Promoting the Normal- and Low-Temperature Performances of Natural Graphite by the F-Doping Derived from PVDF Modification Promoting the Normal- and Low-Temperature Performances of Natural Graphite by the F-Doping Derived from PVDF Modification AITranslate
Abstract AITranslate
The inferior rate performance, cyclability, and low-temperature performance plague the wide application of natural graphite (NG). In this work, NG was modified with polyvinylidene fluoride (PVDF) by a simple hydrothermal route at 180 °C and subsequent sintering at 300 °C. The two-step treatment not only boosted the graphitization degree of NG but also strengthened the binding of PVDF with NG to yield uniform PVDF coating and F-doping adjacent to the NG surface. The modification contributes to enhancing the structural stability of NG, electron transfer, and Li-ion diffusion, facilitating the formation of a uniform and dense solid electrolyte interface film, reducing impedance, and alleviating polarization, thus endowing the PVDF-modified NG with elevated electrochemical performance, especially the marked enhancement in rate performance, cyclability, and low-temperature performance. This work opens up a simple avenue to promote the performance of NG, and the technique could be scaled up to industrially produce NG with high performance in a wide temperature range.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00939
Chinese Library Classification Number:
Citation Information:
The inferior rate performance, cyclability, and low-temperature performance plague the wide application of natural graphite (NG). In this work, NG was modified with polyvinylidene fluoride (PVDF) by a simple hydrothermal route at 180 °C and subsequent sintering at 300 °C. The two-step treatment not only boosted the graphitization degree of NG but also strengthened the binding of PVDF with NG to yield uniform PVDF coating and F-doping adjacent to the NG surface. The modification contributes to enhancing the structural stability of NG, electron transfer, and Li-ion diffusion, facilitating the formation of a uniform and dense solid electrolyte interface film, reducing impedance, and alleviating polarization, thus endowing the PVDF-modified NG with elevated electrochemical performance, especially the marked enhancement in rate performance, cyclability, and low-temperature performance. This work opens up a simple avenue to promote the performance of NG, and the technique could be scaled up to industrially produce NG with high performance in a wide temperature range.
quote
| GB/T 7714-2015 | [1] ZongXiao Zhao, Xue Bai, HuiLing Zhu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00939. |
| MLA | [1] ZongXiao Zhao, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00939. |
| APA | [1] ZongXiao Zhao, Xue Bai, HuiLing Zhu, Wei Liu, YongXin Qi, Tao Li, & YuJun Bai. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00939 |
| IEEE | [1] ZongXiao Zhao, Xue Bai, HuiLing Zhu, Wei Liu, YongXin Qi, Tao Li, and YuJun Bai, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00939. keywords: {natural graphite polyvinylidene fluoride hydrothermal treatment rate performance low temperature} |