Influences of Dy_2O_3 Addition on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnets AITranslate

Taiyuan University of Technology Surface Engineering Research Institute;Taiyuan University of Technology Surface Engineering Research Institute;Taiyuan University of Technology Surface Engineering Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Analysis is made of the influences of addition of different mass fraction of Dy2 Oa powders during milling on density, microstructure, orientation degree and magnetic properties of the sintered Nd-Fe-B mag-net (PrNd) 32. 5 Febal Nb0.65 Cu0.20 Al0.65 B1.15. The results show that with the increase of Dy2 O3 the average grain size of the magnet decreases at first and then rapidly increases, its dens mass fraction, ity slightly clines,and orientation degree gradually rises. Both Br and (BH)max decrease linearly with the increase Dy2O3 dosage while Hcj increases and then decreases. During liquid p sulting from Dy diffusion into the ence microstructure and magnetic linearly, and the squareness of d hase sintering process of the mag primary phase grains and Nd2 O3 properties of the magnet. Adding de-of emagnetization curve increases at first net,both (Nd,Dy)2Fe14 B formation re-formation in grain boundary can influ- appropriate Dy2 O3 is beneficial for im- provement of microstructure, orientation degree and magnetic properties of th fraction of Dy2O3 is 0.8%, the grain size of the magnet reaches the minimum of tion,the surface morphology is regular, and the squareness of demagnetization e magnet the most curve is also When the mass uniform distribu-lso the highest.

KeyWords AITranslate

sintered Nd-Fe-B magnet Dy2 O3 addition microstructure density orientation degree magneticproperty

1王占勇.添加Dy_2O_3对烧结NdFeB磁体微观结构的影响[J].热加工工艺,2007,36(6):10-11. 被引量:3

2Sepehri-Amin H,Li W F,Ohkubo T,et al. Effect of Ga addition on the microstructure and magnetic properties of HDDR processed Nd-Fe-B powder[J]. Acta Materia- lia,2010,58:1 309-1 316.

3孙绪新,包小倩,高学绪,张茂才,董清飞,周寿增.烧结Nd-Fe-B磁体表面渗镀Dy2O3对磁体显微组织和磁性能的影响[J].中国稀土学报,2009(1):86-91. 被引量:13

4Park H D,Baik W H,Yoon D Y,etal. The effect of Mo addition on the liquid-phase sintering of W heavy alloy [J]. Metallurgical and Materials Transactions A, 1996, 27:3 120-3 125.

5刘湘涟,周寿增.Nd-Fe-B磁体烧结过程晶粒长大行为的研究[J].中国稀土学报,2006,24(5):580-585. 被引量:12

6周寿增,董清飞.超强永磁体-稀土铁系永磁材料[M].北京:冶金工业出版社,2010.308.

7何叶青,王震西,周寿增,张臻蓉,韩宝善.液相烧结对Nd-Fe-B粉末压坯及磁体取向度的影响[J].中国稀土学报,2003,21(4):367-370. 被引量:3

8Chang W C,Wu T B,Liu K S. A texture study of aniso tropic sintered Nd-Fe-B magnets[J]. J Appl Phys, 1988,63(8) :3 531-3 533.

9周寿增,张瑾,马德青,高茂林.添加Dy和Dy_2O_3的烧结NdFeB系永磁体的显微结构与磁硬化[J].金属学报,1992,28(3). 被引量:8

10王占勇,谷南驹,王宝奇,刘金芳,赵金伶,张志清,张巧格.影响烧结Nd-Fe-B磁体退磁曲线方形度的因素[J].磁性材料及器件,2003,34(1):7-11. 被引量:8

1管立斌.Y代替PrNd制作烧结钕铁硼磁体研究[J].电子材料与电子技术,2012,39(2):25-27.

2刘湘涟,阳娣莎,孙允成,苏晋学,周寿增.Nd-Fe-B磁体退磁曲线方形度与烧结过程的关系[J].磁性材料及器件,2007,38(1):46-50. 被引量:3

3万永.烧结Nd—Fe-B永磁体J-H退磁曲线方形度浅析[J].金属材料研究,2009,35(2):18-23. 被引量:1

4唐国团,陈福峰,郭林,赵家成,王会杰.稀土及氧含量对烧结Nd-Fe-B磁体退磁曲线方形度的影响[J].磁性材料及器件,2014,45(3):36-38. 被引量:6

5彭龙,徐光亮,张明,王敬东,付玉群,刘莉.烧结温度对稀土永磁Sm(Co_(0.72)Fe_(0.15)Cu_(0.1)Zr_(0.03))_(7.5)的磁性能的影响[J].功能材料与器件学报,2006,12(5):409-412.

6张琪,刘心宇,吴轶.Sr(Cu_(0.5)W_(0.5))O_3掺杂Ba_(0.85)Ca_(0.15)Zr_(0.1)Ti_(0.9)O_3压电陶瓷性能研究[J].电子元件与材料,2014,33(6):6-8.

7顾正飞,张伟华,余宁森,雷友德,周怀营,庄应烘.Sm对Sm(Co,Cu,Fe,Zr)z永磁合金性能和退磁曲线方形度的影响[J].材料科学与工艺,1995,3(2):9-13. 被引量:7

8管立斌.Gd代替PrNd制作烧结钕铁硼磁体生产研究[J].电子材料与电子技术,2011(2):22-25.

9左林,李元勋,李强,郁国良,张怀武.片式电感用NiCuZn铁氧体材料制备性能研究[J].实验科学与技术,2014,12(2):221-223. 被引量:1

10刘国征,邹敏.Mo的添加对(PrNd)FeCoAlB磁体性能和热稳定性的影响[J].电工合金文集,1990(1):14-16.

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

Analysis is made of the influences of addition of different mass fraction of Dy2 Oa powders during milling on density, microstructure, orientation degree and magnetic properties of the sintered Nd-Fe-B mag-net (PrNd) 32. 5 Febal Nb0.65 Cu0.20 Al0.65 B1.15. The results show that with the increase of Dy2 O3 the average grain size of the magnet decreases at first and then rapidly increases, its dens mass fraction, ity slightly clines,and orientation degree gradually rises. Both Br and (BH)max decrease linearly with the increase Dy2O3 dosage while Hcj increases and then decreases. During liquid p sulting from Dy diffusion into the ence microstructure and magnetic linearly, and the squareness of d hase sintering process of the mag primary phase grains and Nd2 O3 properties of the magnet. Adding de-of emagnetization curve increases at first net,both (Nd,Dy)2Fe14 B formation re-formation in grain boundary can influ- appropriate Dy2 O3 is beneficial for im- provement of microstructure, orientation degree and magnetic properties of th fraction of Dy2O3 is 0.8%, the grain size of the magnet reaches the minimum of tion,the surface morphology is regular, and the squareness of demagnetization e magnet the most curve is also When the mass uniform distribu-lso the highest.

quote

GB/T 7714-2015 [1] YANG Rui, LIU Xiang-lian, FAN Ai-lan. Influences of Dy_2O_3 Addition on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnets[J]. Rare Metals and Cemented Carbides, 2013(2): 25-29.
MLA [1] YANG Rui, et al., "Influences of Dy_2O_3 Addition on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnets." Rare Metals and Cemented Carbides, no. 2, 2013, pp. 25-29.
APA [1] YANG Rui, LIU Xiang-lian, & FAN Ai-lan. (2013). Influences of Dy_2O_3 Addition on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnets. Rare Metals and Cemented Carbides(2), 25-29.
IEEE [1] YANG Rui, LIU Xiang-lian, and FAN Ai-lan, "Influences of Dy_2O_3 Addition on Microstructure and Magnetic Properties of Sintered Nd-Fe-B Magnets," Rare Metals and Cemented Carbides, no. 2, pp. 25-29, 2013. keywords: {sintered Nd-Fe-B magnet;Dy2 O3 addition;microstructure;density;orientation degree;magneticproperty}