A Mass Transfer Model for the Extraction of Rare Earth Using Emulsion Liquid Membrane(Ⅱ) AITranslate
Abstract AITranslate
Some experiments were carried out to demonstrate the mass transfer model of extraction of rare earth by emulsion liquid membrane. It was shown the present model proposed in Part(Ⅰ) was not only in good agreement with the experiments, but also mathematically simple.
KeyWords AITranslate
1刘兴荣,张秀娟.乳状液膜提取稀土的传质模型研究(Ⅱ)[J].稀有金属与硬质合金,1993,21(4):7-11. 被引量:4
2高广达,王洪元,郑晓东.液膜脱酚的综合传质模型[J].化工学报,1991,42(3):356-361. 被引量:3
1刘兴荣,张秀娟.乳状液膜提取稀土的传质模型研究(Ⅱ)[J].稀有金属与硬质合金,1993,21(4):7-11. 被引量:4
2刘兴荣,张秀娟.络合交换乳状液膜分离稀土镝和铥[J].稀土,1996,17(2):9-13. 被引量:1
3刘兴荣,张秀娟.乳状液膜提取稀土的传质模型研究(Ⅲ)[J].膜科学与技术,1996,16(2):51-57. 被引量:3
4龚福忠,李成海,马培华,唐艳霞,刘经伟.微乳液膜法萃取钕[J].化工学报,2003,54(11):1569-1574. 被引量:21
1刘占宇,夏传波,杨延钊,辛雪梅.微乳液萃取钴的研究[J].山东化工,2007,36(1):1-3. 被引量:4
2刘兴荣,张秀娟.乳状液膜提取稀土的传质模型研究(Ⅱ)[J].稀有金属与硬质合金,1993,21(4):7-11. 被引量:4
3龚福忠,刘力恒,马培华.反胶束、W/O微乳液的特性及其萃取机理[J].广西大学学报:自然科学版,2005,30(2):119-122. 被引量:3
4刘兴荣,张秀娟.络合交换乳状液膜分离稀土镝和铥[J].稀土,1996,17(2):9-13. 被引量:1
5刘兴荣,张秀娟.乳状液膜提取稀土的传质模型研究(Ⅲ)[J].膜科学与技术,1996,16(2):51-57. 被引量:3
6孙玉柱.乳状液膜分离技术的研究进展[J].湿法冶金,2006,25(1):10-17. 被引量:17
7龚福忠,马培华,罗艳,刘力恒,张丽梅.微乳液的增溶、相态及微乳液/中空纤维膜萃取钕[J].化工学报,2006,57(3):590-595. 被引量:8
8周文杰.适用于痕量锌离子迁移的微乳液的制备及迁移条件[J].安徽化工,2006,32(3):23-26. 被引量:1
9龚福忠,马培华,刘力恒,唐艳霞,黄小凤.微乳液体系(OP-4+OP-7)/苯甲醇/D_2EHPA/环己烷/HCl水溶液活性组分的界面性质[J].膜科学与技术,2006,26(5):60-65.
10周富荣,杜金萍.微乳液在萃取分离中的研究进展[J].现代化工,2006,26(12):17-20. 被引量:8
1张瑞华,全水清.乳状液膜提取钯的研究[J].稀有金属,1994,18(1):14-17. 被引量:2
2张瑞华.对我国液膜提取稀土研究的几点看法[J].稀有金属,1992,16(2):140-142. 被引量:1
3张瑞华.关于我国液膜提取稀土研究的几点看法[J].江西有色金属,1989,3(3):11-14.
4蔡清海,严忠,曹汉谨.乳状液液膜法提取金的动力学[J].膜科学与技术,1992,12(1):20-25. 被引量:2
5秦庆伟,赵恒勤,赖延清,李劼,刘业翔,邓佐国.Cyanex272作载体的乳状液膜提取稀土的研究[J].矿冶工程,2002,22(3):74-78. 被引量:11
6张鹏飞.乳状液膜提金技术的研究现状[J].湖南有色金属,1996,12(3):40-44.
7张瑞华.液膜提取金的工艺研究状况[J].黄金,1990,11(7):22-27. 被引量:4
8徐铜文.液膜法和溶剂萃取法处理含铜料液的初步研究[J].安徽化工,1992(2):6-10.
9王靖芳,冯彦琳,窦丽珠,石菊香.N503为载体的乳状液膜提取钯(Ⅱ)的研究[J].稀有金属,2001,25(1):68-70. 被引量:7
10张瑞华.用液膜法从稀土浸出液中分离非稀土杂质[J].江西有色金属,2000,14(3):23-26. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF845.01[冶金工程—有色金属冶金]
Citation Information:
Some experiments were carried out to demonstrate the mass transfer model of extraction of rare earth by emulsion liquid membrane. It was shown the present model proposed in Part(Ⅰ) was not only in good agreement with the experiments, but also mathematically simple.
quote
| GB/T 7714-2015 | [1] LIU Xing-rong, ZHANG Xiu-juan. A Mass Transfer Model for the Extraction of Rare Earth Using Emulsion Liquid Membrane(Ⅱ)[J]. Rare Metals and Cemented Carbides, 1993(4): 7-11. |
| MLA | [1] LIU Xing-rong, and ZHANG Xiu-juan. "A Mass Transfer Model for the Extraction of Rare Earth Using Emulsion Liquid Membrane(Ⅱ)." Rare Metals and Cemented Carbides, no. 4, 1993, pp. 7-11. |
| APA | [1] LIU Xing-rong, & ZHANG Xiu-juan. (1993). A Mass Transfer Model for the Extraction of Rare Earth Using Emulsion Liquid Membrane(Ⅱ). Rare Metals and Cemented Carbides(4), 7-11. |
| IEEE | [1] LIU Xing-rong and ZHANG Xiu-juan, "A Mass Transfer Model for the Extraction of Rare Earth Using Emulsion Liquid Membrane(Ⅱ)," Rare Metals and Cemented Carbides, no. 4, pp. 7-11, 1993. keywords: {emulsion liquid membrane;rare earth;mass transfer model} |