High-Efficiency Photodetector Based on a CVD-Grown WS2 Monolayer High-Efficiency Photodetector Based on a CVD-Grown WS2 Monolayer AITranslate
Abstract AITranslate
Future generation technologies demand high efficiency photodetectors to enable sensing and switching devices for ultrafast communication and machine vision. This requires direct-band gap materials with high photosensitivity, high detectivity, and high quantum efficiency. Monolayered two-dimensional-semiconductor-based photodetectors are the most promising materials for such applications, although experimental realization has been limited due to the unavailability of a high-quality sample. In the current paper, we report about a WS2-based photodetector having a sensitivity of 290 A W–1 upon 405 nm excitation and an incident power density as low as 0.06 mW/cm2. The fabricated device shows a detectivity of 52 × 1014 with an external quantum efficiency of 89 × 103 %. The observed superior photoresponse parameters of the CVD-grown WS2-based photodetector as compared to Si-detectors establish its capability to replace the Si-photodetectors with monolayered ultrathin device having superior performance parameters.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00366
Chinese Library Classification Number:
Citation Information:
Future generation technologies demand high efficiency photodetectors to enable sensing and switching devices for ultrafast communication and machine vision. This requires direct-band gap materials with high photosensitivity, high detectivity, and high quantum efficiency. Monolayered two-dimensional-semiconductor-based photodetectors are the most promising materials for such applications, although experimental realization has been limited due to the unavailability of a high-quality sample. In the current paper, we report about a WS2-based photodetector having a sensitivity of 290 A W–1 upon 405 nm excitation and an incident power density as low as 0.06 mW/cm2. The fabricated device shows a detectivity of 52 × 1014 with an external quantum efficiency of 89 × 103 %. The observed superior photoresponse parameters of the CVD-grown WS2-based photodetector as compared to Si-detectors establish its capability to replace the Si-photodetectors with monolayered ultrathin device having superior performance parameters.
quote
| GB/T 7714-2015 | [1] Rakesh K. Prasad, Koushik Ghosh, Pravat K. Giri, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00366. |
| MLA | [1] Rakesh K. Prasad, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00366. |
| APA | [1] Rakesh K. Prasad, Koushik Ghosh, Pravat K. Giri, DaiSik Kim, & Dilip K. Singh. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00366 |
| IEEE | [1] Rakesh K. Prasad, Koushik Ghosh, Pravat K. Giri, DaiSik Kim, and Dilip K. Singh, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00366. keywords: {monolayer tungsten disulfide 2dimensional growth CVD high photosensitivity photodetectors} |