Investigating the Effect of Changing the Nanostructure of the Core in the Core–Shell Assembly for High-Efficiency Electromagnetic Wave Absorbers Investigating the Effect of Changing the Nanostructure of the Core in the Core–Shell Assembly for High-Efficiency Electromagnetic Wave Absorbers AITranslate
Abstract AITranslate
The magnetic-dielectric core–shell structure is considered to achieve high-performance electromagnetic absorption due to the ability to use a wide range of materials and different geometrics. In this work, the effects of various nanostructures of cores on the electromagnetic absorption behavior of magnetic-dielectric core–shell structures are investigated. Herein, a BaFe12O19@MoS2 core–shell was synthesized by a hydrothermal method, and for preparing BaFe12O19 as a core with two different geometrics, the hydrothermal and sol–gel methods are used. The minimum value of reflection loss (RLmin) for BaFe12O19@MoS2, where the hexaferrite core is prepared as a nanostructure, is −53.36 at 13.1 GHz (Ku band), and the absorption bandwidth is 4.6 GHz (11.0–15.6 GHz) at a 2.0 mm thickness. Meanwhile, for BaFe12O19@MoS2, in which the structure of its core is a nanostructure (a hexagonal plate-like structure), RLmin is −41.71 at 5.1 GHz (C band), and the absorption bandwidth is 2.0 GHz (4.3–6.3 GHz) at 5.0 mm. However, in our research, by changing the size and geometry of the core nanostructures, a suitable reflection loss with an appropriate absorption bandwidth is obtained in C or Ku band frequencies.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00001
Chinese Library Classification Number:
Citation Information:
The magnetic-dielectric core–shell structure is considered to achieve high-performance electromagnetic absorption due to the ability to use a wide range of materials and different geometrics. In this work, the effects of various nanostructures of cores on the electromagnetic absorption behavior of magnetic-dielectric core–shell structures are investigated. Herein, a BaFe12O19@MoS2 core–shell was synthesized by a hydrothermal method, and for preparing BaFe12O19 as a core with two different geometrics, the hydrothermal and sol–gel methods are used. The minimum value of reflection loss (RLmin) for BaFe12O19@MoS2, where the hexaferrite core is prepared as a nanostructure, is −53.36 at 13.1 GHz (Ku band), and the absorption bandwidth is 4.6 GHz (11.0–15.6 GHz) at a 2.0 mm thickness. Meanwhile, for BaFe12O19@MoS2, in which the structure of its core is a nanostructure (a hexagonal plate-like structure), RLmin is −41.71 at 5.1 GHz (C band), and the absorption bandwidth is 2.0 GHz (4.3–6.3 GHz) at 5.0 mm. However, in our research, by changing the size and geometry of the core nanostructures, a suitable reflection loss with an appropriate absorption bandwidth is obtained in C or Ku band frequencies.
quote
| GB/T 7714-2015 | [1] Hajar. Kazemi, Mahmood. Moradi, Gholam Hossein Bordbar. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00001. |
| MLA | [1] Hajar. Kazemi, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00001. |
| APA | [1] Hajar. Kazemi, Mahmood. Moradi, & Gholam Hossein Bordbar. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00001 |
| IEEE | [1] Hajar. Kazemi, Mahmood. Moradi, and Gholam Hossein Bordbar, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00001. keywords: {core−shell structure BaFe12O19 MoS2 electromagnetism microwave absorbers nanostructure} |