Analysis for Key Process Parameters during Isothermal Pressure Torsion of 7A60 Aluminium Alloy Cup AITranslate
Abstract AITranslate
The effects of key parameters on forming performance of 7A60 aluminum alloy cup during isothermal pressure torsion were investigated by technological experiments and finite element simulation. The results show that the effect of height to diameter ratio of the blank on cumulative deformation is mainly in upsetting deformation stage. As lower mould torsion speed increases, the forming load is reduced and the torque increases. When lower mould torsion speed is too large, the damage value of transition fillet area of the torsional disk would be greater than 1, and the edge is easy to fracture. The influence is significant of forming temperature on forming load and torque. The continuity of the alloy cannot be destroyed with a torsional shear deformation of less than one ring during forming process,and its strength is improved corn pared with the alloy obtained by conventional extrusion.
KeyWords AITranslate
1张宝红,张治民,李大旭.温成形杯形件组织性能研究[J].材料科学与工艺,2007,15(1):118-120. 被引量:11
2徐文臣,单德彬,陈宇,康达昌,吕炎.钛合金薄壁筒形件热旋成形技术研究[J].锻压技术,2008,33(3):56-59. 被引量:20
3薛克敏,张君,李萍,黄科帅.高压扭转法的研究现状及展望[J].合肥工业大学学报:自然科学版,2008,31(10):1613-1616. 被引量:30
4李萍,章凯,薛克敏,王晓溪.新型药型罩温压扭成形模拟与实验研究[J].兵工学报,2012,33(4):437-442. 被引量:4
5陈勇军,王渠东,彭建国,翟春泉,丁文江.大塑性变形制备细晶材料的研究、开发与展望[J].材料导报,2005,19(4):77-80. 被引量:33
6上官丰收,谢季佳,洪友士.高压扭转致纯铜晶粒细化及与应变的关系[J].材料研究学报,2007,21(1):72-76. 被引量:16
7王成国,林俐菁,刘红丽,王莉,薛克敏,袁宝国.基于高压扭转法制备SiCp/Al基复合材料[J].精密成形工程,2012,4(6):82-84. 被引量:5
1崔华丽,吴媛媛.基于热拉深技术的车用轻量化高强7075铝板拉深性能研究[J].锻压技术,2018,43(5):76-79. 被引量:1
2黄和銮,李辉,罗铭强,林丽荧.铝合金等温挤压技术研究及应用分析[J].世界有色金属,2021,46(22):150-151. 被引量:1
1岳智.车用铝合金中铝板冲压的设计及生产关键技术探讨[J].时代汽车,2020(13):131-132.
2李浩,黎华杰,黄东男.挤压速度对6063铝合金内螺纹管管壁组织形貌的影响[J].轻合金加工技术,2023,51(6):34-44.
1杨永明,肖斌,赵军.颚式破碎机偏心轴楔横轧成形可行性研究[J].热加工工艺,2013,42(15):115-117. 被引量:1
2刘鹏涛,马立峰,贾伟涛,徐海洁,蒋亚平.宽幅AZ31B铸轧镁合金温轧工艺条件的组织性能[J].材料热处理学报,2015,36(S2):34-40. 被引量:1
3历时8年,变速箱复杂锻件技术终被攻克[J].锻造与冲压,2017,0(11):16-16.
4郑彦博,谢彪,令狐荣波,姜奥雄.凿岩机钎套温挤压工艺数值模拟优化[J].模具制造,2017,17(6):54-57.
5景屹峰.用铝合金5056热挤压导体零件[J].金属加工:热加工,2017,0(13):36-38.
6郎利辉,巫永坤,陈杨锴,王耀,孙志莹.铝合金汽车顶盖充液成形的数值模拟[J].精密成形工程,2017,9(3):13-18. 被引量:7
7李芮宇,孙宇新,付艳恕,孙其然,赵亚运.铝—铝爆炸焊接界面波形成与特征[J].焊接学报,2017,38(5):92-95. 被引量:3
8薛勇,陈帅帅,吴耀金,李宏,张治民.杯形件径向-反向复合挤压成形的应变分析[J].兵器材料科学与工程,2017,40(3):74-78.
9冯志军,阮明,李宇飞,王伟,石飞,吴江,苏鑫,李泽华.铸造技术路线图:半固态铸造[J].铸造,2017,66(6):541-547.
10蒋方敏,吴运新,张涛,龚海.基于元胞自动机法的7055铝合金动态再结晶模拟研究[J].热加工工艺,2017,46(12):235-238. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG376[金属学及工艺—金属压力加工]
Citation Information:
The effects of key parameters on forming performance of 7A60 aluminum alloy cup during isothermal pressure torsion were investigated by technological experiments and finite element simulation. The results show that the effect of height to diameter ratio of the blank on cumulative deformation is mainly in upsetting deformation stage. As lower mould torsion speed increases, the forming load is reduced and the torque increases. When lower mould torsion speed is too large, the damage value of transition fillet area of the torsional disk would be greater than 1, and the edge is easy to fracture. The influence is significant of forming temperature on forming load and torque. The continuity of the alloy cannot be destroyed with a torsional shear deformation of less than one ring during forming process,and its strength is improved corn pared with the alloy obtained by conventional extrusion.
quote
| GB/T 7714-2015 | [1] XUE Ke-min, BAO Dong-qing, WANG Jiu-lin, et al. Analysis for Key Process Parameters during Isothermal Pressure Torsion of 7A60 Aluminium Alloy Cup[J]. Rare Metals and Cemented Carbides, 2017(3): 50-55. |
| MLA | [1] XUE Ke-min, et al., "Analysis for Key Process Parameters during Isothermal Pressure Torsion of 7A60 Aluminium Alloy Cup." Rare Metals and Cemented Carbides, no. 3, 2017, pp. 50-55. |
| APA | [1] XUE Ke-min, BAO Dong-qing, WANG Jiu-lin, & LI Ping. (2017). Analysis for Key Process Parameters during Isothermal Pressure Torsion of 7A60 Aluminium Alloy Cup. Rare Metals and Cemented Carbides(3), 50-55. |
| IEEE | [1] XUE Ke-min, BAO Dong-qing, WANG Jiu-lin, and LI Ping, "Analysis for Key Process Parameters during Isothermal Pressure Torsion of 7A60 Aluminium Alloy Cup," Rare Metals and Cemented Carbides, no. 3, pp. 50-55, 2017. keywords: {7 A60 aluminum alloy;cup;isothermal pressure torsion;molding temperature;torsion angle} |