daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fabrication of Metal–Organic Framework/Polymer Composites via a One-Pot Solvent Crystal Template Strategy AITranslate

Zhejiang University; The Chinese University of Hong Kong; Zhejiang University; The Chinese University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal–organic framework (MOF)/polymer composites combining advantages of both materials have received significant attention in the recent years. However, the complexity and inefficiency of the current fabrication approaches have hindered their further development. Herein, we demonstrate a facile one-pot solvent crystal template strategy to efficiently fabricate ZIF-8/polyurethane (PU) composites. This method eliminated the pre-synthesis and purification of MOFs, thus greatly simplifying the fabrication process. Moreover, the solvent crystal template introduced macropores in the polymer matrix, which generated a hierarchically porous structure to facilitate the molecular diffusion in the composite. The obtained ZIF-8/PU composites exhibited an accelerated dye adsorption rate constant of 1.89 × 10–3 g mg–1 min–1, which was 2.6 times higher than that of MOF powders. The Langmuir isotherm study further confirmed favorable adsorption of dye molecules with a maximum adsorption capacity of 18.1 mg g–1.

KeyWords AITranslate

metal−organic framework polymer composite onepot fabrication strategy solvent crystal template dye adsorption
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00096

Chinese Library Classification Number:

Citation Information:

Metal–organic framework (MOF)/polymer composites combining advantages of both materials have received significant attention in the recent years. However, the complexity and inefficiency of the current fabrication approaches have hindered their further development. Herein, we demonstrate a facile one-pot solvent crystal template strategy to efficiently fabricate ZIF-8/polyurethane (PU) composites. This method eliminated the pre-synthesis and purification of MOFs, thus greatly simplifying the fabrication process. Moreover, the solvent crystal template introduced macropores in the polymer matrix, which generated a hierarchically porous structure to facilitate the molecular diffusion in the composite. The obtained ZIF-8/PU composites exhibited an accelerated dye adsorption rate constant of 1.89 × 10–3 g mg–1 min–1, which was 2.6 times higher than that of MOF powders. The Langmuir isotherm study further confirmed favorable adsorption of dye molecules with a maximum adsorption capacity of 18.1 mg g–1.

quote

GB/T 7714-2015 [1] Congcong Chen, He Zhu, BoGeng Li, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00096.
MLA [1] Congcong Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00096.
APA [1] Congcong Chen, He Zhu, BoGeng Li, & Shiping Zhu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00096
IEEE [1] Congcong Chen, He Zhu, BoGeng Li, and Shiping Zhu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00096. keywords: {metal−organic framework;polymer composite;onepot fabrication strategy;solvent crystal template;dye adsorption}