Dispersionprestrengthened Ni Powder as Substitution of Cofor Hard Metal Binder AITranslate
Abstract AITranslate
The possibility of the substitution of Co as binder in the cemented carbide with dispersionprestrengthened Ni powder has been investigated. The quality of the WCNi cemented carbide can be improved with predispersion of nanosized Al2O3 powder into Ni. The mechanical properties of WC8%Ni(Al2O3) alloy, prepared by this method is comparable with WC8% Co cemented carbide.
KeyWords AITranslate
1柳春林.WC-Ni硬质合金研究[J].硬质合金,1997,14(4):211-213. 被引量:6
2汪仕元,潘启芳,雍志华,张伟,张习武,朱俊峰.稀土元素对WC-Ni硬质合金性能的影响[J].粉末冶金技术,1996,14(4):291-296. 被引量:8
3李维.纳米化硬质合金粘结剂的研究,中南工业大学博士论文[M].,1997,11..
1沈军,张法明,孙剑飞.Fabrication and mechanical properties of WC-Co-Al_2O_3 nanocomposites by spark plasma sintering[J].中国有色金属学会会刊:英文版,2005,15(2):233-237.
2郭智兴,熊计.WC-Ni硬质合金的研究与应用[J].工具技术,2005,39(8):15-19. 被引量:16
3李铁晶,张传福,湛菁,邬建辉.配位沉淀-直接还原法制备球形超细镍粉[J].矿冶工程,2006,26(6):68-72. 被引量:2
4李启厚,张程,王红军,刘志宏,刘智勇.超细镍粉的制备、应用现状及发展趋势[J].湿法冶金,2009,28(4):193-197. 被引量:4
5梁文军,张宏,沈承金,马瑞勇.粘结剂对超音速火焰喷涂碳化钨涂层磨粒磨损性能的影响[J].电镀与涂饰,2012,31(2):67-71. 被引量:3
6陈贵芳,盛勇.机械球磨法制备片状微米级镍粉的研究[J].热加工工艺,2014,43(10):51-53.
7郑德庆,梁武,谭共志.基于浏览器/服务器结构的网络无纸化考试和管理系统[J].电子质量,2002(6):114-117.
8牛明勤,吴介达.超细镍粉的制备进展[J].精细化工,2003,20(12):715-717. 被引量:19
1宋金鹏,肖利民,吕明,高姣姣.烧结温度对短切碳纤维增强WC-TaC-Csf刀具材料组织及性能的影响[J].热加工工艺,2019,0(24):75-77.
2李杏英,刘志强,林衍洲.制备超细镍粉的研究进展[J].广东有色金属学报,2005,15(1):19-21. 被引量:9
3伍贺东,陈为亮,孟德龙,张凌义,戴永年.超细镍粉制备技术研究进展[J].湖南有色金属,2006,22(6):35-39. 被引量:2
4伍贺东,陈为亮,孟德龙,张凌义,戴永年.超细镍粉制备技术研究进展[J].冶金丛刊,2007(1):37-41. 被引量:7
5伍贺东,陈为亮,孟德龙,张凌义,戴永年.超细镍粉制备技术研究进展[J].湿法冶金,2007,26(2):57-61. 被引量:4
6徐燕军,柳成渊,陈哲,刘一波,尹翔,赵万林.粉末触媒合成柱真空烧结工艺的研究[J].金刚石与磨料磨具工程,2008,28(4):18-21. 被引量:2
7黄国勇,徐盛明,徐刚,李林艳,陈崧哲.导电浆料用镍粉的制备方法及发展趋势[J].稀有金属,2007,31(S2):66-71. 被引量:5
8徐涛.硬质合金发展与钴粉市场变化[J].硬质合金,2009,26(2):116-121. 被引量:9
9邱志刚,俞宏英,孙冬柏,李怀娜,王旭东,樊自拴,孟惠民.一维结构镍纳米粉的制备研究[J].中国科技论文在线,2007,2(5):336-340. 被引量:1
10万祥明,刘建雄,吴正宇,詹肇麟.影响硬质合金与钢基体高频感应钎焊质量的主要因素及改善措施[J].热加工工艺,2010,39(23):183-186. 被引量:4
1陈德勇,罗在清.WC-Ni硬质合金的特性、发展及其应用[J].硬质合金,2007,24(1):43-46. 被引量:23
2柳春林.WC-Ni硬质合金研究[J].硬质合金,1997,14(4):211-213. 被引量:6
3柳春林.WC-Ni硬质合金研究[J].四川有色金属,1997(1):18-20. 被引量:5
4熊继,沈保罗.混合稀土CeLa对WC-Ni硬质合金性能和显微结构的影响[J].工具技术,2003,37(6):18-20. 被引量:5
5胡海波.添加剂对WC-Ni硬质合金组织结构与力学性能的影响[J].稀有金属与硬质合金,2013,41(1):55-59. 被引量:4
6BernhardWittmann,邱智海,佘建芳.以镍和铁为粘结相的硬质合金中WC晶粒长大及其抑制[J].国外难熔金属与硬质材料,2004,20(1):6-15.
7刘寿荣.WC-Ni硬质合金游离碳的无损测定原理[J].硬质合金,2001,18(1):33-34. 被引量:2
8邱成滨,彭英彪,何旭文,杜勇,张忠健,徐涛,刘向中,王辉平,王社权.晶粒生长抑制剂在WC-Ni硬质合金粘结相中固溶度的实验研究[J].硬质合金,2016,33(2):89-95. 被引量:6
9董凯林,曹万里,时凯华,江庆,高建.碳含量对WC-9Ni-1Cr细晶硬质合金组织结构及性能的影响[J].粉末冶金材料科学与工程,2015,20(3):449-455. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF125.5[冶金工程—粉末冶金];TF125.3[冶金工程—粉末冶金]
Citation Information:
The possibility of the substitution of Co as binder in the cemented carbide with dispersionprestrengthened Ni powder has been investigated. The quality of the WCNi cemented carbide can be improved with predispersion of nanosized Al2O3 powder into Ni. The mechanical properties of WC8%Ni(Al2O3) alloy, prepared by this method is comparable with WC8% Co cemented carbide.
quote
| GB/T 7714-2015 | [1] HUANG Jia-ming, LI Wei, HUANG Jing-song, et al. Dispersionprestrengthened Ni Powder as Substitution of Cofor Hard Metal Binder[J]. Rare Metals and Cemented Carbides, 1999(2): 1-3. |
| MLA | [1] HUANG Jia-ming, et al., "Dispersionprestrengthened Ni Powder as Substitution of Cofor Hard Metal Binder." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 1-3. |
| APA | [1] HUANG Jia-ming, LI Wei, HUANG Jing-song, & ZHOU Luo-san. (1999). Dispersionprestrengthened Ni Powder as Substitution of Cofor Hard Metal Binder. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] HUANG Jia-ming, LI Wei, HUANG Jing-song, and ZHOU Luo-san, "Dispersionprestrengthened Ni Powder as Substitution of Cofor Hard Metal Binder," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 1999. keywords: {Ni binder;Co binder;cemented carbide;dispersion strengthenning;nanosized Al2O3 particle} |