Abstract AITranslate
The reduction smelting process was used to process wolframite alkali-leaching residue and recover valuable elements such as Fe,Mn,W,Sn and Nb in the form of alloys,and the harmful elements such as As and Pb were separated.The effects of reducing agent(graphite powder)dosage,smelting temperature and time on smelting efficiency were studied.The experimental results show that the alloying rates of Fe,Mn,W,Sn and Nb in wolframite alkali-leaching residue are 88.67%,56.28%,98.23%,67.74% and 84.72%,respectively,when reducing agent dosage is 16%,smelting temperature is 1550℃,and smelting time is 120 min.Meanwhile,As,Pb and Bi basically enter the smoke and dust.
KeyWords AITranslate
1汪加军,王晓辉,黄波,郑诗礼.废钨渣中钽、铌、钨高效共提新工艺研究[J].有色金属科学与工程,2013,4(5):91-96. 被引量:12
2苏正夫,刘宇晖.钨渣中钨回收利用新工艺研究[J].稀有金属与硬质合金,2014,42(4):11-13. 被引量:13
3范泽坤,黄超,徐国钻,杨正锋,胡家园,唐孝江,梁勇.钨冶炼渣酸分解减量资源化实验研究[J].稀有金属与硬质合金,2020,48(2):1-4. 被引量:4
4杨秀丽,王晓辉,向仕彪,孙青,魏昶,郑诗礼.盐酸法富集钨渣中的钽和铌[J].中国有色金属学报,2013,23(3):873-881. 被引量:21
5戴艳阳,钟海云,李荐,钟晖.钨渣中有价金属综合回收工艺[J].中南工业大学学报,2003,34(1):36-39. 被引量:24
6肖超,刘景槐,吴海国.低品位钨渣处理工艺试验研究[J].湖南有色金属,2012,28(4):24-26. 被引量:19
7张立,钟晖,戴艳阳.钨渣酸浸与钠碱熔融回收钽铌的研究[J].稀有金属与硬质合金,2008,36(2):6-9. 被引量:21
8戴艳阳,钟晖,钟海云.废钨渣中同时回收铁锰的实验研究[J].应用化工,2009,38(6):924-927. 被引量:11
9罗仙平,刘北林,唐敏康.从钨冶炼渣中综合回收有价金属的试验研究[J].中国钨业,2005,20(3):24-26. 被引量:20
10何旭初,范鹏,周渝生,杨天钧,董一诚.高炉中铌还原产生的碳化铌滞留带[J].北京科技大学学报,1990,12(6):504-509. 被引量:7
1刘永刚.中频电炉维修技术探讨[J].休闲,2021(21):0245-0245.
2於利慧.两步法熔融制样-X射线荧光光谱法测定硅钙钡合金中9种主次量元素[J].理化检验:化学分册,2021,57(9):840-844. 被引量:2
3邓中一,王宗礼,李长明,查全性.卟啉化合物的电催化行为(Ⅵ)--在经热处理的载于石墨上的四对甲氧基苯基卟啉钴电极上半胱氨酸氧化反应的动力学研究[J].高等学校化学学报,1987,8(5):453-458.
Basic Information:
DOI:
Chinese Library Classification Number:TF805.1[冶金工程—有色金属冶金]
Citation Information:
The reduction smelting process was used to process wolframite alkali-leaching residue and recover valuable elements such as Fe,Mn,W,Sn and Nb in the form of alloys,and the harmful elements such as As and Pb were separated.The effects of reducing agent(graphite powder)dosage,smelting temperature and time on smelting efficiency were studied.The experimental results show that the alloying rates of Fe,Mn,W,Sn and Nb in wolframite alkali-leaching residue are 88.67%,56.28%,98.23%,67.74% and 84.72%,respectively,when reducing agent dosage is 16%,smelting temperature is 1550℃,and smelting time is 120 min.Meanwhile,As,Pb and Bi basically enter the smoke and dust.
quote
| GB/T 7714-2015 | [1] LIAO Chun-fa, WANG Liang-hui, HUO Rui-hao, et al. Study on Recovery of Valuable Metals from Wolframite Alkali-leaching Residue by Reduction Smelting[J]. Rare Metals and Cemented Carbides, 2021(5): 7-12. |
| MLA | [1] LIAO Chun-fa, et al., "Study on Recovery of Valuable Metals from Wolframite Alkali-leaching Residue by Reduction Smelting." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 7-12. |
| APA | [1] LIAO Chun-fa, WANG Liang-hui, HUO Rui-hao, XIE Sui, GUO Shao-yu, & LIU De-gang. (2021). Study on Recovery of Valuable Metals from Wolframite Alkali-leaching Residue by Reduction Smelting. Rare Metals and Cemented Carbides(5), 7-12. |
| IEEE | [1] LIAO Chun-fa, WANG Liang-hui, HUO Rui-hao, XIE Sui, GUO Shao-yu, and LIU De-gang, "Study on Recovery of Valuable Metals from Wolframite Alkali-leaching Residue by Reduction Smelting," Rare Metals and Cemented Carbides, no. 5, pp. 7-12, 2021. keywords: {wolframite alkali-leaching residue;reduction smelting;valuable element;harmful element;alloy-ing rate;recovery} |