daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Wet Spinning and Structure Analysis of α-1,3-Glucan Regenerated Fibers AITranslate

The University of Tokyo; The University of Tokyo; The University of Tokyo; The University of Tokyo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Because of the increasing concerns related to fiber wastes resulting from non-biodegradable plastics and their impact in terms of environmental pollution, the demand for the development of biodegradable fibers has increased. Regenerated fibers of polysaccharides are expected as biomass fibers because of their biodegradability and structural variety. In this study, a linear polysaccharide synthesized by in vitro enzymatic polymerization, α-1,3-glucan, was wet-spun using 8% (w/w) lithium chloride in a dimethylacetamide solution. When ethanol (EtOH) was used in the coagulation bath, the resulting fibers were transparent, flexible, and dense, whereas the fibers produced with water in the coagulation bath were translucent, brittle, and aggregated. The former regenerated fibers exhibited tensile strength (11 cN/tex, 138 MPa), elongation at break (12%), and Young’s modulus (3.5 GPa). The X-ray fiber diagram of the regenerated fibers coagulated in EtOH showed that the fibers were well-oriented along the fiber axis. The crystalline structure was determined to consist of a twofold helix with crystal lattice parameters of a = 1.59 nm, b = 0.976 nm, and c (fiber axis) = 0.852 nm.

KeyWords AITranslate

wet spinning regenerated fibers polysaccharides α1 3glucan crystal structure
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00114

Chinese Library Classification Number:

Citation Information:

Because of the increasing concerns related to fiber wastes resulting from non-biodegradable plastics and their impact in terms of environmental pollution, the demand for the development of biodegradable fibers has increased. Regenerated fibers of polysaccharides are expected as biomass fibers because of their biodegradability and structural variety. In this study, a linear polysaccharide synthesized by in vitro enzymatic polymerization, α-1,3-glucan, was wet-spun using 8% (w/w) lithium chloride in a dimethylacetamide solution. When ethanol (EtOH) was used in the coagulation bath, the resulting fibers were transparent, flexible, and dense, whereas the fibers produced with water in the coagulation bath were translucent, brittle, and aggregated. The former regenerated fibers exhibited tensile strength (11 cN/tex, 138 MPa), elongation at break (12%), and Young’s modulus (3.5 GPa). The X-ray fiber diagram of the regenerated fibers coagulated in EtOH showed that the fibers were well-oriented along the fiber axis. The crystalline structure was determined to consist of a twofold helix with crystal lattice parameters of a = 1.59 nm, b = 0.976 nm, and c (fiber axis) = 0.852 nm.

quote

GB/T 7714-2015 [1] Azusa Togo, Shiori Suzuki, Satoshi Kimura, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00114.
MLA [1] Azusa Togo, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00114.
APA [1] Azusa Togo, Shiori Suzuki, Satoshi Kimura, & Tadahisa Iwata. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00114
IEEE [1] Azusa Togo, Shiori Suzuki, Satoshi Kimura, and Tadahisa Iwata, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00114. keywords: {wet spinning;regenerated fibers;polysaccharides;α1;3glucan;crystal structure}