Study on Composition and Texture of Ni4WV Alloy Substrate Tape for Coated Conductor AITranslate
Abstract AITranslate
Ni4WxV(x=2,4,6)alloys were produced by vacuum induction melting,and 200μm thick alloy substrate tapes were fabricated by rolling assisted biaxial texture substrate tape technology.The magnetic properties and yield strength of the alloy substrate tapes were measured.By using X-ray diffraction(XRD)and electron backscattering diffraction(EBSD),the cold rolling texture and recrystallization texture of the alloy substrate tapes with different composition were analyzed and compared with those of Ni5 Wsubstrate tape,to select the composition with better comprehensive performance.The results show that Ni4W2V alloy substrate tape has the best comprehensive performance with yield strength of 150.7 MPa,which is equivalent to Ni5 Walloy substrate tape.Ni4W2V alloy substrate tape has 55%saturation magnetization of Ni5 Wat room temperature,and its cube texture content is 56%(〈30°).Therefore,Ni4W2V is a promising alloy composition.
KeyWords AITranslate
1古宏伟,杨坚,刘慧舟,屈飞,张华.YBa_2Cu_3O_(7-x)涂层导体的研究进展[J].中国稀土学报,2006,24(3):257-268. 被引量:42
2梁雅儒,田辉,索红莉,马麟,王金华,孟易辰,王盼,彭发学.涂层导体用Ni9W合金基带再结晶及强立方织构的形成研究[J].稀有金属材料与工程,2015,44(10):2491-2495. 被引量:1
3唐先莉,马勇虎.YBCO-NiW超导电缆中导体层的交流损耗测量研究[J].低温与超导,2016,44(9):43-46. 被引量:1
1马麟,索红莉,喻丹,刘婧,彭发学,梁雅儒,王盼,田辉.W含量对Ni-W合金基带取向及织构形成的影响[J].稀有金属材料与工程,2017,46(11):3332-3337.
2王玥瑶,李杰,冯运莉,万德成.热轧工艺对含铌取向硅钢一次冷轧织构的影响[J].金属热处理,2017,42(11):39-44. 被引量:3
3杨文姣,刘坤,马光同.基于磁场强度的高温超导磁悬浮轴承数值仿真方法[J].低温物理学报,2017,0(5):26-32. 被引量:6
4丁宝国.新时期移动4G通信应用现状及关键技术研究[J].科技经济导刊,2017(20):33-33.
5陈艳霞,杨延清.Al-Zn-Mg-Cu合金铣削表面变形层的微观组织和织构[J].航空材料学报,2017,37(6):95-101.
6熊邦汇,王均安,陈永充,刘成红,黄宏川,贺英.Ni-32.7at%Cu合金的调幅分解及其对再结晶织构的影响[J].金属热处理,2018,43(1):46-52. 被引量:1
7林男,刘施峰,范海洋,邓超.单向轧制与交叉轧制高纯铜锰合金再结晶微观组织及织构演变[J].电子显微学报,2017,36(6):564-570. 被引量:2
8潘炳燕.探索打好提升城市生活垃圾分类经济效益组合拳[J].现代经济信息,2017,0(13):38-39. 被引量:1
9哈提热.艾合买提江.《女职工劳动保护特别规定》贯彻落实情况调查报告(二)——原因分析及对策建议[J].兵团工运,2018,0(1):22-24.
10和正华,沙玉辉,张芳,左良.轧制Fe_(81)Ga_(19)合金薄带再结晶织构演变[J].东北大学学报:自然科学版,2017,38(12):1707-1711. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]
Citation Information:
Ni4WxV(x=2,4,6)alloys were produced by vacuum induction melting,and 200μm thick alloy substrate tapes were fabricated by rolling assisted biaxial texture substrate tape technology.The magnetic properties and yield strength of the alloy substrate tapes were measured.By using X-ray diffraction(XRD)and electron backscattering diffraction(EBSD),the cold rolling texture and recrystallization texture of the alloy substrate tapes with different composition were analyzed and compared with those of Ni5 Wsubstrate tape,to select the composition with better comprehensive performance.The results show that Ni4W2V alloy substrate tape has the best comprehensive performance with yield strength of 150.7 MPa,which is equivalent to Ni5 Walloy substrate tape.Ni4W2V alloy substrate tape has 55%saturation magnetization of Ni5 Wat room temperature,and its cube texture content is 56%(〈30°).Therefore,Ni4W2V is a promising alloy composition.
quote
| GB/T 7714-2015 | [1] SONG Yu, WANG Yi-nong. Study on Composition and Texture of Ni4WV Alloy Substrate Tape for Coated Conductor[J]. Rare Metals and Cemented Carbides, 2017(6): 31-34. |
| MLA | [1] SONG Yu, and WANG Yi-nong. "Study on Composition and Texture of Ni4WV Alloy Substrate Tape for Coated Conductor." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 31-34. |
| APA | [1] SONG Yu, & WANG Yi-nong. (2017). Study on Composition and Texture of Ni4WV Alloy Substrate Tape for Coated Conductor. Rare Metals and Cemented Carbides(6), 31-34. |
| IEEE | [1] SONG Yu and WANG Yi-nong, "Study on Composition and Texture of Ni4WV Alloy Substrate Tape for Coated Conductor," Rare Metals and Cemented Carbides, no. 6, pp. 31-34, 2017. keywords: {Ni4WV alloy substrate tape;coated conductor;Ni5W alloy substrate tape;cube texture;magnetic property;yield strength} |