Sequential-Twice-Doping Approach toward Synergistic Optimization of Carrier Concentration and Mobility in Thiophene-Based Polymers Sequential-Twice-Doping Approach toward Synergistic Optimization of Carrier Concentration and Mobility in Thiophene-Based Polymers AITranslate
Abstract AITranslate
The chemical doping of polymer semiconductors represents a powerful strategy for advancing organic electronic applications. However, there remains an issue in that dopants tend to disrupt the molecular packing of conjugated polymers and cause low doping efficiency in a conventional chemical doping process. In this work, we provide a sequential-twice-doping (STD) approach, in which the polymer is doped twice, sequentially by a single-solution doping (predoping) process and an immersion doping (postdoping) process. By employing an STD approach, the destruction of the original polymer packing upon doping can be avoided, and the doping efficiency is simultaneously maximized. As a result, the thiophene-based polymer with a large π-conjugated backbone shows a high electrical conductivity of up to 408 S cm–1 attributed to its high mobility and high carrier concentration. It is proved that the predoping process mainly endows the doping reaction occurring in the amorphous region and ensures moderate crystalline domains for charge transport. Then, the postdoping process significantly improves the doping efficiency as well as the carrier mobility without interference in the film morphology built by the predoping process. The results suggest that the STD approach is an efficient strategy toward optimizing polymer crystallinity and doping efficiency to achieve high electrical conductivity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00940
Chinese Library Classification Number:
Citation Information:
The chemical doping of polymer semiconductors represents a powerful strategy for advancing organic electronic applications. However, there remains an issue in that dopants tend to disrupt the molecular packing of conjugated polymers and cause low doping efficiency in a conventional chemical doping process. In this work, we provide a sequential-twice-doping (STD) approach, in which the polymer is doped twice, sequentially by a single-solution doping (predoping) process and an immersion doping (postdoping) process. By employing an STD approach, the destruction of the original polymer packing upon doping can be avoided, and the doping efficiency is simultaneously maximized. As a result, the thiophene-based polymer with a large π-conjugated backbone shows a high electrical conductivity of up to 408 S cm–1 attributed to its high mobility and high carrier concentration. It is proved that the predoping process mainly endows the doping reaction occurring in the amorphous region and ensures moderate crystalline domains for charge transport. Then, the postdoping process significantly improves the doping efficiency as well as the carrier mobility without interference in the film morphology built by the predoping process. The results suggest that the STD approach is an efficient strategy toward optimizing polymer crystallinity and doping efficiency to achieve high electrical conductivity.
quote
| GB/T 7714-2015 | [1] Haoyu Chai, Zhen Xu, Hui Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00940. |
| MLA | [1] Haoyu Chai, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00940. |
| APA | [1] Haoyu Chai, Zhen Xu, Hui Li, Fei Zhong, Shengqiang Bai, & Lidong Chen. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00940 |
| IEEE | [1] Haoyu Chai, Zhen Xu, Hui Li, Fei Zhong, Shengqiang Bai, and Lidong Chen, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00940. keywords: {conductive polymers chemical doping electrical conductivity sequentialtwicedoping approach carrier mobility} |