Study on Thermal Stability of Cathode Materials for Lithium-ion Batteries AITranslate

China Southern Power Grid Electric Vehicle Service Co.,Ltd.;China Southern Power Grid Electric Vehicle Service Co.,Ltd.;China Southern Power Grid Electric Vehicle Service Co.,Ltd.;China Southern Power Grid Electric Vehicle Service Co.,Ltd.;China Southern Power Grid Electric Vehicle Service Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The thermal decomposition of ternary materials and electrolyte was systematically studied by differential scanning calorimetry(DSC).The effects of different potentials and the amount of electrolyte on the thermal decomposition of ternary materials were analyzed.The results show that the thermal decomposition process of ternary materials undergoes a structural transformation from lamellar structure to spinel and then to rock-salt phase,accompanied by the precipitation of oxygen.The higher the Ni content and the higher the potential,the worse the thermal stability of the ternary material with lower thermal decomposition temperature and greater thermal decomposition enthalpy.For high-nickel materials,there is a corresponding relationship between the thermal stability and the structural phase change during charging,and there is an obvious difference in thermal stability at the phase transition point.The decomposition of electrolyte goes through the endothermic process of lithium salt decomposition and the exothermic process of the reaction of decomposition products with gasification solvent,and the addition amount of electrolyte has a great influence on the thermal decomposition process of ternary materials.

KeyWords AITranslate

lithium-ion battery ternary cathode material DSC electrolyte thermal decomposition thermal stability

1朱广焱,刘雪省,潘磊,蒋宁懿.三元材料在锂离子动力电池上的应用[J].电源技术,2009,33(7):547-551. 被引量:20

1冯婷,王睿,王京玥,王磊营,石沁灵,王立帆,詹纯.压电材料K_(0.5)Na_(0.5)NbO_(3)表面修饰高镍正极材料LiNi_(0.83)Co_(0.12)Mn_(0.05)O_(2)的电化学性能研究[J].稀有金属与硬质合金,2022,50(5):89-95. 被引量:1

2赵光金,李博文,胡玉霞,董锐锋,王放放.退役动力电池梯次利用技术及工程应用概述[J].储能科学与技术,2023,12(7):2319-2332.

1韦玉红,华骏,彭商权,肖佳俊,章聪华,谭旭峰,颜文斌.TiO_(2)包覆对V_(2)O_(5)锂离子电池负极材料电化学性能的影响[J].稀有金属与硬质合金,2023,51(2):90-97.

1傅岩,张铁鹰,孙英霞,李松育.通过定向进化技术提高角蛋白酶的热稳定性研究[J].动物营养学报,2021,33(10):5887-5894. 被引量:3

2吴江,钱佳炜,陈浩,李学彬,谷科城,刘浩.不同体系结构NCM正极材料环境适应性研究[J].化工新型材料,2021,49(9):107-110.

3戴闽光,高月英,赵振国,顾惕人.硅胶表面结构的热稳定性研究[J].高等学校化学学报,1981,2(4):495-502. 被引量:5

4汪涛,于维珂.高镍三元材料匹配钛酸锂负极电池的性能[J].电池,2021,51(5):498-501. 被引量:2

5李丽娟,朱振东,代娟,王蓉蓉,彭文.锂离子电池正极材料Li[Ni_(x)Co_(y)Mn_(z)]O_(2)(x=0.6,0.85)相变对比[J].电化学,2021,27(4):405-412. 被引量:2

6吕培召,杨春晖,沈仕轩,霍宇涛,饶中浩.基于表面改性的锂电池热质传递及热稳定性[J].工程热物理学报,2021,42(10):2657-2664.

7袁希召,侯自杰,黄文魁.碘杂环化合物的质谱研究[J].高等学校化学学报,1984,5(6):823-828. 被引量:1

8熊伦,李斌,涂朴.钇铝金属玻璃Y_(66.7)Al_(33.3)和Y_(75)Al_(25)的高压状态方程[J].四川师范大学学报:自然科学版,2021,44(6):806-811.

9吉莉,董霁红,房阿曼,黄艳利,李全生,曹志国.宝日希勒大型露天矿敏感区划定及重金属累积效应[J].生态学杂志,2021,40(10):3325-3338. 被引量:4

10曲凌辉,孟建兵,张宏伟,董小娟,李丽,王帅柯,关庆义,魏修亭.镍钛形状记忆合金表面微弧氧化膜的制备及性能[J].电镀与涂饰,2021,40(19):1507-1514.

Basic Information:

DOI:

Chinese Library Classification Number:TM911[电气工程—电力电子与电力传动]

Citation Information:

The thermal decomposition of ternary materials and electrolyte was systematically studied by differential scanning calorimetry(DSC).The effects of different potentials and the amount of electrolyte on the thermal decomposition of ternary materials were analyzed.The results show that the thermal decomposition process of ternary materials undergoes a structural transformation from lamellar structure to spinel and then to rock-salt phase,accompanied by the precipitation of oxygen.The higher the Ni content and the higher the potential,the worse the thermal stability of the ternary material with lower thermal decomposition temperature and greater thermal decomposition enthalpy.For high-nickel materials,there is a corresponding relationship between the thermal stability and the structural phase change during charging,and there is an obvious difference in thermal stability at the phase transition point.The decomposition of electrolyte goes through the endothermic process of lithium salt decomposition and the exothermic process of the reaction of decomposition products with gasification solvent,and the addition amount of electrolyte has a great influence on the thermal decomposition process of ternary materials.

quote

GB/T 7714-2015 [1] CHEN Hao-zhou, ZOU Da-zhong, LI Xun, et al. Study on Thermal Stability of Cathode Materials for Lithium-ion Batteries[J]. Rare Metals and Cemented Carbides, 2021(5): 47-52.
MLA [1] CHEN Hao-zhou, et al., "Study on Thermal Stability of Cathode Materials for Lithium-ion Batteries." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 47-52.
APA [1] CHEN Hao-zhou, ZOU Da-zhong, LI Xun, LIU Jin-hai, & HUANG Peng. (2021). Study on Thermal Stability of Cathode Materials for Lithium-ion Batteries. Rare Metals and Cemented Carbides(5), 47-52.
IEEE [1] CHEN Hao-zhou, ZOU Da-zhong, LI Xun, LIU Jin-hai, and HUANG Peng, "Study on Thermal Stability of Cathode Materials for Lithium-ion Batteries," Rare Metals and Cemented Carbides, no. 5, pp. 47-52, 2021. keywords: {lithium-ion battery;ternary cathode material;DSC;electrolyte;thermal decomposition;thermal stability}