the furnace loading sequence,carefully designing and manufacturing beryllium oxide crucibles,and controlling the smelting power,vacuum,casting temperature and speed.
KeyWords AITranslate
1王妤.基于专利数据的熔炼法制备镍基高温合金的技术研究及发展分析[J].有色冶金节能,2021,37(5):82-88.
2管金鑫,李艳阳,杜春玮,赵慧.吉林镇赉县农民的施肥误区及测土配方施肥技术的应用[J].农业工程技术,2021,41(23):39-39. 被引量:1
3李坤,李伟伟,康国强,张开兴.提高计算机硬盘驱动臂用铝合金圆锭清洁度工艺研究[J].中国科技期刊数据库 科研,2021(5):00070-00073.
4李强,杨必文,章小兵,郑朝振,刘三平.废线路板自热熔炼渣物化性能研究[J].有色金属工程,2021,11(7):114-120. 被引量:1
5张星,娄方亮.褐煤粉成型试验研究[J].云南化工,2021,48(6):29-31.
6张帅,任毅,王爽,高红.装炉温度对管线用高强度宽厚板性能和组织的影响[J].材料热处理学报,2021,42(10):87-94.
7高峰(文/图),陶磊(文/图).扫码点餐绘出新“食”代[J].解放军生活,2021(9):56-56.
Basic Information:
DOI:
Chinese Library Classification Number:TF824[冶金工程—有色金属冶金]
Citation Information:
Vacuum induction smelting experiments were carried out using beryllium beads with different magnesium contents and different particle size ratios,and the effect of the chemical composition and particle size of the beryllium beads on the yield of beryllium ingots was investigated.Based on the long-term accumulated production experience,the influences of design and manufacture of beryllium oxide crucible,control of smelting power,smelting vacuum,casting temperature and speed on the yield of beryllium ingots are discussed.The experimental results show that the beryllium ingot yield is increased by 5%~8% on ave-rage,by strictly controlling the magnesium content(<0.8%)of the raw beryllium beads,scientifically matching the particle size of beryllium beads and reasonably arranging the furnace loading sequence,carefully designing and manufacturing beryllium oxide crucibles,and controlling the smelting power,vacuum,casting temperature and speed.
quote
| GB/T 7714-2015 | [1] MOU Peng-yuan, WANG Dong-xin, LI Jun-yi, et al. Effect of Beryllium Bead Raw Material and Smelting Process on Yield of Beryllium Ingots[J]. Rare Metals and Cemented Carbides, 2021(5): 13-16. |
| MLA | [1] MOU Peng-yuan, et al., "Effect of Beryllium Bead Raw Material and Smelting Process on Yield of Beryllium Ingots." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 13-16. |
| APA | [1] MOU Peng-yuan, WANG Dong-xin, LI Jun-yi, & XIE Yao. (2021). Effect of Beryllium Bead Raw Material and Smelting Process on Yield of Beryllium Ingots. Rare Metals and Cemented Carbides(5), 13-16. |
| IEEE | [1] MOU Peng-yuan, WANG Dong-xin, LI Jun-yi, and XIE Yao, "Effect of Beryllium Bead Raw Material and Smelting Process on Yield of Beryllium Ingots," Rare Metals and Cemented Carbides, no. 5, pp. 13-16, 2021. keywords: {beryllium ingot;yield;beryllium bead;magnesium content;particle size ratio;smelting process} |