Study on Thermodynamics and Kinetics for Extraction of Erbium with Di(2-ethylhexyl) phosphoric Acid AITranslate

Institute of Environmental Science, South China University of Technology;Institute of Environmental Science, South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Studies of extraction equilibrium of erbium by di(2-ethylhexyl) phosphoric acid (D2EHPA)in sulphonated kerosene were made.The equation, for the extraction equilibrium and the [equilibrium constant were obtained.The extraction and stripping rates were measured using a constant interfacial area cell. The effects of the concentrations of Er3+ , H+. D2EHPA and the complex on the reaction rates were investigated and the rate expression of this reaction was obtained. The interfacial reaction model was proposed, which was identified by kinetic study and the measurement of interfacial tension

KeyWords AITranslate

di (2-ethylhexyl) phosphoric acid erbium extraction equilib- rium extraction rate stripping rate interfacial reaction model

1王向德,陈新棉,万印华,冯肇霖,张秀娟.液膜法自低品位稀土矿生产氯化稀土和富铕、富钇氯化物中间试验[J].稀土,1992,13(2):30-35. 被引量:23

1高照国,曹耀华,刘红召.含铟铅烟尘提铟试验研究[J].稀有金属,2010,34(3):413-419. 被引量:6

2郑雅杰,陈昆昆,孙召明.SO_2还原沉金后液回收硒碲及捕集铂钯[J].中国有色金属学报,2011,21(9):2258-2264. 被引量:35

3殷秀梅,汪红,邢明铭,付姚,田莹,沈显良,于伟光,罗昔贤.Upconversion luminescence of Y2Ti2O7:Er3+ under 1550 and 980 nm excitation[J].稀土学报:英文版,2017,35(3):230-234.

4陈兰,李成威,谷晴晴,王飞飞,陈雪婷.阴极旋转电解法制备纳米铜粉的实验研究[J].粉末冶金工业,2013,23(3):21-25. 被引量:4

5张魁芳,刘志强,曹洪杨,朱薇,高远,金明亚.不同磷酸酯萃取剂从硫酸体系萃镓性能研究[J].有色金属:冶炼部分,2017,0(4):35-38. 被引量:5

6王劲松,阳静.牛顿迭代法在求解物料平衡式中的应用[J].自动化与仪器仪表,2014(7):124-126.

7一种平衡式高炉炉顶溜槽布料器[J].冶金设备,2006(2):57-57.

8刘智安,张知见,刘启旺.液相生化法烟气脱硫机理及动力学[J].应用基础与工程科学学报,2011,19(4):644-652. 被引量:2

9厉学武,唐军利,唐丽霞,崔玉青,王磊.氢离子对合成十二钼酸铵的影响[J].中国钼业,2010,34(5):32-34. 被引量:4

10胡晓辉.金属镁还原炉热能平衡方法及节能途径[J].节能,1997(1):24-26. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF845.301[冶金工程—有色金属冶金]

Citation Information:

Studies of extraction equilibrium of erbium by di(2-ethylhexyl) phosphoric acid (D2EHPA)in sulphonated kerosene were made.The equation, for the extraction equilibrium and the [equilibrium constant were obtained.The extraction and stripping rates were measured using a constant interfacial area cell. The effects of the concentrations of Er3+ , H+. D2EHPA and the complex on the reaction rates were investigated and the rate expression of this reaction was obtained. The interfacial reaction model was proposed, which was identified by kinetic study and the measurement of interfacial tension

quote

GB/T 7714-2015 [1] PAN Yong-zhang, ZHANG Xiu-juan. Study on Thermodynamics and Kinetics for Extraction of Erbium with Di(2-ethylhexyl) phosphoric Acid[J]. Rare Metals and Cemented Carbides, 1993(4): 11-17.
MLA [1] PAN Yong-zhang, and ZHANG Xiu-juan. "Study on Thermodynamics and Kinetics for Extraction of Erbium with Di(2-ethylhexyl) phosphoric Acid." Rare Metals and Cemented Carbides, no. 4, 1993, pp. 11-17.
APA [1] PAN Yong-zhang, & ZHANG Xiu-juan. (1993). Study on Thermodynamics and Kinetics for Extraction of Erbium with Di(2-ethylhexyl) phosphoric Acid. Rare Metals and Cemented Carbides(4), 11-17.
IEEE [1] PAN Yong-zhang and ZHANG Xiu-juan, "Study on Thermodynamics and Kinetics for Extraction of Erbium with Di(2-ethylhexyl) phosphoric Acid," Rare Metals and Cemented Carbides, no. 4, pp. 11-17, 1993. keywords: {di (2-ethylhexyl) phosphoric acid erbium, extraction equilib- rium, extraction rate, stripping rate, interfacial reaction model}