Effect of Ti Addition on Microstructure and Properties of Sintered NdFeB Magnets AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sintered(PrNd)29.8Tb1Dy0.2Cu0.5Al0.2Co1.5B0.99TixFe(x=00.8)magnets with different Ti content were prepared by intergranular alloying,and their microstructure,magnetic properties and mechanical properties were studied.The results show that the magnet grain can be effectively refined by adding Ti.The proper addition of Ti can improve intrinsic coercivity force and squareness of the magnets,but decrease the remanence and maximum magnetic energy product.Furthermore,Ti addition can decrease the bending strength of the magnets without no obvious effect on their hardness.

KeyWords AITranslate

sintered NdFeB magnet titanium intergranular alloying microstructure magnetic property mechanical property

1李安华,董生智,李卫.烧结NdFeB永磁材料的力学性能及断裂行为的各向异性[J].稀有金属材料与工程,2003,32(8):631-634. 被引量:20

1孔梦燃,田晓,王瑜,夏峰,孙彩娜,伟伟,姚占全.烧结钕铁硼磁体的组织结构及合金成分优化研究进展[J].材料导报,2023,37(S01):313-321.

1唐杰,魏成富,王晓军,赵导文,邹萍.非均一形状烧结NdFeB磁体的耐蚀性研究[J].稀有金属与硬质合金,2017,45(6):41-43.

2电专.专利集锦[J].磁性材料及器件,2017,48(5):70-72.

3满田囡,张林,项兆龙,王文斌,高建文,王恩刚.添加Ti对Al-Bi难混溶合金组织和性能的影响[J].物理学报,2018,67(3):169-175. 被引量:5

4周燕.高丰度稀土添加对NdFeB微观结构及性能影响[J].福建冶金,2017,46(5):44-46. 被引量:1

5吕蒙,孔拓,朱明原,胡业旻,金红明,李文献,李瑛.非稀土金属及合金化合物改性烧结NdFeB磁体的研究进展[J].上海师范大学学报:自然科学版,2017,46(6):899-911.

6霍知节.永磁材料的“前世今生”——从“司南”到“钕铁硼”[J].新材料产业,2018,0(2):70-74. 被引量:1

7詹朋璇,卢超,杨仕清,史卫梅.锶铁氧体改性研究现状与进展[J].磁性材料及器件,2018,49(1):64-68. 被引量:3

8王海艳,笪秋攀,郑开宏,龙骏,路建宁.Nb/Ti对过共晶高铬铸铁组织及性能影响[J].铸造技术,2018,39(2):267-270. 被引量:1

9陈俪钊,王玉华,杨蓉,李佳伟,黄叶,马颖涵.磁场强度对各向异性粘结NdFeB磁体性能的影响[J].科技经济导刊,2017(24):101-101. 被引量:1

10张国清,黄有林,侯育花,李志浩,石志强.Ce掺杂对Nd-Fe-B快淬薄带结构及磁性能影响[J].南昌航空大学学报:自然科学版,2017,31(3):67-72.

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

Sintered(PrNd)29.8Tb1Dy0.2Cu0.5Al0.2Co1.5B0.99TixFe(x=00.8)magnets with different Ti content were prepared by intergranular alloying,and their microstructure,magnetic properties and mechanical properties were studied.The results show that the magnet grain can be effectively refined by adding Ti.The proper addition of Ti can improve intrinsic coercivity force and squareness of the magnets,but decrease the remanence and maximum magnetic energy product.Furthermore,Ti addition can decrease the bending strength of the magnets without no obvious effect on their hardness.

quote

GB/T 7714-2015 [1] YU Jun, JIANG Feng, CHEN Yun-zhi, et al. Effect of Ti Addition on Microstructure and Properties of Sintered NdFeB Magnets[J]. Rare Metals and Cemented Carbides, 2017(6): 44-47.
MLA [1] YU Jun, et al., "Effect of Ti Addition on Microstructure and Properties of Sintered NdFeB Magnets." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 44-47.
APA [1] YU Jun, JIANG Feng, CHEN Yun-zhi, LIU Yu-hui, ZHU Wang-wei, PENG Yan, & WANG Chuan. (2017). Effect of Ti Addition on Microstructure and Properties of Sintered NdFeB Magnets. Rare Metals and Cemented Carbides(6), 44-47.
IEEE [1] YU Jun, JIANG Feng, CHEN Yun-zhi, LIU Yu-hui, ZHU Wang-wei, PENG Yan, and WANG Chuan, "Effect of Ti Addition on Microstructure and Properties of Sintered NdFeB Magnets," Rare Metals and Cemented Carbides, no. 6, pp. 44-47, 2017. keywords: {sintered NdFeB magnet;titanium;intergranular alloying;microstructure;magnetic property;mechanical property}