Study on La and Ce Distribution Ratio and Separation Factor in P204-HCl-H_3cit System AITranslate
Abstract AITranslate
In view of low separation factor of La( Ⅲ ) and Ce( Ⅲ ) in P204-HCl system, study was made of the effects of the feed solution acidity and citric acid(H3cit) concentration on the distribution ratio and the separation factor of La( Ⅲ ) and Ce( Ⅲ )and the extraction capacity. The mechanism of the increase of the La ( Ⅲ ) and Ce( Ⅲ ) separation factor was analyzed by FT-IR method. The experiment results showed that in P204-HCl-H3cit system,La and Ce distribution ratio and separation factor were lower with higher acidity but higher with higher citric acid concentration, while RE element extraction capacity was increased with higher citric acid concentration. With acid concentration 0.25 mol/L and feed acidity pH = 1.0, La and Ce separation factor was 4.1 ,and the maximum RE element extraction capacity was 24 g/L,which was superior to saponified P204-HCl system with the same acidity.
KeyWords AITranslate
1余晓皎,姚秉华,永长幸雄.二(2-乙基己基)膦酸萃取镧系元素研究[J].稀土,2006,27(6):59-61. 被引量:4
2卢克义.稀土湿法冶炼工艺学[M].北京:中国有色金属工业总公司职工教育教材编审办公室,1986.208.
3Nagaosa Y, Binghua Y. Recovery and separation of lanthanum(Ⅲ) ,aluminum(Ⅲ ), cobalt(Ⅱ), and nickel(Ⅱ) from mish metal by solvent extraction using bis(2-ethyl hexyl) phosphinic acid[J]. Sep Sci Technol, 1997, 32(6):1053-1065.
4Morais C A, Ciminelli V S T. Process development for the recovery of high-grade lanthanum by solvent extraction[J]. Hydrometallurgy, 2004,73:237-244.
5Luu Minh Dai,Dang Vu Minha, Pham Van Hai. Solvent extraction of lanthanides with triisoamylphosphate and di-(2-ethylhexyl) phosphoric acid from trichloroacetic acid and nitric acid solutions[J]. Journal of Alloys and Compounds, 2000,311 : 46-52.
6Sun Xiao-bo,Wang Yi-ge, Li De-qian. Selective separation of yttrium by CA-100 in the presence of a complexing agent[J]. Journal of Alloys and Compounds, 2006,408-412:999-1002.
7Zhang Yu-liang,Jiang Wei-hua, Liu Wei-sheng, et al. Complexation and extractability studies of lanthanide elements by2-[- 1,2-phenylenebis (oxy)] -bis ( N-methyl-N- phenyl(acetamide) [J]. Polyhedron, 2003, 22:1695- 1699.
8Kedari C S,Pandit S S,Ramanuiam A. Studies on the in situ electrooxidation and selective permeation of cerium (IV pho 199 across a bulk liquid membrane containing tributyl phate as the ion transporter[J]. Sep Sci Technol, ,34(9):1907-1923.
9Morais C A, Ciminelli V S T. Recovery of europium from a rare earth chloride solution[J]. Hydrometallurgy, 1998,49 :167-177.
10Morais C A,Ciminelli V S T. Recovery of europium by chemical reduction of a commercial solution of europium and gadolinium chlorides [J]. Hydrometallurgy, 2001,60 : 247-253.
1李剑虹,张兴.P204-HCl-HAc体系萃取La的机理分析与萃取平衡常数[J].稀有金属与硬质合金,2010,38(2):11-13. 被引量:1
2李剑虹.D_2EHPA-HCl-HAc体系萃取P_m(Ⅲ)的机理与平衡常数[J].有色金属:冶炼部分,2010(5):40-42.
3李剑虹.D_2 EHPA-HCl-HAc体系萃取Nd(Ⅲ)的机理分析与萃取平衡常数[J].矿冶,2011,20(1):43-46.
4徐志高,王力军,吴延科,池汝安,李攀红,阳慧芳.DIBK-P204体系萃取分离锆和铪的机理[J].中国有色金属学报,2013,23(7):2061-2068. 被引量:10
1徐志高,王力军,吴延科,池汝安,李攀红,阳慧芳.DIBK-P204体系萃取分离锆和铪的机理[J].中国有色金属学报,2013,23(7):2061-2068. 被引量:10
2徐志高,李攀红,池汝安,王力军,吴明,赵骏.DIBK协萃体系负载有机相反萃行为研究[J].有色金属:冶炼部分,2015(4):20-23. 被引量:4
3董雪平,郭树军,徐欣.锆铪萃取分离机理的研究进展[J].广州化工,2015,43(23):42-44. 被引量:3
4李洁,王占明.电感耦合等离子体原子发射光谱法测定铪合金中锆[J].冶金分析,2016,36(1):71-74. 被引量:9
5李攀红,徐志高,池汝安,赵骏,王力军,徐源来.湿法分离锆铪的研究进展[J].稀有金属,2016,40(5):499-508. 被引量:8
6赵骏,徐志高,张文杰,李攀红,池汝安,徐源来.DIBK-TOPO体系萃取锆和铪的动力学研究[J].稀有金属,2017,41(1):108-112. 被引量:6
7柴延全,郑仕鸿,赵卓.锆铪分离技术的研究现状及发展趋势[J].有色金属工程,2017,7(2):30-34. 被引量:9
8王俊莲,付家帅,许文,王化军.基于锆铪溶剂萃取分离的萃取剂性能[J].稀有金属,2020,44(6):658-667. 被引量:7
9徐志高,徐斐,董攀飞,吴明,何正艳,瞿军,池汝安.溶剂协同萃取分离锆和铪技术研究进展[J].有色金属工程,2021,11(12):57-67.
10梁耕宇,苏学斌,刘康,王桂硕,程浩,张承天,刘忠臣,刘会武,向秋林.用N235从独居石优溶渣浸出液中萃取铁的动力学研究[J].湿法冶金,2023,42(2):127-132.
1常宏涛,吴文远,涂赣峰,赵治华,李东,桑晓云.P204-HCl-H3cit体系萃取分离轻稀土的研究[J].稀土,2008,29(3):18-21. 被引量:15
2何捍卫,贾守亚,郭伟信.HEDTA-H_3Cit体系阳离子交换色层法分离镱和镥的研究[J].中国稀土学报,2010,28(1):43-47. 被引量:4
3王振文,徐晓辉,阮书锋,江培海.钴白合金浸出工艺研究[J].矿冶,2009,18(4):41-43. 被引量:10
4马亮帮,范必威,宁丽荣.TBP从加表面活性剂的碱性溶液中萃取金[J].有色金属,2007,59(4):78-81. 被引量:1
5杨幼明,张胜其,黄振华,张剑,管新地,刘建华.P507-N235载酸有机相分解稀土的试验研究[J].有色金属科学与工程,2016,7(1):114-118. 被引量:4
6潘路.丁基苯并噻唑亚砜萃取钯(II)的性能研究[J].有色金属:冶炼部分,2005(4):31-33. 被引量:1
7张寅生,王成彦,江培海,邱定蕃,梁德华,邓春龙.P204萃取分离锑铁工艺研究[J].有色金属:冶炼部分,2003(2):2-4. 被引量:5
8杨利姣,陈南春,钟夏平,解庆林,高军,郎耀秀,刘长淼,吴照洋.NaCl-HCl体系浸出铅渣中铅的动力学分析[J].中国有色金属学报,2015,25(6):1705-1712. 被引量:10
9凌育柱.P_(507)—HCl体系轻、中、重稀土全萃取连续分离工艺在寻乌的应用[J].稀土,1989(2):68-68.
10林河成.江西省稀土研究所4项科技成果通过鉴定[J].稀土信息,1994(9):6-6.
Basic Information:
DOI:
Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]
Citation Information:
In view of low separation factor of La( Ⅲ ) and Ce( Ⅲ ) in P204-HCl system, study was made of the effects of the feed solution acidity and citric acid(H3cit) concentration on the distribution ratio and the separation factor of La( Ⅲ ) and Ce( Ⅲ )and the extraction capacity. The mechanism of the increase of the La ( Ⅲ ) and Ce( Ⅲ ) separation factor was analyzed by FT-IR method. The experiment results showed that in P204-HCl-H3cit system,La and Ce distribution ratio and separation factor were lower with higher acidity but higher with higher citric acid concentration, while RE element extraction capacity was increased with higher citric acid concentration. With acid concentration 0.25 mol/L and feed acidity pH = 1.0, La and Ce separation factor was 4.1 ,and the maximum RE element extraction capacity was 24 g/L,which was superior to saponified P204-HCl system with the same acidity.
quote
| GB/T 7714-2015 | [1] CHANG Hong-tao, WU Wen-yuan, WANG Dan, et al. Study on La and Ce Distribution Ratio and Separation Factor in P204-HCl-H_3cit System[J]. Rare Metals and Cemented Carbides, 2008(2): 1-5. |
| MLA | [1] CHANG Hong-tao, et al., "Study on La and Ce Distribution Ratio and Separation Factor in P204-HCl-H_3cit System." Rare Metals and Cemented Carbides, no. 2, 2008, pp. 1-5. |
| APA | [1] CHANG Hong-tao, WU Wen-yuan, WANG Dan, BIAN Xue, & TU Gan-feng. (2008). Study on La and Ce Distribution Ratio and Separation Factor in P204-HCl-H_3cit System. Rare Metals and Cemented Carbides(2), 1-5. |
| IEEE | [1] CHANG Hong-tao, WU Wen-yuan, WANG Dan, BIAN Xue, and TU Gan-feng, "Study on La and Ce Distribution Ratio and Separation Factor in P204-HCl-H_3cit System," Rare Metals and Cemented Carbides, no. 2, pp. 1-5, 2008. keywords: {P204;RE;separation factor;extraction capacity;citric acid} |