daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Experimental Study on TiO_2 Nanoparticles Prepared by Gaseous Detonation AITranslate

School of Civil Engineering, Liaoning University of Technology;School of Civil Engineering, Liaoning University of Technology;School of Civil Engineering, Liaoning University of Technology;School of Civil Engineering, Liaoning University of Technology;School of Civil Engineering, Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using the premixed H2/Air as explosion source,TiO2 nanoparticles were prepared by gaseous detonation in a self-made explosion reaction tube.The variation law was discussed of the detonation pressure in the tube under different initial conditions(initial temperature of 25200℃and H2/Air mixing ratio of 0.20.8).Particle size,composition of crystal phase and morphologies of TiO2 nanoparticles synthesized by detonation at different initial temperature and calcinated at high temperature were characterized by means of XRD and TEM.The results show that the end of the explosion reaction tube has the largest detonation pressure when the premixed H2/Air with the chemical equivalent ratio is employed as explosion source.The detonation pressure at the tube end is increased eventually increased by 39.03% with the increase of H2/Air mixing ratio,and the increasing rate firstly increases and then decreases.However,the detonation pressure at the tube end is reduced eventually by 36.86% with the initial environmental temperature increasing.The prepared TiO2 nanoparticles are mixed crystals of anatase and rutile,their grain size increases at first and then decreases with the increase of initial temperature,and the anatase phase is gradually reduced.The phase-transition temperature from anatase to rutile is 700900 ℃ during high temperature calcination of detonation products,and the grain size is gradually increased with the rise of calcination temperature.

KeyWords AITranslate

TiO2 nanoparticle gaseous detonation crystal structure morphology characteristic detonation pressure

1闫鸿浩,王胜杰,李晓杰,吴林松.初始压力对气相爆轰制备纳米SnO_2的影响[J].功能材料,2013,44(20):3016-3019. 被引量:1

2田诗雅,刘剑,高科.密闭管道瓦斯爆炸冲击波冲量及压力上升速率的实验研究[J].中国安全生产科学技术,2015,11(8):16-21. 被引量:17

3李晓杰,欧阳欣,闫鸿浩,赵铮,姜力.气相爆轰压力及环境温度对制备纳米TiO_2粉末的影响[J].稀有金属材料与工程,2007,36(A03):371-373. 被引量:2

4曲艳东,孔祥清,李晓杰,闫鸿浩.热处理对爆轰合成的纳米TiO_2混晶的结构相变的影响[J].物理学报,2014(3):376-381. 被引量:4

5闫鸿浩,吴林松,李晓杰,王胜杰.颗粒长大模型在气相爆轰合成纳米材料中的应用[J].稀有金属材料与工程,2015,44(5):1144-1148. 被引量:4

6王华,邓军,葛岭梅.初始压力对矿井可燃性气体爆炸特性的影响[J].煤炭学报,2011,36(3):423-428. 被引量:14

7章文姣,曲艳东,孔祥清.爆轰法合成纳米TiO_2及其光催化性能[J].材料科学与工程学报,2016,34(4):540-544. 被引量:4

8文潮,金志浩,关锦清,李迅,周刚,林俊德.炸药爆轰法制备纳米石墨粉[J].稀有金属材料与工程,2004,33(6):628-631. 被引量:18

9李润之,黄子超,司荣军.环境温度对瓦斯爆炸压力及压力上升速率的影响[J].爆炸与冲击,2013,33(4):415-419. 被引量:20

10Ning Luo,Hongwen Jing,Zhanguo Ma,Yingchao Wang,Guilei Sun,Weidong Liu.Growth characteristics of spherical titanium oxide nanoparticles during the rapid gaseous detonation reaction[J].颗粒学报:英文版,2016,14(3):102-107. 被引量:4

1曲艳东,高凌霞,章文姣,刘伟.爆炸合成纳米粉体及其团聚控制研究进展[J].化工进展,2020,39(12):5136-5147. 被引量:1

1刘卫孝,刘洋,高福磊,汪伟,汪营磊.微反应器在含能材料合成与品质提升中的应用[J].化工进展,2023,42(7):3349-3364.

1王前进,叶长青,邵先安,徐长江,黄奕江,马宏昊,郝建,齐晓林.水下爆炸致兔急性肺损伤的实验研究[J].创伤外科杂志,2017,19(11):865-868. 被引量:4

2孔祥清,朱凯泽,高化东,曲艳东.气相爆轰法制备纳米TiO_2-SiO_2复合氧化物及其表征[J].稀有金属与硬质合金,2018,46(1):44-48. 被引量:1

3张阳,安娅,魏声培,田娟,秦好丽.可见光下氮掺杂罗丹明B分子印迹TiO_2的选择性光催化性能[J].化工环保,2017,37(4):454-459. 被引量:3

4张健,毕德贵,张忠孝,岳朴杰.煤粉炉高温还原性氛围下NH_3还原NO_x[J].燃烧科学与技术,2017,23(5):406-411. 被引量:3

5赵焕娟,严屹然,张英华,刘杰.预混气爆轰马赫反射实验研究[J].推进技术,2017,38(11):2572-2579. 被引量:1

6吴苗苗,李洺阳,刘佳昊,刘宇丹,李国华.TiO_2/ACF复合光催化材料研究进展[J].功能材料,2017,48(10):10001-10008. 被引量:7

7毛宇,贺红坡,郭欣,刘泰生.吡咯类氮富氧燃烧的分子动力学研究[J].热能动力工程,2017,32(10):59-65. 被引量:5

8张宇航,邹学军,杨宝灵,董玉瑛,郭宇飞.不同pH值条件合成纳米Bi_2WO_6及其可见光下活性研究[J].水资源与水工程学报,2017,28(5):106-111. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TQ134.11[化学工程—无机化工]

Citation Information:

Using the premixed H2/Air as explosion source,TiO2 nanoparticles were prepared by gaseous detonation in a self-made explosion reaction tube.The variation law was discussed of the detonation pressure in the tube under different initial conditions(initial temperature of 25200℃and H2/Air mixing ratio of 0.20.8).Particle size,composition of crystal phase and morphologies of TiO2 nanoparticles synthesized by detonation at different initial temperature and calcinated at high temperature were characterized by means of XRD and TEM.The results show that the end of the explosion reaction tube has the largest detonation pressure when the premixed H2/Air with the chemical equivalent ratio is employed as explosion source.The detonation pressure at the tube end is increased eventually increased by 39.03% with the increase of H2/Air mixing ratio,and the increasing rate firstly increases and then decreases.However,the detonation pressure at the tube end is reduced eventually by 36.86% with the initial environmental temperature increasing.The prepared TiO2 nanoparticles are mixed crystals of anatase and rutile,their grain size increases at first and then decreases with the increase of initial temperature,and the anatase phase is gradually reduced.The phase-transition temperature from anatase to rutile is 700900 ℃ during high temperature calcination of detonation products,and the grain size is gradually increased with the rise of calcination temperature.

quote

GB/T 7714-2015 [1] QU Yan-dong, SUN Cong-huang, ZHU Kai-ze, et al. Experimental Study on TiO_2 Nanoparticles Prepared by Gaseous Detonation[J]. Rare Metals and Cemented Carbides, 2017(6): 48-53.
MLA [1] QU Yan-dong, et al., "Experimental Study on TiO_2 Nanoparticles Prepared by Gaseous Detonation." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 48-53.
APA [1] QU Yan-dong, SUN Cong-huang, ZHU Kai-ze, KONG Xiang-qing, & ZHANG Wen-jiao. (2017). Experimental Study on TiO_2 Nanoparticles Prepared by Gaseous Detonation. Rare Metals and Cemented Carbides(6), 48-53.
IEEE [1] QU Yan-dong, SUN Cong-huang, ZHU Kai-ze, KONG Xiang-qing, and ZHANG Wen-jiao, "Experimental Study on TiO_2 Nanoparticles Prepared by Gaseous Detonation," Rare Metals and Cemented Carbides, no. 6, pp. 48-53, 2017. keywords: {TiO2 nanoparticle;gaseous detonation;crystal structure;morphology characteristic;detonation pressure}