Abstract AITranslate
<Abstrcat>Study is made on the technical requirements for the tests and production of ultra-pure tantalum oxide/ultra-pure niobium oxideDescription is made of the bench-scale tests,pilot tests and commercial-scale tests on the ultra-pure tantalum oxide/ultra-pure niobium oxide.It also describes the technical index and its application.
KeyWords AITranslate
1王肇信 幸良佐 曾芳屏.钽铌冶金学[M].北京:稀有金属冶金学会,1998.232-254.
1李光伟,许延辉,赵文怡,马升峰.富铌渣硫酸浸出液中铌的分离工艺研究[J].稀土,2013,34(4):57-62. 被引量:5
2晏慧娟,唐德胜.传统工艺生产氧化钽(铌)除杂技术特点及研究进展[J].稀有金属与硬质合金,2016,44(4):14-19. 被引量:4
3孙林泉,王丽娜,于宏东,苏慧,陈德胜,齐涛.低品位含铌矿物中铌的提取工艺研究进展[J].化工学报,2021,72(4):1847-1862. 被引量:3
4黄永,贾秀敏,刘会武,刘忠臣,向秋林.用N503从低浓度铌溶液中萃取铌试验研究[J].湿法冶金,2023,42(3):258-262.
1郭财胜,李梅,柳召刚,张栋梁,高凯.白云鄂博稀土、铌资源综合利用现状及新思路[J].稀土,2014,35(1):96-100. 被引量:53
2王常清,易艳萍,曹小华,严平.以铌铁作为铌矿替代原料生产高纯氧化铌的研究[J].有色金属:冶炼部分,2018(9):40-43. 被引量:2
3王威,柳林,曹耀华,刘红召,张博,王洪亮.从某钾长石尾矿中提取稀土和铌工艺研究[J].有色金属:冶炼部分,2020,0(6):43-47. 被引量:1
4鲁东,喻文斌,王诗海,张伟宁,郭洪范.结晶法和萃取法制备高纯氧化铌的研究[J].广州化工,2020,48(20):53-54. 被引量:1
5颉维平,喻文斌,鲁东,李辉,张伟宁,郭洪范.以汞为介质分离钽、铌金属废料的研究[J].中国金属通报,2020(16):228-229.
6潘岩,鄢锋,郭徽,唐昭辉,杨静雅,曾祥吉.有色金属冶炼自动控制研究现状与展望[J].中国有色金属学报,2021,31(1):96-105. 被引量:2
7孙林泉,王丽娜,于宏东,苏慧,陈德胜,齐涛.低品位含铌矿物中铌的提取工艺研究进展[J].化工学报,2021,72(4):1847-1862. 被引量:3
8刘建迪,王静静,李伟,刘平,马凤仓,张柯,陈小红.钽的提取研究进展[J].矿产保护与利用,2021,41(2):163-173.
9洪汛海,文明,王储,郭靖.微波场中铌精矿碳热还原反应行为研究[J].有色金属:冶炼部分,2022(2):76-82. 被引量:2
10冉孟杰,任国兴,肖松文,陈雯.白云鄂博铌资源提取研究进展[J].稀有金属与硬质合金,2022,50(5):12-18. 被引量:1
1王振铎,李洪坤.精炼炉铬尘处理方案实践效果[J].铁合金,2010,41(2):27-29.
2卢苏君,王书友,诸葛福瑜,张晗,张鹏.Co(Ⅲ)-Na_2SO_3-H_2SO_4体系浸出钴的研究[J].有色金属:冶炼部分,2013(5):17-19. 被引量:5
3王振文,江培海,尹飞,阮书锋,姚志超.高硅钴白合金加压浸出工艺研究[J].矿冶,2013,22(2):67-70. 被引量:3
4赵江华,朱贺民.炼钢污泥直接混入烧结的试验与生产[J].安徽冶金科技职业学院学报,2004,14(4):23-25.
5向天德.莱钢竖炉配加印度精粉试验与生产[J].球团技术,2004(1):32-34.
6何焕杰,赵德启,詹适新,冯建中.中性磷萃淋树脂吸附铼的性能和机理研究——CL-TBP-KReO_4-H_2SO_4体系[J].湿法冶金,1992(4):20-23.
7孙志鹏.南钢高MgO烧结矿试验生产实践[J].南钢科技与管理,2004(2):1-4. 被引量:1
8贾福存.绝热板的试验与生产[J].唐钢科技,1989(1):29-32.
9陈曙光,许志军.电弧炼钢炉衬不烘烤炼钢工艺试验与生产应用[J].河北机械,1993(3):78-79.
10王百年,左权,陈洋,王艳成,杨保俊.H_2O_2-Fe_2(SO_4)_3-H_2SO_4体系中辉铜矿的浸取研究[J].有色金属:冶炼部分,2016(12):5-9. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
<Abstrcat>Study is made on the technical requirements for the tests and production of ultra-pure tantalum oxide/ultra-pure niobium oxideDescription is made of the bench-scale tests,pilot tests and commercial-scale tests on the ultra-pure tantalum oxide/ultra-pure niobium oxide.It also describes the technical index and its application.
quote
| GB/T 7714-2015 | [1] KUANG Guo-zhen, ZHOU Huo-gen, ZHANG Hao, et al. Production of Ultra-pure Tantalum Oxide/Ultra-pure Niobium Oxide from CH_3(CH_2)_5CHOHCH_3-HF-H_2SO_4 System[J]. Rare Metals and Cemented Carbides, 2005(2): 1-3. |
| MLA | [1] KUANG Guo-zhen, et al., "Production of Ultra-pure Tantalum Oxide/Ultra-pure Niobium Oxide from CH_3(CH_2)_5CHOHCH_3-HF-H_2SO_4 System." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 1-3. |
| APA | [1] KUANG Guo-zhen, ZHOU Huo-gen, ZHANG Hao, DUAN Qin-zheng, WAN Guo-shun, & YANG Ji-hong. (2005). Production of Ultra-pure Tantalum Oxide/Ultra-pure Niobium Oxide from CH_3(CH_2)_5CHOHCH_3-HF-H_2SO_4 System. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] KUANG Guo-zhen, ZHOU Huo-gen, ZHANG Hao, DUAN Qin-zheng, WAN Guo-shun, and YANG Ji-hong, "Production of Ultra-pure Tantalum Oxide/Ultra-pure Niobium Oxide from CH_3(CH_2)_5CHOHCH_3-HF-H_2SO_4 System," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 2005. keywords: {extraction;ultra-pure tantalum oxide;ultra-pure niobium oxide;technical index} |