Discussion on Electrolytic Technology of Mirror White Molybdenum Wire AITranslate
Abstract AITranslate
The process technology was studied of mirror white molybdenum wire preparation by electrolytic polishing.Electrolytic method,electrolytic parameter,electrolytic medium,electrode material,and high temperature annealing were experimentally studied.The results show that mirror white molybdenum wire with surface roughness(Ra)of 0.2 can be produced by direct current electrolysis with direct contact between molybdenum wire and anode and using sulfuric acid electrolyte as the medium.Surface passivation and polishing of white molybdenum wire by high temperature annealing can not only improve surface oxidation resistance of white molybdenum wire,but also adjust its physical performance indexes.
KeyWords AITranslate
1朱然,张永康,孙桂芳,沈旭婷,李普.多点激光冲击强化表面粗糙度的有限元分析(英文)[J].稀有金属材料与工程,2018,47(1):33-38. 被引量:3
2谢学林,傅骏,王泽忠,雷德江,雍歧龙.GCr15SiMn钢LF精炼渣系脱硫研究[J].铸造技术,2018,39(1):154-156. 被引量:1
3郝燕霞,钱猛,徐吉健,毕辉,黄富强.棉花基多孔碳材料的合成、微结构及超电性能研究(英文)[J].无机材料学报,2018,33(1):93-99. 被引量:2
4李志刚,刘曾亮,吕纪文,段维常,高浩.铁路用耐油性道岔橡胶垫板的研制[J].绿色科技,2017,0(24):128-129. 被引量:2
5刘惠婧,惠飞.无机隔离分仓聚苯乙烯颗粒保温板物理性能研究[J].河南建材,2018(1):69-70. 被引量:3
6薛乐星,冯博,赵娟,封雪松,冯晓军.炸药在等离子体起爆下的能量输出特性[J].火炸药学报,2017,40(6):83-86. 被引量:1
7伍书军,夏昌勇,杨红,冷永波.耐火泥浆加热永久线变化率试验方法的探讨[J].耐火材料,2017,51(6):465-467. 被引量:1
8闵凡奇,周敦凡,党国举,张道明,张全生,解晶莹.氧阴极在阳离子膜电解硫酸钠中的应用研究[J].无机盐工业,2018,50(3):38-42.
9孙海波,王双成,吕冬生,唐一林.生物质石墨烯定岛型海岛纤维生产工艺分析[J].国际纺织导报,2017,45(10):28-30. 被引量:4
10张谦,孙怡.镁橄榄石熔盐电脱氧制备锂离子电池负极材料[J].广东化工,2018,45(3):4-5.
Basic Information:
DOI:
Chinese Library Classification Number:TG175[金属学及工艺—金属表面处理]
Citation Information:
The process technology was studied of mirror white molybdenum wire preparation by electrolytic polishing.Electrolytic method,electrolytic parameter,electrolytic medium,electrode material,and high temperature annealing were experimentally studied.The results show that mirror white molybdenum wire with surface roughness(Ra)of 0.2 can be produced by direct current electrolysis with direct contact between molybdenum wire and anode and using sulfuric acid electrolyte as the medium.Surface passivation and polishing of white molybdenum wire by high temperature annealing can not only improve surface oxidation resistance of white molybdenum wire,but also adjust its physical performance indexes.
quote
| GB/T 7714-2015 | [1] JIANG Zi-guang. Discussion on Electrolytic Technology of Mirror White Molybdenum Wire[J]. Rare Metals and Cemented Carbides, 2017(6): 35-37. |
| MLA | [1] JIANG Zi-guang. "Discussion on Electrolytic Technology of Mirror White Molybdenum Wire." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 35-37. |
| APA | [1] JIANG Zi-guang. (2017). Discussion on Electrolytic Technology of Mirror White Molybdenum Wire. Rare Metals and Cemented Carbides(6), 35-37. |