daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Castor Oil-Based Bioplastics via Polyesterification: Synthesis, Characterization, and Functionalization AITranslate

Huazhong Agricultural University; Huazhong Agricultural University; Huazhong Agricultural University; Huazhong Agricultural University; Huazhong Agricultural University; Wuhan Textile University; Huazhong Agricultural University; Peking University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Synthesis and application of biobased polymers are at the forefront of polymer science. Herein, we report the synthesis, characterization, and functionalization of castor oil-based bioplastics. At first, polymer P1 was synthesized via polyesterification by using monomer 11-bromoundecanoic acid (1) to demonstrate the feasibility of this step-growth polymerization method. The success of this polycondensation technique relies on the high substitution efficiency between terminal groups, carboxylic acid, and carbon-bromide moieties under alkaline conditions. Subsequently, copolymers P2–P5 with varied compositions were obtained by random copolymerization of monomers 1 and 6-bromohexanoic acid (2) in different feed ratios. Linear positive correlation is disclosed between the crystallization (Tc) and melting (Tm) temperatures of P1–P5 and the molar fraction of 1 within these specimens. Differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (WAXD) results illustrate good crystallinity of these bioplastics. Furthermore, the degradation of polymers P1–P5 is propelled by an external basic environment while hindered by their intrinsic hydrophobicity, indicating that alkalinity and composition are two essential factors to manipulate the degradation behaviors of biobased polyesters in the bulk state. Ultimately, polymerization of 1 in the presence of 1-pyrenebutyric acid (3), an end-capping agent, was carried out to yield α-pyrene functionalized polymer P7. This material is capable of serving as a practical fluorescent probe and multiwalled carbon nanotube (MWNT) dispersion stabilizer. Polyesterification reported herein represents a facile and cost-effective synthetic strategy and shows great prospects in sustainable polymer materials.

KeyWords AITranslate

castor oil bioplastic polyesterification fluorescent probe carbon nanotube
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00109

Chinese Library Classification Number:

Citation Information:

Synthesis and application of biobased polymers are at the forefront of polymer science. Herein, we report the synthesis, characterization, and functionalization of castor oil-based bioplastics. At first, polymer P1 was synthesized via polyesterification by using monomer 11-bromoundecanoic acid (1) to demonstrate the feasibility of this step-growth polymerization method. The success of this polycondensation technique relies on the high substitution efficiency between terminal groups, carboxylic acid, and carbon-bromide moieties under alkaline conditions. Subsequently, copolymers P2–P5 with varied compositions were obtained by random copolymerization of monomers 1 and 6-bromohexanoic acid (2) in different feed ratios. Linear positive correlation is disclosed between the crystallization (Tc) and melting (Tm) temperatures of P1–P5 and the molar fraction of 1 within these specimens. Differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (WAXD) results illustrate good crystallinity of these bioplastics. Furthermore, the degradation of polymers P1–P5 is propelled by an external basic environment while hindered by their intrinsic hydrophobicity, indicating that alkalinity and composition are two essential factors to manipulate the degradation behaviors of biobased polyesters in the bulk state. Ultimately, polymerization of 1 in the presence of 1-pyrenebutyric acid (3), an end-capping agent, was carried out to yield α-pyrene functionalized polymer P7. This material is capable of serving as a practical fluorescent probe and multiwalled carbon nanotube (MWNT) dispersion stabilizer. Polyesterification reported herein represents a facile and cost-effective synthetic strategy and shows great prospects in sustainable polymer materials.

quote

GB/T 7714-2015 [1] JunLin Pan, ChuRan Xu, FuRong Zeng, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00109.
MLA [1] JunLin Pan, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00109.
APA [1] JunLin Pan, ChuRan Xu, FuRong Zeng, Yang Liang, Tao Zhang, Jing Xu, ZiLong Li, & ZiChen Li. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00109
IEEE [1] JunLin Pan, ChuRan Xu, FuRong Zeng, Yang Liang, Tao Zhang, Jing Xu, ZiLong Li, and ZiChen Li, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00109. keywords: {castor oil;bioplastic;polyesterification;fluorescent probe;carbon nanotube}