daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Comparative Study of Cold Electron Emission from 2D Ti3C2TX MXene Nanosheets with Respect to Its Precursor Ti3SiC2 MAX Phase Comparative Study of Cold Electron Emission from 2D Ti3C2TX MXene Nanosheets with Respect to Its Precursor Ti3SiC2 MAX Phase AITranslate

CSIR-Institute of Minerals and Materials Technology; Savitribai Phule Pune University; Savitribai Phule Pune University; Amity University Maharashtra;Centre for Nano and Material Sciences, Jain Global Campus;Seismology Division, Bhabha Atomic Research Centre; India|Homi Bhabha National Institute; CSIR-Institute of Minerals and Materials Technology; CSIR-Institute of Minerals and Materials Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

2-D Ti3C2TX MXene nanosheets are obtained by etching Ti3SiC2 MAX phase that is synthesized by heating the elemental Ti, Si, and C mixture at high temperature. The electron emission behavior of both Ti3C2TX MXene and Ti3SiC2 MAX phase is studied. MXene exhibits excellent field emission characteristics with a turn-on field of 4.7 V μm–1, and that for the Ti3SiC2 MAX phase is 6.5 V μm–1. The turn-on electric field corresponding to an emission current density of 10 μA cm–2 is 5.0 V μm–1 for Ti3C2TX MXene and 7.5 V μm–1 for the Ti3SiC2 MAX phase. The calculated enhancement factor of MXene nanosheets is ∼4280, which is one of the highest reported enhancement factors to date. In order to get theoretical insight into the field emission properties for Ti3C2 and OH-terminated Ti3C2 MXene in comparison to the Ti3SiC2 MAX phase, we have presented the structure and electronic properties from state of the art density functional theory (DFT) simulations. The interaction of – OH with Ti3C2 involves charge transfer from the “Ti” 3d orbital to −OH. The computed work function follows the trend Ti3SiC2 > Ti3C2 > Ti3C2/OH, which supports the maximum field emission in −OH-terminated Ti3C2 MXene and the minimum field emission in the Ti3SiC2 MAX phase.

KeyWords AITranslate

MAX MXene field emission turnon field enhancement factor work function nanosheets
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00128

Chinese Library Classification Number:

Citation Information:

2-D Ti3C2TX MXene nanosheets are obtained by etching Ti3SiC2 MAX phase that is synthesized by heating the elemental Ti, Si, and C mixture at high temperature. The electron emission behavior of both Ti3C2TX MXene and Ti3SiC2 MAX phase is studied. MXene exhibits excellent field emission characteristics with a turn-on field of 4.7 V μm–1, and that for the Ti3SiC2 MAX phase is 6.5 V μm–1. The turn-on electric field corresponding to an emission current density of 10 μA cm–2 is 5.0 V μm–1 for Ti3C2TX MXene and 7.5 V μm–1 for the Ti3SiC2 MAX phase. The calculated enhancement factor of MXene nanosheets is ∼4280, which is one of the highest reported enhancement factors to date. In order to get theoretical insight into the field emission properties for Ti3C2 and OH-terminated Ti3C2 MXene in comparison to the Ti3SiC2 MAX phase, we have presented the structure and electronic properties from state of the art density functional theory (DFT) simulations. The interaction of – OH with Ti3C2 involves charge transfer from the “Ti” 3d orbital to −OH. The computed work function follows the trend Ti3SiC2 > Ti3C2 > Ti3C2/OH, which supports the maximum field emission in −OH-terminated Ti3C2 MXene and the minimum field emission in the Ti3SiC2 MAX phase.

quote

GB/T 7714-2015 [1] N Usha Kiran, Amol B. Deore, Mahendra A. More, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00128.
MLA [1] N Usha Kiran, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00128.
APA [1] N Usha Kiran, Amol B. Deore, Mahendra A. More, Dattatray J. Late, Chandra Sekhar Rout, Pratap Mane, Brahmananda Chakraborty, Laxmidhar Besra, & Sriparna Chatterjee. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00128
IEEE [1] N Usha Kiran, Amol B. Deore, Mahendra A. More, Dattatray J. Late, Chandra Sekhar Rout, Pratap Mane, Brahmananda Chakraborty, Laxmidhar Besra, and Sriparna Chatterjee, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00128. keywords: {MAX MXene field emission turnon field enhancement factor work function nanosheets}