The Thermodynamics Analysis on the Deposition Process of Metal Carbonates AITranslate

School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on concentration-pH graph,study is made of relationship between pH and equilibrium concentration of some representative metal ion in the solution containing CO2-_3.In terms of thermodynamic analysis,the characteristic and the pH conditions of carbonate deposition,the possibility of separating metals by the process of carbonate deposition is discussed.

KeyWords AITranslate

carbonate deposition concentration-pH graph thermodynamics analysis

1刘建本,易保华,肖卓炳,陈德根,陈上,张永康.液相法制备纳米氧化锌的研究(Ⅰ)[J].吉首大学学报,2000,21(2):9-11. 被引量:11

2陈洪龄,吕家桢,陆小华,张吕正,王延儒.沉淀法制备超细碳酸钙[J].南京化工大学学报,1998,20(3):23-26. 被引量:13

3崔爱莉,孙晓明,董亚杰,李亚栋.控制沉淀法制备不同形貌的碳酸钙超细粉(英文)[J].无机化学学报,2001,17(4):518-522. 被引量:10

1常皓,柴立元,王云燕,舒余德,周敏.Cu^(2+)-H_2O系羟合配离子配位平衡研究[J].矿冶工程,2007(6):37-40. 被引量:9

2柴立元,常皓,王云燕,舒余德,李敬,袁林,王璞,方艳,赵堃.Cd^(2+)-H_2O系羟合配离子配位平衡[J].中国有色金属学报,2007,17(3):487-491. 被引量:7

3王云燕,柴立元,王庆伟,舒余德.重金属离子(Zn^2+,Cu^2+,Cd^2+,Pb^2+)-水系羟合配离子配位平衡研究[J].中国有色金属学报,2008,18(E01):183-191. 被引量:17

4王云燕,柴立元,常皓,彭小玉,舒余德.Equilibrium of hydroxyl complex ions in Pb^(2+)-H_2O system[J].中国有色金属学会会刊:英文版,2009,19(2):458-462. 被引量:2

5杨天足,任晋,刘伟锋,窦爱春,刘伟,张杜超.Zn(Ⅱ)-Glu^(2-)-CO_3^(2-)-H_2O体系热力学平衡分析[J].中国有色金属学报,2009,19(6):1155-1161. 被引量:8

6杨春.Ni^(2+)-H_2O系配位平衡研究[J].贵州大学学报:自然科学版,2011,28(2):130-132.

7杜蓉娟,衣守志,陈琛.酸洗废液制备高纯氧化铁红[J].化工环保,2012,32(5):448-451. 被引量:7

8杨晨璟,杜景红,甘国友,严继康,易健宏.掺杂TiO_2粉体共沉淀包膜过程中的热力学研究[J].材料科学与工艺,2012,20(4):70-75. 被引量:1

9梅颖,薛余化,叶恒朋,杜冬云.利用二氧化碳选择性分离回收含锰废水中的锰[J].化工学报,2017,68(7):2798-2804. 被引量:9

10侯柏秋,俞小花,沈庆峰,杨大锦,张候文,赵群,谢刚.锌电解液中铅的去除研究现状[J].化学研究,2023,34(4):366-376.

1周敏,闵小波,柴立元,王云燕,舒余德,王娜.Ni-NH_3-H_2O系热力学平衡研究[J].有色金属:冶炼部分,2009(1):2-5. 被引量:2

2杨天足,刘珍珍,任晋,窦爱春,刘伟,刘伟锋,张杜超.Cu(II)-Glu^(2-)-CO_3^(2-)-H_2O体系热力学平衡分析[J].过程工程学报,2009(4):745-749. 被引量:7

3柴立元,尤翔宇,舒余德,杨杰,王云燕.印刷电路板含铜配离子复杂废水脱铜研究[J].中南大学学报:自然科学版,2010,41(1):27-33. 被引量:7

4刘伟锋,杨天足,夏星.Behavior of silver and lead in selective chlorination leaching process of gold-antimony alloy[J].中国有色金属学报:英文版,2010,20(2):322-329. 被引量:4

5王瑞祥,武岩鹏,唐谟堂.Cd(Ⅱ)-NH_3-Cl^--H_2O体系配合平衡[J].有色金属:冶炼部分,2010(4):2-5. 被引量:1

6许家友,叶柳英,林凯勉,周细濠.月桂酸锌的合成及其红外特征的研究[J].聚氯乙烯,2010,38(9):31-34. 被引量:1

7杨天足,雷存茂,刘伟,窦爱春,张杜超,刘伟锋.Cu(Ⅱ)在谷氨酸根配合物体系中的电沉积行为[J].中南大学学报:自然科学版,2011,42(2):305-311.

8李新颖,Francis Ruzagiliza Innocent,陈泉源,薛罡.沉淀法处理含铜废水及其沉淀产物的表征[J].化工环保,2011,31(4):298-303. 被引量:11

9高万超,杨朝晖,黄兢,邓久华,徐海音,谢华明.微生物絮凝剂捕集Cu(Ⅱ)的响应面优化及机理研究[J].环境工程学报,2011,5(11):2411-2416. 被引量:5

10刘智勇,刘志宏,曹志阎,李启厚,杨天足.硅锌矿在(NH_4)_2SO_4-NH_3-H_2O体系中的浸出机理[J].中国有色金属学报,2011,21(11):2929-2935. 被引量:11

1林清泉,顾帼华,王晖,王重庆,刘有才,朱仁锋,符剑刚.碳酸盐沉淀法分离硫酸盐溶液中的锰与钙和镁(英文)[J].中国有色金属学报:英文版,2016,0(4):1118-1125. 被引量:6

2姜萍,徐迎春.钨钼分离方法的研究现状与发展[J].世界有色金属,2000(10):16-17. 被引量:1

3李洪桂,孙培梅,李运姣,赵中伟,苏鹏抟,刘茂盛.钨酸盐溶液中除钼砷锑锡等杂质的研究[J].中国有色金属学报,2000,10(4):539-541. 被引量:8

4徐艳娥,谢克强,邢鹏.湿法冶金中钴锰分离方法综评[J].矿冶,2014,23(1):55-60. 被引量:5

5田占欣.以硫化物状态选择性沉淀分离锌和镍的可行性研究[J].有色矿冶,1996,12(1):34-36. 被引量:1

6方成开,谭佩君.从钴镍废料电溶液中分离回收钴镍[J].湿法冶金,2003,22(4):169-182. 被引量:21

7韩新罡,席晓丽,马立文,聂祚仁,周志理.配合-沉淀体系中铁与钴、镍的分离性能[J].中国有色金属学报,2013,23(11):3218-3224. 被引量:5

8韩旗英,杨金华,凌诚,白炜.晶型重稀土碳酸盐沉淀工艺技术[J].湖南有色金属,2009,25(6):31-34. 被引量:6

9何显达,许开华,陈尧,陈艳红,王勤,叶红齐.pH和加料方式对选择性沉淀分离镍锰的影响[J].湿法冶金,2011,30(4):298-303. 被引量:1

10闻振乾,刘忠臣,刘会武,赵杰.沉淀法分离镍锌研究进展[J].湿法冶金,2013,32(5):281-283. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF111.34[冶金工程—冶金物理化学]

Citation Information:

Based on concentration-pH graph,study is made of relationship between pH and equilibrium concentration of some representative metal ion in the solution containing CO2-_3.In terms of thermodynamic analysis,the characteristic and the pH conditions of carbonate deposition,the possibility of separating metals by the process of carbonate deposition is discussed.

quote

GB/T 7714-2015 [1] LI Bo. The Thermodynamics Analysis on the Deposition Process of Metal Carbonates[J]. Rare Metals and Cemented Carbides, 2005(2): 4-8.
MLA [1] LI Bo. "The Thermodynamics Analysis on the Deposition Process of Metal Carbonates." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 4-8.
APA [1] LI Bo. (2005). The Thermodynamics Analysis on the Deposition Process of Metal Carbonates. Rare Metals and Cemented Carbides(2), 4-8.
IEEE [1] LI Bo, "The Thermodynamics Analysis on the Deposition Process of Metal Carbonates," Rare Metals and Cemented Carbides, no. 2, pp. 4-8, 2005. keywords: {carbonate deposition;concentration-pH graph;thermodynamics analysis}